Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004139
EISBN: 978-1-62708-184-9
... of components on recreational and small workboats. It discusses the materials selection and corrosion control for the components. These components include hulls, fittings, fasteners, metal deck gear, winches, backing plates, lifeline supports, inboard engines, cooling systems, propulsion systems, electrical...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004119
EISBN: 978-1-62708-184-9
... gear, this phenomenon may lead to catastrophic failure. The montage in Fig. 2 illustrates where oxides or corrosion products collect due to dissolution of metal in the pit and where hydrogen evolution and absorption occur causing HE and cracking. Fig. 2 A cracking model illustrating...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006553
EISBN: 978-1-62708-210-5
... Structural members; cylinder heads and pistons; gear, pump, and aerospace housings 208.0 General-purpose castings; valve bodies, manifolds, and other pressure-tight parts 222.0 Bushings; meter parts; bearings; bearing caps; automotive pistons; cylinder heads 238.0 Sole plates for electric hand...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004138
EISBN: 978-1-62708-184-9
..., it is difficult to repair to its original structural integrity. Courtesy of the NRPA NPSI Fig. 6 A noncompatible metal bushing in contact with a stainless steel bolt and other adjacent metal surfaces if left uncorrected may corrode away and weaken the connection. Courtesy of the NRPA NPSI Fig. 7...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004126
EISBN: 978-1-62708-184-9
.... 3 Rusting on a phosphated part after service in a desert environment. The phosphate coating had been blasted off by blowing sand leaving a bare metal surface. Phosphate coatings are specified on 75 to 90% of the parts for small arms. Fig. 1 Pitting of 25 μm (1.0 mil) chromium plating...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001472
EISBN: 978-1-62708-173-3
... of the fusion zone for full and even penetration. An alternative method for inspecting complete weld penetration is that of immersion pulse-echo ultrasonic testing. The planet gear carrier assembly shown in Fig. 9(a) consists of three decks (plates) and eight curved spacer sections. The assembly, which...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004127
EISBN: 978-1-62708-184-9
..., exfoliation, and dissimilar metal galvanic (steel fasteners in aluminum structures) Moisture entrapment, paint failure from flex, and vibration in flight V, U RBR. Item replaced if damage is extensive Wing assembly Forward spar caps and web assembly Intergranular, exfoliation, and stress...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001403
EISBN: 978-1-62708-173-3
... A 607 A 607 Principal ASTM specifications for weldable nonferrous sheet metals Table 23 Principal ASTM specifications for weldable nonferrous sheet metals Type Principal alloying elements ASTM No. Nickel alloys None B 162 Cu B 127 Cr-Fc B 168 Mo B 333 Fe-Cr B...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005252
EISBN: 978-1-62708-187-0
...Abstract Abstract Shell molding is used for making production quantities of castings that range in weight from a few ounces to approximately 180 kg (400 lb), in both ferrous and nonferrous metals. This article lists the limitations or disadvantages of shell mold casting. It describes the two...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006411
EISBN: 978-1-62708-192-4
..., CCMC −34 −29 29.0 221 430 75.0 11.5 146 0.54 1.0 … 75W-90 synthetic hydrocarbon gear oil, GL-5, MIL-L-2105C, limited slip −46 −51 28.0 163 325 106 15.2 149 0.56 … … 15W-40 motor oil, CE/SG, CD-II, MIL-L-2104E, MIL-L-46152D, Caterpillar TO-2, Allison C-4 −29 −20 28.2 232...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004169
EISBN: 978-1-62708-184-9
... grouping of metals and alloys commonly used in commercial airplane design Fig. 5 Manufacturing factors contributing to corrosion Fig. 4 Chrome plating wear and corrosion of steel on a 747 flap carriage journal. The bottom view shows missing chromium plating and corroded journal...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003528
EISBN: 978-1-62708-180-1
... found in metals and their alloys as well as in polycrystalline ceramics (i.e., oxides, carbides, nitrides, etc.). The size of specimens that can be evaluated using XRD can vary widely from as small as the head of a pin to as large as a ship ( Ref 12 , 14 ), a building/structure ( Ref 15 , 16...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006312
EISBN: 978-1-62708-179-5
... International Foundry Congress ( Chicago, IL ), 1982 21. Renfang W. , Yuanheng P. , and Manji C. , “Research on and Experience in the Mass Production of Compacted Graphite Iron Exhaust Manifolds,” BCIRA Conference on Latest and Best in Melting and Metal Treatment in Ferrous and Non...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006768
EISBN: 978-1-62708-295-2
... ). The measurement of residual stress via XRD is generally limited to polycrystalline materials ( Ref 6 ), that is, in materials with a grain structure (long-range ordering) as normally found in metals and their alloys as well as in polycrystalline ceramics (i.e., oxides, carbides, nitrides, etc.). Exceptions occur...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003543
EISBN: 978-1-62708-180-1
... and the welds. Some of the cracking did not occur at casting imperfections or repair welds. Fig. 6 Overload failure of a bronze worm gear ( example 4 ). (a) An opened crack is shown with a repair weld, a remaining casting flaw, and cracking in the base metal. (b) Electron image of decohesive rupture...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... of the cracking did not occur at casting imperfections or repair welds. Fig. 6 Overload failure of a bronze worm gear (Example 4). (a) An opened crack is shown with a repair weld, a remaining casting flaw, and cracking in the base metal. (b) Electron image of decohesive rupture in the fine-grained weld...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003516
EISBN: 978-1-62708-180-1
... at a hole subject to remote tensile loading. Source: Ref 15 Fig. 4 Notch sensitivity versus notch radius for various metals. Approximate values (note shaded band). Not verified for deep notches thickness/radius. Source: Ref 9 Fig. 16 Stress intensity versus loading condition...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006047
EISBN: 978-1-62708-172-6
... in the protective coating/lining industry and a wide variety of applications have been developed. These include coating/lining applications over concrete, geotextile membranes, various metals for corrosion and decorative areas, and some plastics. This article discusses the formulation basics of polyurea technology...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004131
EISBN: 978-1-62708-184-9
... of Pitting Corrosion Fatigue Models , ICAF '99 Proc. ( Seattle, WA ), July 12–16, 1999 16. Bond G.M. , Robertson I.M. , and Birnbaum K. , Effects of Hydrogen on Deformation and Fracture Processes in High-Purity Aluminum Acta Metall. , Vol 36 , 1988 , p 2193 – 2197 10.1016...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006392
EISBN: 978-1-62708-192-4
...  Nonlubricated, such as fasteners, nuts, and bolts Rolling:  Lubricated, such as roller bearings and gears  Nonlubricated, such as wheels on tracks Liquid or vapor impingement on metals Wet steam, such as turbines Combustion gases, such as gas turbines Water, such as pump impellers...