Skip Nav Destination
Close Modal
Search Results for
melt treatment
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1519
Search Results for melt treatment
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006535
EISBN: 978-1-62708-207-5
... on aluminum-silicon modification. aluminum alloys grain refinement melt degassing melt fluxing melt treatment melting cast aluminum alloys melting furnaces wrought aluminum alloys solid fluxes ALUMINUM AND ALUMINUM ALLOYS can be melted in a variety of ways. Coreless and channel induction...
Abstract
There are a wide variety of furnace types and designs for melting aluminum. This article discusses the various types of furnaces, including gas reverberatory furnaces, crucible furnaces, and induction melting furnaces. It describes the classification of solid fluxes: cover fluxes, drossing fluxes, cleaning fluxes, and furnace wall cleaner fluxes. The article reviews the basic considerations in proper flux selection and fluxing practices. It explains the basic principles of degassing and discusses the degassing of wrought aluminum alloys. The article describes filtration in wrought aluminum production and in shape casting. It also reviews grain refinement in aluminum-silicon casting alloys, aluminum-silicon-copper casting alloys, aluminum-copper casting alloys, aluminum-zinc-magnesium casting alloys, and aluminum-magnesium casting alloys. The article concludes with a discussion on aluminum-silicon modification.
Image
Published: 30 November 2018
Image
Published: 01 December 2008
Fig. 30 Treatment cycle of a 75 Mg (80 ton) vacuum arc degassing-heated melt. 1, tapping; 2, additions of C + Al + 0.5% CaO; 3, temperature check; 4, sampling and temperature check; 5, addition of 1.5% alloys + 0.5% CaO; 6, temperature check; 7, additions + 0.5% CaO; 8, degassing; 9, venting
More
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005303
EISBN: 978-1-62708-187-0
... Abstract This article describes the casting characteristics and practices of copper and copper alloys. It discusses the melting and melt control of copper alloys, including various melt treatments to improve melt quality. These treatments include fluxing and metal refining, degassing...
Abstract
This article describes the casting characteristics and practices of copper and copper alloys. It discusses the melting and melt control of copper alloys, including various melt treatments to improve melt quality. These treatments include fluxing and metal refining, degassing, deoxidation, grain refining, and filtration. The article provides a discussion on these melt treatments for group I to III alloys. It describes the three categories of furnaces for melting copper casting alloys: crucible furnaces, open-flame furnaces, and induction furnaces. The article explains the important factors that influence the selection of a casting method. It discusses the production of copper alloy castings. The article concludes with information on the gating and feeding systems used in production of copper alloy castings.
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005903
EISBN: 978-1-62708-167-2
... Abstract Interplays of metallurgical factors, such as dissolved oxygen, carbon, and silicon content, that control the molten metal from melting to pouring, have a decisive influence on the quality of the castings. This article focuses on the magnesium treatment and desulfurization carried out...
Abstract
Interplays of metallurgical factors, such as dissolved oxygen, carbon, and silicon content, that control the molten metal from melting to pouring, have a decisive influence on the quality of the castings. This article focuses on the magnesium treatment and desulfurization carried out during inoculation and nucleation of molten cast iron, assisting in the formation of cast iron. The different types of cast irons are gray cast iron, nodular cast iron, compacted graphite iron, malleable cast iron, and alloyed cast iron. The article provides an overview of the melt treatment processes carried out in cast steel, wrought and cast aluminum, and copper materials.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003174
EISBN: 978-1-62708-199-3
..., inoculation, alloying, and melt treatment of these major ferrous alloys as well as carbon and alloy steels. It explains the principles of solidification by describing the iron-carbon phase diagram, and provides a pictorial presentation of the basic microstructures and processing steps for cast irons...
Abstract
Cast iron, which usually refers to an in situ composite of stable eutectic graphite in a steel matrix, includes the major classifications of gray iron, ductile iron, compacted graphite iron, malleable iron, and white iron. This article discusses melting, pouring, desulfurization, inoculation, alloying, and melt treatment of these major ferrous alloys as well as carbon and alloy steels. It explains the principles of solidification by describing the iron-carbon phase diagram, and provides a pictorial presentation of the basic microstructures and processing steps for cast irons.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005299
EISBN: 978-1-62708-187-0
... characteristics, melting practices, melt treatment, and feeding of the molten steel into the mold used in steel foundries. It discusses the features of melting furnaces used in direct arc melting and induction melting. It reviews factors such as wall thickness and designing for avoidance of hot spots. The article...
Abstract
Sand mold and permanent mold casting are the major methods for shape casting of steels, with production closely split among green sand, chemically bonded sand, and permanent mold processes. This article describes key aspects of the steel casting process, including steel solidification characteristics, melting practices, melt treatment, and feeding of the molten steel into the mold used in steel foundries. It discusses the features of melting furnaces used in direct arc melting and induction melting. It reviews factors such as wall thickness and designing for avoidance of hot spots. The article explains the sand casting and permanent mold casting of steel. The process design and casting of thin sections are also discussed.
Image
Published: 01 December 2004
Fig. 41 Schematic of eutectic melting regions during (a) heat treatment and (b) welding. T H , temperature of annealing; T EM , temperature of eutectic melting; T o , alloy solidus temperature. Dark areas represent regions of eutectic melting.
More
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003109
EISBN: 978-1-62708-199-3
.... A listing of tensile properties of various CG irons produced by different melt treatment methods is also provided. chemical composition compacted graphite iron graphite morphology mechanical properties physical properties COMPACTED GRAPHITE (CG) IRONS are the newest member of the cast iron...
Abstract
This article discusses the graphite morphology, chemical composition, mechanical and physical properties, and applications of compacted graphite (CG) irons. It compares the selected properties of gray, ductile and CG irons, and lists their property requirements as per ASTM A 842. A listing of tensile properties of various CG irons produced by different melt treatment methods is also provided.
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006318
EISBN: 978-1-62708-179-5
... during melting, treatment, and inoculation of cast iron melts to neutralize the effects of tramp elements that may be present and to control the nucleation and growth of graphite during solidification. These trace element additions, if not properly balanced with tramp element levels present in the melt...
Abstract
During the melting and solidification of cast irons, certain trace (minor) elements may unintentionally accumulate to an extent that they have a detrimental effect on the microstructure of castings. This article discusses the residual elements, trace elements, and tramp elements in cast irons. Elements that influence the matrix structure of cast irons are commonly classified as ferrite-promoting elements or pearlite-promoting elements. The article describes the effects of minor elements on microstructure and properties of cast irons. It discusses the use of a combination of tools to control the effects of minor elements on the structure and properties of cast irons. The article concludes with information on allowable levels of trace and tramp elements in cast irons.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005353
EISBN: 978-1-62708-187-0
... the article “Gases in Metals” ). Degassing of steels is described in the article “Steel Melt Processing” in this Volume. Aluminum Foundry Degassing Degassing of aluminum alloy melts is a critical melt treatment technology necessary to provide readiness of the melt for casting into many applications...
Abstract
Gas porosity is a major factor in the quality and reliability of castings. The major cause of gas porosity in castings is the evolution of dissolved gases from melting and dross or slag containing gas porosity. Degassing is the process of removing these gases. This article describes the methods of degassing aluminum, magnesium, and copper alloys. It provides information on the sources of hydrogen in aluminum and gases in copper.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005294
EISBN: 978-1-62708-187-0
... Abstract This article reviews the production stages of iron foundry casting, with particular emphasis on the melting practices, molten metal treatment, and feeding of molten metal into sand molds. It discusses the molten metal treatments for high-silicon gray, high-nickel ductile, and malleable...
Abstract
This article reviews the production stages of iron foundry casting, with particular emphasis on the melting practices, molten metal treatment, and feeding of molten metal into sand molds. It discusses the molten metal treatments for high-silicon gray, high-nickel ductile, and malleable irons. Foundry practices are also described for compacted graphite, high-silicon ductile, and high-alloy white irons.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005300
EISBN: 978-1-62708-187-0
... is similar to that of the aluminum alloy. Nonmetallic and metallic impurities are introduced into the melt during the charging process, the molten metal treatment, and the handling operations. Even when melting primary ingot, nonmetallic impurities such as hydrogen and aluminum oxide are introduced...
Abstract
Aluminum fluxing is a step in obtaining clean molten metal by preventing excessive oxide formation, removing nonmetallic inclusions from the melt, and preventing and/or removing oxide buildup on furnace walls. This article discusses the solid fluxes and gas fluxes used in foundries. It reviews the classification of solid fluxes depending on their use and function at the foundry operation. These include cover fluxes, drossing fluxes, cleaning fluxes, and furnace wall cleaner fluxes. The article also examines the operational practices and applications of the flux injection in the foundries. It describes the applications of the aluminum fluxing such as crucible furnaces, transfer ladles, reverberatory furnaces, and holding/casting furnaces.
Book Chapter
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006329
EISBN: 978-1-62708-179-5
... Abstract Foundry practices critical to the production of cast irons include melting, alloying, molten metal treatment, pouring, and the design of feeding systems (gating and risering) to allow proper filling of the casting mold. This article reviews these production stages of iron foundry...
Abstract
Foundry practices critical to the production of cast irons include melting, alloying, molten metal treatment, pouring, and the design of feeding systems (gating and risering) to allow proper filling of the casting mold. This article reviews these production stages of iron foundry casting, with particular emphasis on the melting practices, molten metal treatment, and feeding of molten metal into sand molds. It discusses the castability factors, such as fluidity, shrinkage, and resistance, of gray iron. Typical cupola charge compositions and the final analyses for class 30 and class 40 gray iron castings are presented in a table. The article describes the induction melting and arc furnace melting used in gray iron foundries. It also reviews the inoculation methods such as stream inoculation and mold inoculation, of gray iron.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005340
EISBN: 978-1-62708-187-0
... elongation of the A356 aluminum alloy. As expected, higher hydrogen content (resulting from ineffective or no melt treatment) is observed to decrease percent elongation. Fig. 14 Effect of increasing hydrogen content of melt on percent elongation of A356 aluminum alloy. Source: Ref 2...
Abstract
Several qualitative, semiquantitative, and quantitative tests are available to estimate and control metal cleanliness, particularly inclusion concentration of aluminum alloys. This article provides a description of a few of the metal cleanliness assessment techniques, such as chemical analysis, pressure filter tests, electric resistivity tests, reduced-pressure test, and ultrasonic technique. Detection methods based on the certain principles and the types of impurities in chemical analysis are discussed.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006421
EISBN: 978-1-62708-192-4
... to modify surface properties when bulk material properties do not meet requirements include surface heat treatment and melting to cause phase transformations and refinement of the microstructure. Because only certain materials respond to such treatments, surface alloying in the form of coatings and thin...
Abstract
Lasers evolved as a versatile materials processing tool due to their advantages such as rapid, reproducible processing, chemical cleanliness, ability to handle variety of materials, and suitability for automation. This article focuses on state-of-the-art laser applications to improve tribological performance of structural materials in lubricated and nonlubricated environments. It discusses the fundamentals of various laser materials interactions and reviews laser-based surface-modification strategies, including laser surface heating and melting, laser-synthesized coatings, and laser-based design approaches such as laser patterning and dimpling. Laser-surface modification of novel materials, such as high-entropy alloys and metallic glasses, is explored. The article provides an overview of hybrid techniques involving laser as a secondary tool, as well as a discussion on the improved capabilities of laser surface engineering for tribological applications by means of integrated computational process modeling.
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006561
EISBN: 978-1-62708-290-7
... ). Because the build plate is routinely reused, it can also develop stresses, and, therefore, it must be creep flattened by placing weighted blocks on it during the stress-relief treatment ( Fig. 3b ). Fig. 2 Illustration of the effect of a stress-relief heat treatment on strain in laser-melted iron...
Abstract
This article focuses on various vacuum heat treating processes for additively manufactured parts, namely annealing and stress relieving, solid-solution annealing, and solution treating and aging. It addresses several practical concerns involved in using vacuum heat treatment, including temperature measurement, unvented cavities, loose powder, and direct contact of metals in the high-temperature vacuum. The article provides a short discussion on sintering and evaporation of metals in vacuum furnaces.
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006315
EISBN: 978-1-62708-179-5
..., distribution, and morphology and their growth pattern to obtain different final graphite morphologies (lamellar/flake, vermicular/compacted, or nodular/spheroidal) could be influenced by modification and/or inoculation treatments. Modification Modification treatment of the iron melt mainly influences...
Abstract
This article describes the modification and inoculation of cast iron, and schematically illustrates the major effects of inoculation in gray cast irons. Inoculation could be considered as a common liquid-state treatment for all commercial cast irons (gray/compacted/ductile irons), while modification is essential to produce compacted graphite iron (intermediate level) and ductile iron. The article discusses the most important aspects of a gray cast iron inoculation treatment and the factors influencing its inoculation efficiency. It describes the modification and inoculation of ductile cast iron and compacted graphite cast iron.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005199
EISBN: 978-1-62708-187-0
... production. Electric arc and induction melting are common methods of melting steels. After furnace melting, the molten steel may be refined in a converter (outside the melting unit) or in a ladle. Thus, steel melt refinements are classified as treatments by either converter metallurgy or ladle metallurgy...
Abstract
This article discusses the most common methods of melting steels, namely, electric arc and induction melting. It describes the classification of refractories by an index of the “basicity” of the slag formed on the steel surface. The article provides a discussion on the converter metallurgy, which includes melt refinement in argon oxygen decarburization (AOD) vessels and vacuum oxygen decarburization (VODC) in a converter vessel. It also discusses ladle metallurgy, which includes vacuum induction degassing, vacuum oxygen decarburization, and vacuum ladle degassing.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005287
EISBN: 978-1-62708-187-0
... an overview on the common methods of aluminum shape casting. Details on melting and melt treatment are covered in the article “Dross, Melt Loss, and Fluxing of Light Alloy Melts” in this Volume. Structure control and grain refinement are detailed in the following articles in this Volume: “Aluminum...
Abstract
Aluminum casting alloys are the most versatile of all common foundry alloys and generally have the highest castability ratings. This article provides an overview of the common methods of aluminum shape casting. These include gravity casting, die casting, sand casting, lost foam casting, shell mold casting, plaster casting, investment casting, permanent mold casting, squeeze casting, semisolid forming, centrifugal casting, and pressure die casting. The article presents several different factors on which the selection of a casting process depends. It discusses gating and risering principles in casting. The article concludes with information on premium engineered castings that provide higher levels of quality and reliability than in conventionally produced castings.
1