1-20 of 277 Search Results for

mechanized tape layering

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006574
EISBN: 978-1-62708-290-7
... Abstract Ultrasonic additive manufacturing (UAM) is a solid-state hybrid manufacturing technique that leverages the principles of ultrasonic welding, mechanized tape layering, and computer numerical control (CNC) machining operations to create three-dimensional metal parts. This article begins...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005605
EISBN: 978-1-62708-174-0
... between successive layers of tape under the ultrasonic vibrations of the rolling welding horn. The mechanism of the process is that the welding horn, having a roughened surface (typically achieved by an electrical discharge machining, or EDM, process), grips the top surface of the tape, causing it to move...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003360
EISBN: 978-1-62708-195-5
... fibers with a greater strain-to-failure ratio than graphite. Several energy-absorbing mechanisms that have been proposed include interlacing resin layers to absorb energy and using fillers to stop cracks. Table 3 shows typical hybrid graphite/ aramid and graphite/glass impact properties. Table 2...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003418
EISBN: 978-1-62708-195-5
... nylon are used to incrementally debulk composite tubing after rolling. They are also used to apply the pressure during cure of noncritical parts such as golf shafts and fishing rods. The amount of actual pressure applied during cure depends on the type of tape used, its thickness, the number of layers...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003053
EISBN: 978-1-62708-200-6
... Removal, p 135–140 F. Kennard, Cold Isostatic Pressing, p 147–152 D. Larson, Green Machining, p 181–185 R.L.K. Matsumoto, Mechanical Consolidation, p 125–129 B.J. McEntire, Dry Pressing, p 141–146 R.E. Mistler, Tape Casting, p 161–165 B.C. Mutsuddy, Injection Molding, p 173–180 J.S...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001111
EISBN: 978-1-62708-162-7
.... A15 superconductors applications of A15 superconductors critical current density layer growth matrix materials multifilamentary wires phase diagrams production methods reaction heat treatment tape conductors layer growth matrix materials multifilamentary wires production methods THE...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003048
EISBN: 978-1-62708-200-6
... Abstract This article is an informative primer on sealants and the role they play in engineered assemblies. It discusses the physical, thermal, chemical, and electrical properties of sealant materials and the various forms in which they are applied, including liquids, pastes, and extruded tapes...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003044
EISBN: 978-1-62708-200-6
... also discusses the test methods of the four major types of mechanical testing of polymer-matrix composites: tensile, compression, flexural, and shear. compression test environmental exposures fiber-reinforced composite stress-strain relationship flexural test laminate mechanical testing...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006562
EISBN: 978-1-62708-290-7
... based on paste type and the method of shape retention of the deposited layer: extrusion freeforming, robocasting ceramic on-demand extrusion, and freeze-form extrusion fabrication. The article then focuses on post-processing considerations and the mechanical properties of sintered ceramic parts. It...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006007
EISBN: 978-1-62708-172-6
... Abstract Functional fusion-bonded epoxy (FBE) coatings are used as external pipe coatings, base layer for three-layer pipe-coating systems, internal pipe linings, and corrosion coatings for concrete reinforcing steel (rebar). This article provides information on the chemistries of FBE, and...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003330
EISBN: 978-1-62708-176-4
... Abstract This article begins with a review of the purposes of mechanical characterization tests and the general considerations related to the mechanical properties of anisotropic systems, specimen fabrication, equipment and fixturing, environmental conditioning, and analysis of test results. It...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003036
EISBN: 978-1-62708-200-6
.... Another major contribution was the use of the expertise of the machine tool industry to improve mechanical designs and computer controls in tape-laying processes. The information in this article is largely taken from H.J. Borstell, Hand Lay-Up, Spray-Up, and Prepreg Molding, Engineering...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002415
EISBN: 978-1-62708-193-1
... throughout specimen volume, in contrast to the localized formation of a predominant, single crack, as is common in isotropic, brittle materials. The four basic failure mechanisms in composites are layer cracking, delamination, fiber breakage, and fiber-matrix interfacial debonding. Any combination of these...
Book Chapter

By Ted Kostilnik
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001235
EISBN: 978-1-62708-170-2
... Abstract Shot peening is a method of cold working in which compressive stresses are induced in the exposed surface layers of metallic parts by the impingement of a stream of shot, directed at the metal surface at high velocity under controlled conditions. This article focuses on the major...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006521
EISBN: 978-1-62708-207-5
... Abstract Chemical conversion coatings are adherent surface layers of low-solubility oxide, phosphate, chromate, and chromate-free compounds produced by the reaction of suitable reagents with the metallic surface. This article provides an overview on chromate-free coatings, along with coverage...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006546
EISBN: 978-1-62708-210-5
... Abstract Aluminum and its alloys are highly corrosion resistant, protected by a self-healing oxide film that effectively passivates the underlying surface. This article examines the various processes by which the protective layer can be breached and the types of corrosion that can occur. It...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006415
EISBN: 978-1-62708-192-4
... mild oxidative wear. The mechanisms of oxidative wear vary depending service conditions and the joint response of the matrix substrate and oxide layer. Oxidation has long been considered a fundamental aspect of sliding wear, and it is well known that oxides reduce wear...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... Abstract Corrosion is the electrochemical reaction of a material and its environment. This article addresses those forms of corrosion that contribute directly to the failure of metal parts or that render them susceptible to failure by some other mechanism. Various forms of corrosion covered are...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005777
EISBN: 978-1-62708-165-8
... parts is difficult; it consumes time and money and may not be feasible. The barrier contaminant layers may have to be removed mechanically, for example, by grinding or blasting, which may create other problems, such as a change in dimensions of the workpiece and the roughness of the surface. Afterwards...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003324
EISBN: 978-1-62708-176-4
... Abstract Adhesive joints involve joining parts by bonding component parts together with an adhesive. This article provides a discussion on the purpose of testing adhesive joints and on the factors influencing mechanical strength of these joints. It describes the various tests used in the...