1-20 of 3228

Search Results for mechanical properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006544
EISBN: 978-1-62708-210-5
... Abstract Understanding the mechanical properties of aluminum alloys is useful for the designer for choosing the best alloy and establishing appropriate allowable stress values, and for the aluminum producer to control the fabrication processes. This article discusses the nature and significance...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006307
EISBN: 978-1-62708-179-5
... Abstract This article describes a method to predict mechanical properties of cast iron materials and illustrates how to use the predictions in computer-aided tools for the analysis of castings subjected to load. It outlines some ways to predict the hardness and elastic modulus of cast iron...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006344
EISBN: 978-1-62708-179-5
... Abstract A wide range of mechanical properties can be obtained with a given composition of cast iron, depending on the microstructural constituents that form during solidification and subsequent solid-state processing. This article discusses the mechanical properties of gray iron and provides...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006345
EISBN: 978-1-62708-179-5
... of ductile iron designated by their tensile properties in the specification ASTM A536 are presented in a table. The article various reviews factors, such as microstructure, composition, and section effect, affecting the mechanical properties of ductile iron. It discusses the hardness properties, tensile...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006346
EISBN: 978-1-62708-179-5
... Abstract The main factors affecting the mechanical properties of compacted graphite irons both at room temperatures and at elevated temperatures are composition, structure (nodularity and matrix), and section size. This article presents a comparison between some properties of flake graphite (FG...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006347
EISBN: 978-1-62708-179-5
... and discusses the chemical composition of malleable iron. A summary of mechanical properties and specifications of malleable iron castings is presented in a table. The article also reviews the mechanical properties of ferritic malleable iron and pearlitic and martensitic-pearlitic malleable irons...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006270
EISBN: 978-1-62708-169-6
... a detailed discussion on the effects of heat treatment on the mechanical properties for three general classes of titanium alloys, namely, alpha and near-alpha titanium alloys, alpha-beta alloys, and beta alloys. alpha and near-alpha titanium alloys alpha-beta alloys fatigue crack propagation fatigue...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006120
EISBN: 978-1-62708-175-7
... Abstract This article describes the factors influencing the room-temperature and elevated-temperature mechanical properties of powder metallurgy (PM) stainless steels. It contains tables that list the mechanical property specifications of the Metal Powder Industries Federation (MPIF) Standard...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005556
EISBN: 978-1-62708-174-0
... Abstract This article discusses the mechanical properties of soft-interlayer solid-state welds and the implications of these behaviors to service stress states and environments. It illustrates the microstructure of as-deposited coatings and solid-state-welded interlayers. The article reviews...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003257
EISBN: 978-1-62708-176-4
... Abstract An integral aspect of designing and material selection is the use of mechanical properties derived from various mechanical testing. This article introduces the basic concepts of mechanical design and its relation with the properties derived from various mechanical testings, namely...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003093
EISBN: 978-1-62708-199-3
... Abstract The properties of carbon and alloy steels are dependent on the relationships between chemical composition, processing, and microstructure. This article discusses the effects of alloying and residual elements on the mechanical properties of carbon and alloy steels. Tables listing values...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001297
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the evaluation of mechanical properties of freestanding films and films adherent to their substrates. Common methods of testing freestanding films, including uniaxial tensile testing, uniaxial creep testing, biaxial testing, and beam-bending methods...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001352
EISBN: 978-1-62708-173-3
... Abstract Soft-interlayer solid-state welds that join stronger base metals have unique mechanical properties that are of fundamental interest and may be of critical importance to designers. This article discusses the mechanical properties of soft-interlayer solid-state welds and the implications...
Image
Published: 01 January 1990
Fig. 4 Tensile properties of ductile iron versus hardness. Mechanical properties determined on specimens taken from a 25 mm (1 in.) keel block More
Image
Published: 01 December 1998
Fig. 4 Tensile properties of ductile iron versus hardness. Mechanical properties were determined on specimens taken from a 25 mm (1 in.) keel block. More
Image
Published: 01 August 2013
Fig. 5 Variation of mechanical properties of cold-sprayed titanium coatings with process parameters. SOD, standoff distance (nozzle); PFR, powder feed rate. Source: Ref 15 More
Image
Published: 01 January 1994
Fig. 4 Effect of heat treatment on the mechanical properties of Ni-10Co and Ni-15Co alloys More
Image
Published: 01 January 1994
Fig. 1 Effect of testing temperature on mechanical properties of ASTM B 23 tin-base babbitt. (a) Grade 2 (75% Sb, 3.5% Cu). (b) Grade 3 (8% Sb, 8% Cu). RA, reduction in area More
Image
Published: 01 January 1994
Fig. 2 Effect of steam treating on the mechanical properties of sintered carbon P/M steels as a function of density. (a) Transverse rupture strength. (b) Apparent hardness. Source: Ref 5 More
Image
Published: 01 August 2013
Fig. 2 General correlation between steel mechanical properties and cooling rate during quenching. IQ, intensive quenching. Source: Ref 4 More