1-20 of 464 Search Results for

matrix type

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003043
EISBN: 978-1-62708-200-6
... Abstract The structural efficiency of a composite structure is established by its joints and assembly. Adhesive bonding, mechanical fastening, and fusion bonding are three types of joining methods for polymer-matrix composites. This article provides information on surface treatment and the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
... MMC designation system and also describes the types of continuous fiber aluminum MMCs, including aluminum/boron MMC, aluminum/silicon carbide MMC, aluminum/graphite MMC, and aluminum/alumina MMC. aluminum-matrix composites copper-matrix composites intermetallic-matrix composites magnesium...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003845
EISBN: 978-1-62708-183-2
... thermosetting resins. The article concludes with a discussion on the curing system of the thermosetting resins with a wide variety of hardener types. furan fabrication fiberglass-reinforced plastic equipment polyester epoxy vinyl-ester phenolic thermosetting resins MANY FACTORS contribute to the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... Abstract This article discusses the types, properties, and uses of continuous-fiber-reinforced composites, including glass, carbon, aramid, boron, continuous silicon carbide, and aluminum oxide fiber composites. While polyester and vinyl ester resins are the most used matrix materials for...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003045
EISBN: 978-1-62708-200-6
... Abstract Ultrasonic inspection is a nondestructive technique that is useful in both quality control and research applications for flaw detection in fiber-reinforced composite materials. This article describes ultrasonic nondestructive analysis by outlining its three basic types of scans. It...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000629
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of a type of resin-matrix composites, carbon-epoxy composites. The fractographs illustrate the fracture modes found in composite prepregs, composite panels, solid rocket motor...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003042
EISBN: 978-1-62708-200-6
... at least pulses rapidly enough to behave as if it were. This requirement reduces the suitable laser types to two: neodymium-YAG and CO 2 . The neodymium-YAG laser, referred to as YAG, uses an active medium of neodymium, which is dissolved in a matrix of yttrium aluminum garnet. The resulting...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
... influence the reinforcement-matrix interface in a ceramic-matrix composite Factor Example Intrinsic property interaction Load transfer Magnitude of bonding Strong, none, or mixed Type of bonding Chemical, physical, mixed Type of coating Fugitive or “permanent” Reaction products...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003046
EISBN: 978-1-62708-200-6
..., most repair relates to two types of damage: environmental factors (such as hail, lightning and bird strikes, and debris kicked up on takeoff or landing) and hangar rash (mishandling of aircraft or components on the ground). Puncture-type damage and microcracking of composites are common; damage of face...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003839
EISBN: 978-1-62708-183-2
... crevice-type corrosion ( Ref 41 , 42 ). Corrosion problems that do not directly arise from the reinforcement, the matrix alloy, or their interaction are usually induced by processing. Examples are corrosion of diffusion bonds and corrosion due to microstructural chlorides. The B MF /Al and Gr...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005227
EISBN: 978-1-62708-187-0
... about MMC types and their applications, see the article “Synthesis and Processing of Cast Metal-Matrix Composites and Their Applications” in this Volume. Table 1 Specific strength and specific modulus of some metal matrices, reinforcements, and metal-matrix composites Material Amount of...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006478
EISBN: 978-1-62708-190-0
...-matrix composites Manufacturing type of defects In-service type of defects Density, fiber ratio, porosity, delaminations, contamination, interface quality, thermal cracking, fiber alignment, foreign inclusions, fiber cuts, bonding defects Impact damage, chemical/physical degradation, moisture...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005339
EISBN: 978-1-62708-187-0
... materials, it is not possible to cover all types of composites in this short discussion. Therefore, major issues pertaining to processing of cast MMCs are discussed by means of examples related to aluminum-matrix composites. MMCs are classified into three broad categories depending on...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000625
EISBN: 978-1-62708-181-8
...-mixture values. (Compare with Fig. 1256 and 1257 .) Fracture surface reveals interlaminar failure of the aluminum matrix (features of this type are usually obliterated in conventional metallography). Inadequate bonding between matrix foils may have been caused by thin surface oxides that did not...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006258
EISBN: 978-1-62708-169-6
... magnesium alloys are the basis for most of the work conducted on magnesium-matrix composites. There are three basic types that are the most common methods of heat treatment applied to magnesium alloys: solution heat treatment, precipitation strengthening or aging, and annealing. In addition to those...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003034
EISBN: 978-1-62708-200-6
... of fiber type, fiber length, and matrix type on thermoset bulk molding compounds. The markets for long-fiber-reinforced bulk molding compounds are electrical, ordnance, aerospace, industrial, sporting goods, and automotive. applications bulk molding compounds fiber length fiber type...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006653
EISBN: 978-1-62708-213-6
... Abstract This article focuses on some of the factors pertinent to atomic absorption spectroscopy (AAS). It begins by describing the working principle, critical components, and construction of flame atomic absorption instrumentation. This is followed by sections discussing various types of...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005681
EISBN: 978-1-62708-198-6
..., priming, and the placement of a resin adhesive layer. It describes the properties of composite resins that are related to the amount and type of filler and resin-matrix compositions. The article also provides a discussion on the compositions, properties, and clinical applications of polyacid-modified...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003005
EISBN: 978-1-62708-200-6
... materials, including ferrous alloys, nonferrous alloys, ceramics, cermets and cemented carbides, engineering plastics, polymer-matrix composites, metal-matrix composites, ceramic-matrix and carbon-carbon composites, and reviews their general property characteristics and applications. It describes the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003033
EISBN: 978-1-62708-200-6
... Abstract This article addresses the types, properties, forms, and applications of fibers that are available for use in fiber-reinforced polymeric matrix composites, including glass, graphite, carbon, aramid, boron, silicon carbide, ceramic, continuous oxide and discontinuous oxide fibers. It...