1-20 of 36 Search Results for

masts

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003407
EISBN: 978-1-62708-195-5
... and sails 30 15 Interior 1 20 Total 100 100 Fig. 5 Typical mast cross section Fig. 1 Racing monohull ( Kiwi Coyote ) for coastal events. Courtesy of Ivor Wilkins Fig. 2 Offshore performance cruising monohull ( Pinta ). Courtesy of Martin Yachts, New Zealand...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004139
EISBN: 978-1-62708-184-9
... without distribution panel Fig. 10 Typical cable drip loop to prevent water entry into a hollow mast Fig. 4 Engine cooling water systems. (a) Raw water system. (b) Freshwater system Fig. 5 Keel heat exchanger installation Fig. 6 Exhaust systems. (a) Traditional wet...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003481
EISBN: 978-1-62708-195-5
... Submarine fins Masts and mast shrouds Rudders Tanks (fuel, lube oil, water) Torpedo tubes Hatch covers Landing craft reconnaissance (15.8 m, or 52 ft) River patrol boat (9.5m, or 31 ft) Pilot boat Submarine fairwater Submarine nonpressure hull casing Deckhouses for small...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002453
EISBN: 978-1-62708-194-8
... , Granta Design , 1995 11. Hayes M. , Materials Update 2: Springs , Engineering , May 1990 , p 42 12. O'Shea Farrel , Windsurfing , Ward Lock , 1991 13. Barker A.J. and Wearing J.L. , Mechanics and Design for Windsurfer Masts , The Engineering of Sport...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003479
EISBN: 978-1-62708-195-5
... composite mast. Courtesy of Fiberspan. (b) General design of a windsurfer. The flexure of the mast controls the shape of the sail; its pivoting about the universal joint controls the response of the craft. Fig. 6 An inner layer of spiral wrapping of carbon filaments being applied to a carbon...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005119
EISBN: 978-1-62708-186-3
... onto a stacking mast. Stacking masts are usually 380 to 915 mm (15 to 36 in.) high. The tops of the masts are either threaded or have tapped holes so that they can be picked up by handling machines and moved to subsequent operations. The bases of the stacking masts are large or weighted to prevent...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001462
EISBN: 978-1-62708-173-3
... Aluminum and zinc TSCs have a long history of corrosion protection in structural steel work: Buildings Bridges Towers Radio and TV antenna masts Steel gantry structures High-power search radar aerials Overhead walkways Railroad overhead line support columns Electrification...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004159
EISBN: 978-1-62708-184-9
... properly refitted after use. Adequate maintenance can prevent cold air entry, especially at discharge doors and electrode support masts and at access door seals. External lagging must be in good condition to maintain housing temperature above the acid dew point. Air entry upstream of the precipitator...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005339
EISBN: 978-1-62708-187-0
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003418
EISBN: 978-1-62708-195-5
... components Telescopes Launcher tubes Masts tube rolling shrink tape debulking finishing preimpregnated materials unidirectional tape convolute wrapping spiral wrapping cylindrical tapered tubes ...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003475
EISBN: 978-1-62708-195-5
... high-gain antenna mast; 4.8 m (16 ft) carbon/epoxy metering truss structure; C-epoxy truss tube focal plane array; C-epoxy optical bench for camera assembly Milstar LDR for flights 1, 2 1994 Spot beam antennas: GY-70/epoxy with Al H/C reflectors (990 and 635 mm, or 39 and 25 in. diam) GY-70...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005709
EISBN: 978-1-62708-171-9
...: bridges ( Fig. 3 ), walkways, piers, railings, buildings, towers Radio and television antenna masts High-power search radar aerials Waterways, gates, locks, chains Water treatment plants Exterior of steel pipes Gas cylinders Ships, boat trailers, and other marine equipment Traffic...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002445
EISBN: 978-1-62708-194-8
... to extend VHDL in this direction. SPICE, which was originally developed at the University of California at Berkeley, is a de facto standard both as a language and a simulator. There are a number of proprietary versions of it (PSPICE, HSPICE) as well as unrelated languages such as the MAST language for Saber...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006716
EISBN: 978-1-62708-210-5
... requiring good corrosion resistance, truck parts, railroad cars, furniture, and pipelines. For example, Alloy 6061-T6 extrusions and tubes are used for ladders, longitudinal members for truck trailers, drive shafts, bumpers, fishing reels, baseball bats, automotive structure, and boat masts. Rolled-product...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003454
EISBN: 978-1-62708-195-5
... are also being used increasingly in the superstructures of ferries and naval frigates, funnels of cruise liners, and antenna masts of large warships. Future applications for composites include rudders, propellers, and propeller shafts for naval ships and propulsors and control surfaces for submarines. Most...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004015
EISBN: 978-1-62708-185-6
... Shower curtain enclosures Swimming pool structures Window and door frames Sporting goods and recreation equipment Bicycle frames and wheels In-line skate rails Sailboat masts Tennis rackets Other Aircraft cargo containers Cargo and bicycle racks Heating elements Ladders...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003173
EISBN: 978-1-62708-199-3
... arc degassing plant layout. 1, transformer; 2, bus bars; 3, flexible cables; 4, electrode arms; 5, temperature-measuring and sampling device; 6, alloying lock; 7, electrode housing; 8, electrode masts; 9, operating platform; 10, lifting device for platform; 11, vacuum cover; 12, ladle heat shield; 13...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003101
EISBN: 978-1-62708-199-3
... components, jet engine shafts, drive shafts, helicopter masts, and containment rings. Properties Maraging steels can be considered highly alloyed low-carbon, iron-nickel lath martensites. The phase transformations in these steels can be explained with the help of the two phase diagrams shown in Fig...
Book Chapter

By David V. Neff
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005353
EISBN: 978-1-62708-187-0
... the shaft/rotor assembly, a gas source, controls to manipulate the gas injection into the system, and the shaft/rotor assembly itself. Equipment can be as simple as a well-mounted drive unit or more complex, with a fixed-mast drive-up ladle treatment station or a mobile unit that can be moved from furnace...
Book Chapter

By Frank K. Ko
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003361
EISBN: 978-1-62708-195-5
... U.S. Composites New York Applications of braided fabrics and composites Table 4 Applications of braided fabrics and composites Aircraft fuselage frames Aircraft interiors Aircraft propellers Artificial limbs, tendons, bone Automotive parts Boats Boat masts Bridge components Chemical...