Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006337
EISBN: 978-1-62708-179-5
... of pressure-actuated pouring furnaces and provides information on the effect of pouring magnesium-treated melts. cast iron melting channel induction furnace cokeless cupola cupola furnaces electric arc furnaces induction crucible furnace induction furnaces magnesium-treated melts plasma-fired...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005903
EISBN: 978-1-62708-167-2
... solidification. Thus, to produce NCI, the basis melt is subjected to magnesium treatment. The melt poured into the mold then contains 0.03 to 0.05% Mg that, as a rule, produces the desired formation of nodules. Figure 13 provides a simplified overview of the graphite forms that result from treating...
Image
Published: 09 June 2014
Fig. 38 Points of crusting and burn-off reactions when processing iron melts treated with magnesium in the pouring furnace More
Image
Published: 31 August 2017
Fig. 34 Points of crusting and burn-off reactions when processing iron melts treated with magnesium in the pouring furnace More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006573
EISBN: 978-1-62708-210-5
... for heat-treated components with air quenching after solution treatment. 0.35–0.45 % Mg for designs focused on strength in as-cast state or after O, T4 or T6 heat treatment. Tables 2 and 3 summarize, respectively, the effects of magnesium alloying and heat treatment on typical tensile properties...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005294
EISBN: 978-1-62708-187-0
... solidification iron foundry casting melting molten metal treatment cast iron foundry inoculation pouring magnesium treatment production quality tests FOUNDRY PRACTICES critical to the production of cast irons include melting, alloying, molten metal treatment, pouring, and the design of feeding...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005904
EISBN: 978-1-62708-167-2
... in diagram form in Fig. 1 ( Ref 1 ). The main ways of producing ready-to-pour melt are as follows: Melting in a crucible furnace in simplex mode (melting and finishing in one unit), transferring the melt in a ladle, with or without magnesium treatment, to an induction-heated pouring furnace...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.9781627081696
EISBN: 978-1-62708-169-6
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003175
EISBN: 978-1-62708-199-3
... number of castings required. However, because magnesium reacts violently with moisture and with the oxygen in the air, a number of precautions must be taken when melting, pouring, and heat treating magnesium alloy castings. Types of Foundry Alloys Foundry alloys vary with the type of molding...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006315
EISBN: 978-1-62708-179-5
... Strong inoculating elements are also deoxidization elements (rare earths, calcium, magnesium). Lower oxygen in iron melt (usually <25 ppm) Uncontrolled oxygen content in iron melt The possibility of silicates to coagulate High oxygen—not always good inoculation response Sulphur...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006310