DOI: 10.31399/asm.hb.v04e.a0006258
EISBN: 978-1-62708-169-6
... Abstract Magnesium-matrix composites (MgMCs) are very promising as structural materials because of their low density, high specific strength, and excellent castability. This article provides information on the characteristics, mechanical properties, and applications of magnesium alloys...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
... Abstract Metal-matrix composites (MMCs) are a class of materials with potential for a wide variety of structural and thermal applications. This article discusses the mechanical properties of MMCs, namely aluminum-matrix composites, titanium-matrix composites, magnesium-matrix composites, copper...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002186
EISBN: 978-1-62708-188-7
... chip formation and distortion due to thermal expansion, cold work, and clamping and provides information on magnesium-matrix composites. The article describes materials, design, and sharpness as factors for selection of tool for machining magnesium. It illustrates turning and boring, planing...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003820
EISBN: 978-1-62708-183-2
... with a discussion on the corrosion of bulk vapor-deposited alloys and magnesium-matrix composites. corrosion fatigue corrosion protection corrosion resistance galvanic corrosion localized corrosion magnesium alloys magnesium-matrix composites stress-corrosion LOW DENSITY and high strength...
Image
Published: 31 December 2017
Fig. 4 (a) Abrasive wear of ductile materials, involving plastic deformation followed by plowing or cutting. (b) Abrasive wear of brittle materials, involving fracture and delamination. (c) and (d) Worn surface of 304 stainless steel. (e) Worn surface of SiCp-reinforced magnesium-matrix More
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.9781627081696
EISBN: 978-1-62708-169-6
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001101
EISBN: 978-1-62708-162-7
... an overview of the status of MMCs, and provides information on physical and mechanical properties, processing methods, distinctive features, and various types of continuously and discontinuously reinforced aluminum, magnesium, titanium, copper, superalloy, and intermetallic-matrix composites. It further...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
... magnesium, copper, and superalloy MMCs. metal-matrix composites high-pressure die casting pressure infiltration casting liquid metal infiltration spray deposition powder metallurgy continuous fiber-reinforced aluminum composite discontinuously reinforced titanium composites continuous fiber...