1-20 of 341 Search Results for

lubricating mechanism

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003177
EISBN: 978-1-62708-199-3
... information on the various drive systems and the auxiliary equipment. It describes the selection of die materials and lubricants for sheet metal forming and provides information on the lubrication mechanisms and selection with a list of lubricant types for forming of specific sheet materials of ferrous or...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004005
EISBN: 978-1-62708-185-6
... Abstract Cold extrusion is a push-through compressive forming process with the starting material (billet/slug) at room temperature. This article provides information on the different types of steels that can be cold extruded. Mechanical presses and hydraulic presses that are specifically...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004032
EISBN: 978-1-62708-185-6
...- and hot-forging processes. The separating function enhances the “propellant effect” in which pyrolysis of the lubricant contents leads to high gas pressure in the die that enables mechanical separation of the hot metal from the die, easing ejection. However, the lubricant should reduce the tendency...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003012
EISBN: 978-1-62708-200-6
... the ease of processing and to improve the properties of the final product. Processing additives improve processing characteristics by: Increasing lubricity, so that less energy is required for manufacturing and less mechanical degradation occurs during processing Stabilizing the polymer, so...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003104
EISBN: 978-1-62708-199-3
... wear, lubrication and lubricated wear, and selection of steels for wear resistance. The article discusses the effect of alloying elements, composition, and mechanical properties of carbon and low-alloy steels at elevated temperatures. It talks about the fatigue resistance characteristics of steels, and...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003030
EISBN: 978-1-62708-200-6
... Abstract Tribology is the science and technology of interacting surfaces in relative motion or, the study of friction, wear, and lubrication. This article focuses on friction and wear processes that aid in the evaluation and selection of materials, for polymers and some composites used in...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004006
EISBN: 978-1-62708-185-6
... Abstract Hot extrusion is a process in which wrought parts are formed by forcing a heated billet through a shaped die opening. This article discusses nonlubricated and lubricated hot extrusion. The two nonlubricated hot extrusion methods are forward or direct extrusion and backward or indirect...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003053
EISBN: 978-1-62708-200-6
... Abstract Ceramic-forming processes usually start with a powder which is then compacted into a porous shape, achieving maximum particle packing density with a high degree of uniformity. This article compares and contrasts several forming processes, including mechanical consolidation, dry...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004008
EISBN: 978-1-62708-185-6
... increase. Die breakage is usually caused by abnormal reductions, lack of mechanical support for the insert, inadequate lubrication, or use of a tool material that is too hard and brittle for the amount of reduction and speed. Some wear resistance is always sacrificed to minimize breakage. Common sizes...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003178
EISBN: 978-1-62708-199-3
... which the work is clamped. Hydraulic or mechanical pressure holds the clamp against the workpiece. Annular grooves or roughened surfaces grip the bar or bar section. Successful bending depends to a large extent on the type of lubricant used. No one lubricant works equally well on all materials...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003241
EISBN: 978-1-62708-199-3
... testing mechanical testing shear testing stress-strain curves tension testing torsion testing HARDNESS is a term that has different meanings to different people: it is resistance to penetration to a metallurgist, resistance to wear to a lubrication engineer, a measure of flow stress to a...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001268
EISBN: 978-1-62708-170-2
... Abstract Mechanical plating is a method for coating ferrous metals, copper alloys, lead, stainless steel, and certain types of castings by tumbling the parts in a mixture of glass beads, metallic dust or powder, promoter or accelerator chemicals, and water. It offers a straightforward...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003999
EISBN: 978-1-62708-185-6
... lubricants used in nickel-base alloys forging. It describes two major forging processing categories for nickel-base alloys: primary working and secondary working categories. Primary working involves the deformation processing and conversion of cast ingot or similar bulk material into a controlled...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003996
EISBN: 978-1-62708-185-6
... die manufacture. The article discusses the critical aspects of various manufacturing elements of aluminum alloy forging, including the preparation of the forging stock, preheating stock, die heating, lubrication, trimming, forming and repair, cleaning, heat treatment, and inspection. It concludes with...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004000
EISBN: 978-1-62708-185-6
... affecting forgeability. It describes the forging techniques, equipment, and common processing elements associated with titanium alloy forging. The processing elements include the preparation of forging stock, preheating of the stock, die heating, lubrication, forging process, trimming and repair, cleaning...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003983
EISBN: 978-1-62708-185-6
... mechanical feed and ample power are used, lubricants on the work can enhance surface finish and die life, regardless of the entrance angle of the dies. With manual feeding, lubricants on the outside of the work can produce hazardous feeding conditions. Dimensions that can be maintained in the normal...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004004
EISBN: 978-1-62708-185-6
... size, machining, descaling, cutting to length, and lubricating. It lists the advantages of the cold heading over machining. Materials selection criteria for dies and punches in cold heading are also described. The article provides examples that demonstrate tolerance capabilities and show dimensional...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003987
EISBN: 978-1-62708-185-6
... Abstract Coining is a closed-die forging operation in which all surfaces of the workpiece are confined or restrained, resulting in a well-defined imprint of the die on the workpiece. This article focuses on the coining equipment (hammers and presses), lubricants, and general and special die...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005323
EISBN: 978-1-62708-187-0
... normal lubrication is also discussed. The article reviews the use of alloys and heat treatment to modify as-cast properties. It concludes with information on physical properties of gray iron castings. gray iron castings castability dimensional stability fatigue limit fluidity gray iron heat...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003181
EISBN: 978-1-62708-199-3
... alloys, titanium alloys, and platinum metals. It discusses the formability, equipment and tooling, and lubricants used in the forming operations of these nonferrous metals. formability forming equipment forming operations lubricants nonferrous metals tooling ALUMINUM...