1-20 of 149 Search Results for

lithium binary system

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 30 November 2018
Fig. 10 Lower part of the aluminum-lithium binary system. Source: Ref 16 More
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006174
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data lithium binary system phase data THIS ARTICLE includes systems where lithium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006208
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data strontium binary system THIS ARTICLE includes systems where strontium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006201
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data sulfur binary system THIS ARTICLE includes systems where sulfur is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006220
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which zinc (Zn) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006186
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data sodium binary system THIS ARTICLE includes systems where sodium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006214
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data thallium binary system THIS ARTICLE includes systems where thallium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006211
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data tellurium binary system THIS ARTICLE includes systems where tellurium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006204
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data selenium binary system THIS ARTICLE includes systems where selenium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006176
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data magnesium binary system phase data THIS ARTICLE includes systems where magnesium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006207
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which tin (Sn) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006205
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data silicon binary system THIS ARTICLE includes systems where silicon is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006192
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which lead (Pb) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006193
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data palladium binary system phase data THIS ARTICLE includes systems where palladium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006166
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data hydrogen binary system phase data THIS ARTICLE includes systems where hydrogen is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006168
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data mercury binary system phase data THIS ARTICLE includes systems where mercury is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006148
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. barium binary system binary phase diagrams crystallographic data phase data THIS ARTICLE includes systems where barium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006152
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams calcium binary system crystallographic data phase data THIS ARTICLE includes systems where calcium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006153
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams cadmium binary system crystallographic data phase data THIS ARTICLE includes systems where cadmium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006150
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams bismuth binary system crystallographic data phase data THIS ARTICLE includes systems where bismuth is the first-named element...