... Abstract Liquid-penetrant inspection is a nondestructive method used to find discontinuities that are open to the surface of solid, essentially nonporous materials. This article describes the physical principles and the process of liquid-penetrant inspection. It also describes the basic...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006440
EISBN: 978-1-62708-190-0
... Abstract Liquid penetrant inspection is a nondestructive method of revealing discontinuities that are open to the surfaces of solid and essentially nonporous materials. This article provides information on physical principles, evolution, description, and processing parameters of liquid...
Image
Published: 01 December 1998
Fig. 3 Equipment arrangement used in a foundry for liquid-penetrant inspection of a large variety of castings to rigid specifications. Castings are moved by crane and roller conveyor. More
Image
Published: 01 August 2018
Fig. 7 Five essential operations for liquid penetrant inspection using the water-washable system More
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006336
EISBN: 978-1-62708-179-5
..., or number of these anomalies exceeds the maximum allowed by the purchaser. The nondestructive methods include visual inspection, dimensional inspection, liquid penetrant inspection, magnetic-particle inspection, eddy-current inspection, radiographic inspection, ultrasonic inspection, resonant testing...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006467
EISBN: 978-1-62708-190-0
... of flaws encountered in the inspection of steel bars, including porosity, inclusions, scabs, cracks, seams, and laps. Inspection methods, such as magnetic-particle inspection. liquid penetrant inspection, ultrasonic inspection, and electromagnetic inspection, of steel bars are also described. The article...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005355
EISBN: 978-1-62708-187-0
... core knockout machine and the A-frame core knockout machine and lists the advantages and disadvantages of these machines. The article describes the general factors in automated or manual gate removal process. It concludes with discussion on the various types of inspection, such as the liquid penetrant...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005341
EISBN: 978-1-62708-187-0
... Abstract The commonly used nondestructive testing of cast products include liquid penetrant inspection, radiographic inspection, fluoroscopic inspection and automated defect recognition, ultrasonic inspection, eddy current inspection, process-controlled resonant testing (PCRT), leak test...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... of detecting surface discontinuities by magnetic-particle inspection, liquid penetrant inspection, and eddy-current testing. The major NDE methods for internal (volumetric) inspection in failure analysis also are described. eddy-current testing liquid penetrant inspection magnetic-particle inspection...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001343
EISBN: 978-1-62708-173-3
.... The article discusses nondestructive evaluation of welds by encompassing techniques that are used to characterize the locations and structure of internal and surface defects, including radiography, ultrasonic testing, and liquid penetrant inspection. It reviews the macrostructural characterization...
Image
Published: 01 August 2018
Fig. 15 Arrangement of equipment used in one foundry for the liquid penetrant inspection of a large variety of castings to rigid specifications. Many of the castings require handling by crane or roller conveyor. More
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002363
EISBN: 978-1-62708-193-1
... electrode imaging methods. The article discusses the magnetic techniques that are primarily used as inspection techniques for detecting fatigue cracks in structural components. It details the principles and operation procedures of the liquid penetrant methods, positron annihilation techniques, acoustic...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001472
EISBN: 978-1-62708-173-3
... porosity. Normally, eddy current inspection is confined to use on thin-wall welded pipe and tubing because eddy currents are relatively insensitive to flaws that do not extend to the surface or into the near-surface layer. Magnetic particle inspection and liquid penetrant inspection are not suitable...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005330
EISBN: 978-1-62708-187-0
... transitions. Smooth transitions between features promote laminar flow of the liquid metal into the casting and also improve the mechanical performance of the part by reducing stress raisers. An additional advantage of these smooth transitions is that designs for castability and for finite-element stress...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003228
EISBN: 978-1-62708-199-3
... Abstract This article reviews nondestructive testing (NDT) and inspection techniques, namely liquid penetrant, magnetic particle, ultrasonics, X-ray, eddy current, visual and radiography that are commonly used to detect and evaluate flaws or leaks in an engineering system. This article compares...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001431
EISBN: 978-1-62708-173-3
... tests  Microexamination tests Nondestructive tests Visual inspection Liquid penetrant inspection Magnetic particle inspection Radiographic inspection Tests to evaluate the mechanical or corrosion properties of weldments are described in detail in several sources ( Ref 1 , 2...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003437
EISBN: 978-1-62708-195-5
... carbide may be sufficient for detection of mixing anomalies, however, appropriate standards must be provided for correct interpretation. Liquid penetrant inspection has been successfully applied to these composites. The addition of the ceramics to the aluminum matrix does not alter the performance...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006479
EISBN: 978-1-62708-190-0
... for Magnetic Particle Testing” ASTM E165 “Standard Practice for Liquid Penetrant Examination for General Industry” ASTM E1417 “Standard Practice for Liquid Penetrant Testing” ASTM E1208 “Standard Practice for Liquid Penetrant Testing Using the Lipophilic Post-Emulsifiable Process” ASTM E1209...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006449
EISBN: 978-1-62708-190-0
... inspection; LP = liquid penetrant; EC = eddy current; PEC = pulsed eddy current; MP = magnetic particle; FL = flux leakage; RF = remote field; MW = microwave; UT = ultrasonic testing; AE = acoustic emission; RT = radiographic testing. Source: Ref 4 Specification Requirements Standards...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001822
EISBN: 978-1-62708-180-1
... of copper-penetration fractures. The Chesapeake & Ohio Railroad reported on an investigation that began in 1952 to determine what could be done to reduce or eliminate wrecks and hot-boxes due to defective journals. The railroad developed a journal-inspection car that used ultrasonic inspection. During...