Skip Nav Destination
Close Modal
Search Results for
liquid steel processing operations
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1533
Search Results for liquid steel processing operations
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001007
EISBN: 978-1-62708-161-0
.... annealing process blast furnace technology cold rolling controlled rolling hot rolling ironmaking practices liquid steel processing operations solid steel processing operations steelmaking practices thermomechanical processing OVER THE LAST THIRTY YEARS, remarkable advances have been made...
Abstract
This article describes ironmaking and steelmaking practices (melt or liquid processing, including hot metal desulfurization) and discusses the evolution of these processes and their effects on steel properties. The physical chemistry of steelmaking may appear deceptively simple for integrated steel mill operations where ore from the ground is converted into steel. The various refining steps that occur in steelmaking are reviewed. The article also describes solid processing of steel, with emphasis on hot and cold rolling, thermomechanical processing, and annealing of flat steel products.
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005776
EISBN: 978-1-62708-165-8
... Abstract The liquid nitriding process has several proprietary modifications and is applied to a wide variety of carbon steels, low-alloy steels, tool steels, stainless steels, and cast irons. This article discusses the applications, subclassifications, operating procedures, and maintenance...
Abstract
The liquid nitriding process has several proprietary modifications and is applied to a wide variety of carbon steels, low-alloy steels, tool steels, stainless steels, and cast irons. This article discusses the applications, subclassifications, operating procedures, and maintenance procedures, as well as the equipment used (salt bath furnaces) and safety precautions to be undertaken during the liquid nitriding process. It describes the different types of liquid nitriding process, namely, liquid pressure nitriding, aerated bath nitriding, and liquid nitrocarburizing. Environmental considerations and the increased cost of detoxification of cyanide-containing effluents have led to the development of low-cyanide salt bath nitrocarburizing treatments. The article reviews the wear and antiscuffing characteristics of the compound zone produced in salt baths with the help of Falex scuff test.
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005778
EISBN: 978-1-62708-165-8
... of cyanide waste disposal in detail. brazing carbonitriding case depth cyanide waste disposal cyanides cyaniding dimensional change hardness liquid carburizing quenching steel LIQUID CARBURIZING is a process used for case hardening steel or iron parts. The parts are held at a temperature...
Abstract
This article describes the uses of the liquid carburizing process carried out in low and high temperature cyanide-containing baths, and details the noncyanide liquid carburizing process which can be accomplished in a bath containing a special grade of carbon. It presents a simple formula for estimating total case depth, and illustrates the influence of carburizing temperature, duration of carburizing, quenching temperature, and quenching medium with the aid of typical hardness gradients. The article provides information on controlling of cyaniding time and temperature, bath composition, and case depth, and presents examples that relate dimensional change to several shapes that vary in complexity. It also provides information on the quenchant removal and salt removal processes, lists the applications of liquid carburizing in cyanide baths, and discusses the process and importance of cyanide waste disposal in detail.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005926
EISBN: 978-1-62708-166-5
.... This article describes the types of atmospheres used in heat treating. More information on controls is given in the articles “Furnace Atmosphere Controls in Heat Treating” in this Volume. General aspects of furnace atmospheres also are introduced in the article “Steel Heat Treating Process Control...
Abstract
This article provides a detailed discussion on the types of furnace atmospheres required for heat treating. These include generated exothermic-based atmospheres, generated endothermic-based atmospheres, generated exothermic-endothermic-based atmospheres, generated dissociated-ammonia-based atmospheres, industrial gas nitrogen-base atmospheres, argon atmospheres, and hydrogen atmospheres. Atmospheres for backfilling, partial pressure operation, and quenching in vacuum are also discussed. Furnace atmospheres constitute four major groups of safety hazards in heat treating: fire, explosion, toxicity, and asphyxiation. The article reviews the fundamentals of principal gases and vapors. It describes how the evaluation of the atmospheric requirements of heat treating furnaces is influenced by factors such as cost of operation and capital investment.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003197
EISBN: 978-1-62708-199-3
... Variables The successful operation of the gas carburizing process depends on the control of three principal variables: temperature, time, and atmosphere composition. Temperature The maximum rate at which carbon can be added to steel is limited by the rate of diffusion of carbon in austenite...
Abstract
Case hardening is defined as a process by which a ferrous material is hardened in such a manner that the surface layer, known as the case, becomes substantially harder than the remaining material, known as the core. This article discusses the equipment required, process variables, carbon and hardness gradients, and process procedures of different types of case hardening methods: carburizing (gas, pack, liquid, vacuum, and plasma), nitriding (gas, liquid, plasma), carbonitriding, cyaniding and ferritic nitrocarburizing. An accurate and repeatable method of measuring case depth is essential for quality control of the case hardening process and for evaluation of workpieces for conformance with specifications. The article also discusses various case depth measurement methods, including chemical, mechanical, visual, and nondestructive methods.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001223
EISBN: 978-1-62708-170-2
... Vapor degreasing is a generic term applied to a cleaning process that uses the hot vapors of a chlorinated or fluorinated solvent to remove soils, particularly oils, greases, and waxes. A vapor degreasing unit consists of an open steel tank with a heated solvent reservoir, or sump, at the bottom...
Abstract
Solvent cleaning is a surface preparation process that can be accomplished in room temperature baths (cold cleaning ) or by condensing vapors of a solvent on a workpiece (vapor degreasing). This article provides a detailed discussion on solvents, equipment, process limitations and applications, and safety and health hazards of cold cleaning and vapor degreasing. It also includes information on control of contamination, conservation and recovery of solvent, and disposal of solvent wastes.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005296
EISBN: 978-1-62708-187-0
... to productivity is the percentage of total clock time that steel is being processed in the machine. These percentages in high-productivity casters can exceed 90% for frequently used casting operations. The turnaround time required for the dummy bar to restart a cast is one of the factors in producing steel...
Abstract
The purpose of continuous casting is to bypass conventional ingot casting and to cast to a form that is directly rollable on finishing mills. The use of this process has resulted in improvement in yield, surface condition, and internal quality of product when compared to the ingot-made material. This article outlines the advantages of steel continuous casting, along with its developments and challenges for improvement. It provides a general description of the continuous casting process and the design and layout of a continuous casting steelmaking facility. It reviews process enhancements such as near-net shape casting, tundish metallurgy, and pouring stream protection. The article discusses the use and capabilities of different molds for steel continuous casting, including thin-wall tube-type molds, solid molds, and plate molds. The article explains the methods for enhancing productivity and improving quality in steel continuous casting. It evaluates the applications of horizontal continuous casting in casting steel. The article concludes by outlining priorities for future development such as enhanced control systems and automation.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003610
EISBN: 978-1-62708-182-5
... metal coolants is described. Some information on safety precautions for handling liquid metals, operating circulating systems, dealing with fire and spillage, and cleaning contaminated components, are also provided. liquid-metal corrosion liquid-metal system liquid-vapor metal coolants safety...
Abstract
This article provides information on the liquid lithium systems that are exposed to liquid metal. It discusses the forms in which liquid-metal corrosion is manifested. The influence of several key factors on the corrosion of metals and alloys by liquid-metal systems or liquid-vapor metal coolants is described. Some information on safety precautions for handling liquid metals, operating circulating systems, dealing with fire and spillage, and cleaning contaminated components, are also provided.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003213
EISBN: 978-1-62708-199-3
... Oxidizing Salt Process Metal finishing operations involving stainless steels, superalloys, and titanium metals usually require an oxidizing salt conditioning treatment in the processing of bar, rod, wire, and strip on a production basis. The operating temperatures of these salts vary between 205...
Abstract
Metal surfaces must often be cleaned before subsequent operations to remove unwanted substances such as pigmented drawing compounds, unpigmented oil and grease, chips and cutting fluids, polishing and buffing compounds, rust and scale, and miscellaneous contaminants. The article describes common cleaning processes, including alkaline, electrolytic, solvent, emulsion, molten salt bath, ultrasonic and acid cleaning as well as pickling and abrasive blasting. It also explains how to select the appropriate process for a given soil type and surface composition.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006038
EISBN: 978-1-62708-172-6
... substrate, pipeline coatings can be subject to many conditions during yard storage, transport, and lowering-in operations. Abrasion damage can lead to a reduction in coating thickness, the localized loss of individual coating layers, and delamination of the coating from the steel substrate. The need...
Abstract
This article describes the coating materials, surface-preparation requirements, and application techniques used to protect underground pipelines. It provides a valuable insight into the types of polymer-based coatings that are both cost-effective and widely accepted in the pipeline industry.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005929
EISBN: 978-1-62708-166-5
... externally heated furnaces heat treatment immersed-electrode furnaces isothermal quenching furnaces salt baths salt quenching steel submerged-electrode furnaces SALT BATHS are used commercially in a wide variety of heat treating operations including neutral hardening, tempering, liquid...
Abstract
This article provides information on the salt baths used for a variety of heat treatments, including heating, quenching, interrupted quenching (austempering and martempering), case hardening, and tempering. It describes two general types of salt bath systems for steel hardening: the first type uses atmosphere austenitizing followed by salt quench and the second type employs austenitizing salt baths with rapid transfer to the quench salt. The article provides a detailed account on the construction, advantages and disadvantages, and limitations of isothermal quenching furnaces, submerged-electrode furnaces, immersed-electrode furnaces, and externally heated furnaces. It discusses the important applications of various furnace designs, including the austempering of ductile iron, the hardening of tool steels, and the isothermal annealing of high-alloy steels.
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005811
EISBN: 978-1-62708-165-8
... the steel. This article introduces the fundamentals, types, advantages and limitations, and the complications of various forms of carburizing, namely, pack carburizing, liquid carburizing or salt bath carburizing, gas carburizing, and low-pressure (vacuum) carburizing. The related process of carbonitriding...
Abstract
Carburization is the process of intentionally increasing the carbon content of a steel surface so that a hardened case can be produced by martensitic transformation during quenching. Like carburizing, carbonitriding involves heating above the upper critical temperature to austenitize the steel. This article introduces the fundamentals, types, advantages and limitations, and the complications of various forms of carburizing, namely, pack carburizing, liquid carburizing or salt bath carburizing, gas carburizing, and low-pressure (vacuum) carburizing. The related process of carbonitriding is also briefly described in the article.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005200
EISBN: 978-1-62708-187-0
... Abstract Vacuum induction melting (VIM) is often done as a primary melting operation followed by secondary melting (remelting) operations. This article presents the process description of VIM and illustrates potential processing routes for products, which are cast from VIM ingots or electrodes...
Abstract
Vacuum induction melting (VIM) is often done as a primary melting operation followed by secondary melting (remelting) operations. This article presents the process description of VIM and illustrates potential processing routes for products, which are cast from VIM ingots or electrodes. It describes the VIM refinement process, which includes the removal of trace elements, nitrogen and hydrogen degassing, and deoxidation. The article concludes with information on the production of nonferrous materials by VIM.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005265
EISBN: 978-1-62708-187-0
... operations proceed as described for the countergravity low-pressure air process in Fig. 1. Loose Sand Vacuum (LSVAC) Process The LSVAC process ( Fig. 6 ) is used to produce thin-wall automotive components. Exhaust manifolds are produced in stainless steel. The process has been demonstrated...
Abstract
This article discusses the general principles and advantages of countergravity mold filling. It details several production implementations that use differential pressure countergravity mold filling methods, namely the countergravity low-pressure air process, countergravity low-pressure vacuum process, countergravity low-pressure inert atmosphere process, countergravity pressure vacuum process, supported shell technique, loose sand vacuum process, and countergravity centrifugal casting process.
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006440
EISBN: 978-1-62708-190-0
... made from ferromagnetic steels; generally, its sensitivity is greater than that of magnetic particle inspection. In practice, the liquid penetrant process is relatively simple to use and control. The equipment used in liquid penetrant inspection can vary from an arrangement of simple tanks...
Abstract
Liquid penetrant inspection is a nondestructive method of revealing discontinuities that are open to the surfaces of solid and essentially nonporous materials. This article provides information on physical principles, evolution, description, and processing parameters of liquid penetrant inspection as well as materials used. It discusses some of the more generally used types of equipment used in penetrant inspection and their requirements. The article describes various penetrant methods and their selection criteria and provides information on precleaning and postcleaning of workpieces before and after penetrant inspection. The quality assurance and maintenance of penetrant inspection materials are also discussed. The article concludes with information on specifications and standards applicable to penetrant inspection.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004137
EISBN: 978-1-62708-184-9
...), a packed tower absorber, exhaust fan, ducting, liquid piping, and liquid recirculation pumps. Figure 2 shows a standard system arrangement, and installed equipment is shown in Fig. 3 . Fig. 2 Schematic of a general scrubber system arrangement Fig. 3 A stainless steel venturi tube...
Abstract
Corrosion problems and materials selection for emissions control equipment can be difficult because of varied corrosive compounds present and the severe environments encountered. This article discusses the selection of materials for construction of flue gas desulfurization systems. It addresses the problems associated with materials for incinerator off-gas treatment equipment. The off-gases can be classified according to their corrosiveness as: industrial chemical, hospital, municipal solid, and sewage sludge. The article provides information on the selection of materials for the three most common types of dust collection equipment used in bulk solids processing, namely, fabric filters, electrostatic precipitators, and wet scrubbers. It also discusses a wide variety of corrosion problems encountered in chemical and pharmaceutical industries.
Book Chapter
Book: Thermal Spray Technology
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005759
EISBN: 978-1-62708-171-9
... Abstract This article discusses the safety issues associated with the design and operation of thermal spray booths and spray box structures and the equipment or systems required for operating thermal spray processes. It describes the design elements necessary to mitigate sound, dust and fume...
Abstract
This article discusses the safety issues associated with the design and operation of thermal spray booths and spray box structures and the equipment or systems required for operating thermal spray processes. It describes the design elements necessary to mitigate sound, dust and fume, ultraviolet light, and mechanical hazards. The means selected for safeguarding personnel must be based on a formal risk assessment that meets ANSI/RIA standards. The safeguards include sensing devices, barriers, awareness signals, procedures, and training. It also provides guidelines that are intended to increase the safety awareness and the use of safety practices for gas and liquid piping and electrical equipment within thermal spray installations.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003091
EISBN: 978-1-62708-199-3
..., and cold-rolled products, and briefly explains the analytical techniques for liquid steels. continuous casting hot rolling ingot casting ironmaking practices liquid steel analytical techniques secondary steelmaking practices special-quality steels specialized processing routes steelmaking...
Abstract
This article presents a detailed account on the process flow, composition, alternative sources, and the advancement of ironmaking, steelmaking and secondary steelmaking practices. Some steels, such as bearing steels, heat-resistant steels, ultrahigh strength missile and aircraft steels, and rotor steels have higher quality requirements and tighter composition control than plain carbon or ordinary low-alloy steels. The production of special-quality steels requires vacuum-based induction or electric remelting and refining capabilities. The article explores the types and characteristics of various steel manufacturing processes, such as ingot casting, continuous casting, and hot rolling. It provides an outline of specialized processing routes of producing ultralow plain carbon steels, interstitial-free steels, high strength low-alloy steels, ultrahigh strength steels, stainless steels, and cold-rolled products, and briefly explains the analytical techniques for liquid steels.
Book Chapter
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006479
EISBN: 978-1-62708-190-0
... for Magnetic Particle Testing” ASTM E165 “Standard Practice for Liquid Penetrant Examination for General Industry” ASTM E1417 “Standard Practice for Liquid Penetrant Testing” ASTM E1208 “Standard Practice for Liquid Penetrant Testing Using the Lipophilic Post-Emulsifiable Process” ASTM E1209...
Abstract
This article is a brief guide to information sources on nondestructive testing (NDT). It provides examples of some of the standards bodies commonly used by NDT personnel. These include the American Society for Testing and Materials (ASTM) International, European Committee for Standardization (CEN), American Society of Mechanical Engineers (ASME), International Organization for Standardization (ISO), Aerospace Industries Association (AIA), American Welding Society (AWS), American Petroleum Institute (API), and American Society for Nondestructive Testing (ASNT). All of these organizations used industry subject-matter experts and a consensus process in the development of their codes and standards.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003570
EISBN: 978-1-62708-180-1
... Abstract Erosion of solid surfaces can be brought about solely by liquids in two ways: from damage induced by formation and subsequent collapse of voids or cavities within the liquid, and from high-velocity impacts between a solid surface and liquid droplets. The former process is called...
Abstract
Erosion of solid surfaces can be brought about solely by liquids in two ways: from damage induced by formation and subsequent collapse of voids or cavities within the liquid, and from high-velocity impacts between a solid surface and liquid droplets. The former process is called cavitation erosion and the latter is liquid-droplet erosion. This article emphasizes on manifestations of damage and ways to minimize or repair these types of liquid impact damage, with illustrations.
1