1-20 of 208 Search Results for

laser brazing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001345
EISBN: 978-1-62708-173-3
... and laser brazing, microwave brazing, and braze welding. braze welding brazing dip brazing electron-beam brazing exothermic brazing filler-metal flow furnace brazing induction brazing infrared brazing laser brazing manual torch brazing microwave brazing resistance brazing surface...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006828
EISBN: 978-1-62708-329-4
... Abstract The various methods of furnace, torch, induction, resistance, dip, and laser brazing are used to produce a wide range of highly reliable brazed assemblies. However, imperfections that can lead to braze failure may result if proper attention is not paid to the physical properties...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006391
EISBN: 978-1-62708-192-4
... materials, namely, iron-base overlays, chromium carbide-based overlays, nickel- and cobalt-base alloys, and tungsten carbide-based metal-matrix composite overlays. It discusses the types of hardfacing processes, such as arc welding processes, and laser cladded, oxyacetylene brazing and vacuum brazing...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005552
EISBN: 978-1-62708-174-0
...; and fusion welding with directed energy sources, such as laser welding, electron beam welding. The article reviews the different types of nonfusion welding processes, regardless of the particular energy source, which is usually mechanical but can be chemical, and related subprocesses of brazing and soldering...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001344
EISBN: 978-1-62708-173-3
... Abstract This article presents an introduction to brazing, including information on its mechanics, advantages, and limitations. It reviews soldering with emphasis on chronology, solder metals, and flux technology. The article also provides useful information on mass, wave, and drag soldering...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005646
EISBN: 978-1-62708-174-0
... (Yb:YAG) thin disk laser surfacing by thermal spraying. defect A discontinuity or discontinuities that by dip brazing (DB) A brazing process using the heat furnished by a molten chemical or metal electric brazing A nonstandard term for arc nature or accumulated effect (for example, bath. When a molten...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003208
EISBN: 978-1-62708-199-3
.... The metal is not melted. The filler-to-base-metal bond Laser Beam Welding power supply for capacitor-discharge stud weld- is the same as in torch brazing. Flux is applied ing is a low-voltage electrostatic storage system, to the joint surfaces, which (together with the LASER BEAM WELDING (LBW) is a joining...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005712
EISBN: 978-1-62708-171-9
... Abstract This article focuses on coatings and overlays adopted for use as wear- and corrosion-resistant materials in oil sand processing. It describes the most common application processes for oil sand coatings and overlays, including welding, high-velocity oxyfuel thermal spray, laser cladding...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001467
EISBN: 978-1-62708-173-3
..., namely, gas-tungsten arc welding, gas-metal arc welding, electron-beam and laser-beam welding, resistance welding, furnace brazing, friction welding, and explosion welding. alumina electron-beam welding explosion welding friction welding furnace brazing gas-metal arc welding gas-tungsten arc...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.9781627081740
EISBN: 978-1-62708-174-0
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003205
EISBN: 978-1-62708-199-3
... Abstract This article discusses different types of joining processes, including welding, brazing, soldering, mechanical fastening, and adhesive bonding. It examines two broad classes of welding: fusion welding and solid-state welding. The article discusses the process selection considerations...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006133
EISBN: 978-1-62708-175-7
..., machining and joining processes for tungsten, tungsten heavy alloys, molybdenum, tantalum, niobium, and rhenium components. It describes the various types of metal joining processes, including mechanical fastening, brazing, and welding. brazing joining machining mechanical fastening molybdenum...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001452
EISBN: 978-1-62708-173-3
... Abstract The quality of brazed stainless steel joints depends on the selection of the brazing process, process temperature, filler metal, and the type of protective atmosphere or flux. This article provides a detailed discussion on the applicability and brazeability of stainless steel and lays...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006119
EISBN: 978-1-62708-175-7
... of the parts with particulates and residues, which can result in the appearance of surface rust. This article provides information on various secondary operations, including tumbling, re-pressing, resin impregnation, annealing or heat treating, brazing, machining, and welding. It describes those aspects...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005647
EISBN: 978-1-62708-174-0
... bonding; dip brazing DBTT ductile-to-brittle transition temperature dc direct current DCEN direct current, electrode negative DCEP direct current, electrode positive DFB diffusion brazing DFW diffusion welding diam diameter DIN Deutsche Industrie-Normen (German Industrial...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005551
EISBN: 978-1-62708-174-0
... of welding and brazing in weld brazing, and the combining of riveting and adhesive bonding in rivet bonding. Similar hybrids have also been developed within welding, combining two different welding processes to obtain some benefit(s). A few examples include laser/gas tungsten arc, laser/gas metal arc...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005856
EISBN: 978-1-62708-167-2
... Abstract This article focuses on the process design set-up procedure for brazing and soldering. It provides a detailed account of the types of base metals that can be joined by these processes, and reviews the factors to be considered to enhance the joint design. Criteria for selection...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001453
EISBN: 978-1-62708-173-3
... cleaning operations as dictated by the particular metals. Controlled atmospheres commonly are employed in furnace brazing; however, they may also be used with brazing processes that utilize induction, resistance, infrared, laser, and electron-beam heat sources. In applications where a controlled atmosphere...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006079
EISBN: 978-1-62708-175-7
... Abstract Metals and alloy powders are used in welding, hardfacing, brazing, and soldering applications, which include hardface coatings, the manufacturing of welding stick electrodes and flux-cored wires, and additives in brazing pastes or creams. This article reviews these applications...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001456
EISBN: 978-1-62708-173-3
... of base-metal powder to the brazing filler alloy were necessary to prevent Kirkendall void formation ( Ref 3 ). A Mo-20Ru brazing filler was used to braze a doped Mo-3Re filament to a tungsten post. Because of a requirement to minimize any recrystallization of the filament, a laser welder working...