...Abstract Abstract This article describes the safety precautions required for using laboratory equipment. It reviews the various personal protective equipment specified on the Material Safety Data Sheets (MSDS) for laboratory chemicals and products. The article provides information...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003566
EISBN: 978-1-62708-180-1
...Abstract Abstract This article briefly reviews the analysis methods for spalling of striking tools with emphasis on field tests conducted by A.H. Burn and on the laboratory tests of H.O. McIntire and G.K. Manning and of J.W. Lodge. It focuses on the metallography and fractography of spalling...
Book Chapter

By Samuel M. Purdy
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003750
EISBN: 978-1-62708-177-1
... the conventional 1 to 1 hot hydrochloric acid etch for iron and steel, the amount of hydrochloric acid fumes produced by the consumption of acid solutions is reduced. In all etching operations, industrial and laboratory, careful thought must be given to safety and the environment, because these processes can...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006432
EISBN: 978-1-62708-192-4
... safety guidelines operate on the ALARA principle: As Low As Reasonably Achievable. General laboratory safety practices reduce the chances of contamination (gloves and lab coat protect the skin from coming into direct contact with radioactive materials) or incorporation (refraining from eating...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006026
EISBN: 978-1-62708-172-6
...? √ Is the laboratory adequately staffed? √ Does the laboratory have any essential personnel? √ Does the laboratory staff have the required education and degrees? √ Does the laboratory have standard operating procedures? √ Does the laboratory have a written safety program...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002430
EISBN: 978-1-62708-194-8
... practices, manuals, and guides to good engineering practice. The National Safety Council publishes many codes that contain recommended practices for reducing the frequency and severity of industrial accidents. Underwriters' Laboratories (UL) prepares hundreds of detailed product safety standards...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
... of input and information, people interviews, laboratory investigations, stress analysis, and fracture mechanics analysis. The article concludes with information on the categories of failure and failure prevention. failure analysis failure prevention fracture mechanics analysis manufacturing...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002394
EISBN: 978-1-62708-193-1
... of areas to include fracture mechanics in design. These included, as stated above, a series of standards that required contractors to use damage tolerance procedures as the primary design tool to ensure safety for new aircraft, a structural reassessment of in-service aircraft, and laboratory support from...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003749
EISBN: 978-1-62708-177-1
... microetching, macroetching, electropolishing, chemical polishing, and other similar operations. anodizing chemical polishing color etching contrast enhancement electropolishing film deposition film formation heat tinting light microscopy macroetching microetching potentiostatic etching safety...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... and records Operator logs Low-strength copper-nickel alloy construction Material specifications Laboratory analysis Flow-induced cavitation Rumbling noise in system Vibration of system Failure mechanism Erosion-fatigue damage Laboratory examination of disk, thinning Consequences Inability...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003751
EISBN: 978-1-62708-177-1
... in the metallographic laboratory: grinding, polishing, etching, preparing a replica, and obtaining a small sample. The article also illustrates the applications of field metallography with case studies. etching field metallography grinding material characteristics polishing specimen preparation specimen...