Skip Nav Destination
Close Modal
Search Results for
isothermal section
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 585
Search Results for isothermal section
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Determination of phase diagrams using AEM. (a) Isothermal section of the Ni...
Available to PurchasePublished: 01 January 1986
Fig. 82 Determination of phase diagrams using AEM. (a) Isothermal section of the Ni-Cr-Mo system. (b) Bright-field microstructure of alloy composition marked C in (a)
More
Image
Published: 01 January 1986
Image
Portion of the 870 °C (1600 °F) isothermal section of the Fe-Cr-C system wi...
Available to PurchasePublished: 01 December 2004
Fig. 37 Portion of the 870 °C (1600 °F) isothermal section of the Fe-Cr-C system with approximate compositions of AISI H13, A2, D2, and type 420 steels indicated. Source: Ref 7
More
Image
Isothermal section of Fe-W-C diagram at 1200 °C (2190 °F). Nominal composit...
Available to PurchasePublished: 01 December 2004
Fig. 38 Isothermal section of Fe-W-C diagram at 1200 °C (2190 °F). Nominal compositions of tungsten, carbon, and iron for some tungsten hot work steels are plotted. Source: Ref 8
More
Image
Isothermal section of a ternary diagram with phase boundaries deleted for s...
Available to PurchasePublished: 01 December 1998
Fig. 10 Isothermal section of a ternary diagram with phase boundaries deleted for simplification
More
Image
The isothermal section at 900 °C (1652 °F) of the Fe-Cr-Ni ternary phase di...
Available to PurchasePublished: 01 December 1998
Fig. 37 The isothermal section at 900 °C (1652 °F) of the Fe-Cr-Ni ternary phase diagram, showing the nominal composition of 18-8 stainless steel. Source: Ref 8
More
Image
The isothermal section at 1250 °C (2280 °F) of the Cr-Mo-Ni nickel ternary ...
Available to PurchasePublished: 01 December 1998
Fig. 38 The isothermal section at 1250 °C (2280 °F) of the Cr-Mo-Ni nickel ternary phase diagram. Source: Ref 9
More
Image
Diffusion paths in the isothermal section of the Fe-C-N phase diagram at 58...
Available to PurchasePublished: 01 August 2013
Fig. 11 Diffusion paths in the isothermal section of the Fe-C-N phase diagram at 580 °C (853 K) for various stages of compound-layer development upon nitrocarburizing α-Fe at 580 °C (853 K) and as shown in Fig. 10 . On this basis, the time-dependent microstructural evolution of the compound
More
Image
Published: 01 August 2013
Image
Isothermal section of the Fe-Mn-C phase diagram at 740 °C (1365 °F) showing...
Available to PurchasePublished: 01 January 1990
Fig. 11 Isothermal section of the Fe-Mn-C phase diagram at 740 °C (1365 °F) showing both the paraequilibrium and true equilibrium phase boundaries. Source: Ref 13
More
Image
The isothermal section at 900 °C (1652 °F) of the Fe-Cr-Ni ternary phase di...
Available to PurchasePublished: 27 April 2016
Fig. 38 The isothermal section at 900 °C (1652 °F) of the Fe-Cr-Ni ternary phase diagram, showing the nominal composition of 18-8 stainless steel. Source: Ref 6 as published in Ref 5
More
Image
Source: A.K. Omarov, S.V. Sejtzhanov, and A.I. Idirisov, Isothermal Section...
Available to PurchasePublished: 27 April 2016
Source: A.K. Omarov, S.V. Sejtzhanov, and A.I. Idirisov, Isothermal Sections of the Ternary System Al-Ni-Ti for the Temperature Range 1150–600 °C, Izv. Akad. Nauk Kazakh. SSSR, Khim , 1985, p 36–42 ( Ref 35 )
More
Image
Published: 01 November 2010
Image
Isothermal section of the gold-silver-copper ternary phase diagram at 370 °...
Available to Purchase
in Properties of Precious Metals
> Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Published: 01 January 1990
Image
Isothermal section of the gold-nickel-copper ternary phase diagram at 315 °...
Available to Purchase
in Properties of Precious Metals
> Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Published: 01 January 1990
Book Chapter
Fe (Iron) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006241
EISBN: 978-1-62708-163-4
... isothermal section at 750 °C; Fe-Mn-Ni isothermal section at 850 °C; Fe-Mn-Ni isothermal section at 650 °C; Fe-Mn-Ni isothermal section at 550 °C; Fe-Mo-Nb isothermal section at 1050 °C; Fe-Mo-Nb isothermal section at 1150 °C; Fe-Mo-Nb isothermal section at 900 °C; Fe-Mo-Ni liquidus projection; Fe-Mo-Ni...
Abstract
This article is a compilation of ternary alloy phase diagrams for which iron (Fe) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Fe-Mn-Ni liquidus projection; Fe-Mn-Ni isothermal section at 750 °C; Fe-Mn-Ni isothermal section at 850 °C; Fe-Mn-Ni isothermal section at 650 °C; Fe-Mn-Ni isothermal section at 550 °C; Fe-Mo-Nb isothermal section at 1050 °C; Fe-Mo-Nb isothermal section at 1150 °C; Fe-Mo-Nb isothermal section at 900 °C; Fe-Mo-Ni liquidus projection; Fe-Mo-Ni isothermal section at 1100 °C; Fe-Mo-Ni isothermal section at 1200 °C; Fe-Ni-W liquidus and solidus projections; Fe-Ni-W isothermal section at 1500 °C; Fe-Ni-W isothermal section at 1455 °C; Fe-Ni-W isothermal section at 1465 °C; and Fe-Ni-W isothermal section at 1400 °C.
Book Chapter
Ag (Silver) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006232
EISBN: 978-1-62708-163-4
... isothermal section at 850 °C; Ag-Au-Cu isothermal section at 950 °C; Ag-Au-Cu isothermal section at 775 °C; Ag-Au-Cu isothermal section at 300 °C; Ag-Cd-Cu isothermal section at 600 °C; Ag-Cd-Cu liquidus projection; Ag-Cd-Cu isothermal section at 500 °C; Ag-Cd-Cu isothermal section at 300 °C; Ag-Cd-Zn...
Abstract
This article is a compilation of ternary alloy phase diagrams for which silver (Ag) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Ag-Au-Cu liquidus projection; Ag-Au-Cu isothermal section at 850 °C; Ag-Au-Cu isothermal section at 950 °C; Ag-Au-Cu isothermal section at 775 °C; Ag-Au-Cu isothermal section at 300 °C; Ag-Cd-Cu isothermal section at 600 °C; Ag-Cd-Cu liquidus projection; Ag-Cd-Cu isothermal section at 500 °C; Ag-Cd-Cu isothermal section at 300 °C; Ag-Cd-Zn isothermal section at 600 °C; Ag-Cd-Zn liquidus projection; Ag-Cd-Zn isothermal section at 400 °C; Ag-Cd-Zn isothermal section at 200 °C; Ag-Cu-Zn isothermal section at 600 °C; Ag-Cu-Zn liquidus projection; and Ag-Cu-Zn isothermal section at 350 °C.
Book Chapter
Mo (Molybdenum) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006243
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which molybdenum (Mo) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 8 phase diagrams: Mo-Nb-Ti isothermal section at 600 °C...
Abstract
This article is a compilation of ternary alloy phase diagrams for which molybdenum (Mo) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 8 phase diagrams: Mo-Nb-Ti isothermal section at 600 °C; Mo-Nb-Ti isothermal section at 1100 °C; Mo-Ni-Ti isothermal section at 1200 °C; Mo-Ni-Ti isothermal section at 900 °C; Mo-Ni-W isothermal section at 700 °C; Mo-Ni-W isothermal section at 1000 °C; Mo-Ti-W isothermal section at 2227 °C; and Mo-Ti-W isothermal section at 1000 °C.
Book Chapter
Pb (Lead) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006245
EISBN: 978-1-62708-163-4
... isothermal section at 240 °C; Pb-Sb-Sn isothermal section at 189 °C; Pb-Sb-Sn (Pb) liquidus projection; Pb-Sn-Zn liquidus projection; and Pb-Sn-Zn isothermal section at 532 °C. isothermal section lead ternary system liquidus projection ternary alloy phase diagrams THIS ARTICLE includes systems...
Abstract
This article is a compilation of ternary alloy phase diagrams for which lead (Pb) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 7 phase diagrams: Pb-Sb-Sn liquidus projection; Pb-Sb-Sn isothermal section at 240 °C; Pb-Sb-Sn isothermal section at 189 °C; Pb-Sb-Sn (Pb) liquidus projection; Pb-Sn-Zn liquidus projection; and Pb-Sn-Zn isothermal section at 532 °C.
Book Chapter
Cd (Cadmium) Ternary Alloy Phase Diagrams
Available to PurchaseBook: Alloy Phase Diagrams
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006237
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which cadmium (Cd) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 4 phase diagrams: Cd-Sb-Sn isothermal section at 212 °C...
Abstract
This article is a compilation of ternary alloy phase diagrams for which cadmium (Cd) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 4 phase diagrams: Cd-Sb-Sn isothermal section at 212 °C; Cd-Sb-Sn liquidus projection; Cd-Sb-Sn isothermal section at 175 °C; and Cd-Sb-Sn isothermal section at 20 °C.
1