... Abstract This article describes the liquidus plots, isothermal plots, and isopleth plots used for a hypothetical ternary phase space diagram. It discusses the single-phase boundary (SPB) line and zero-phase fraction (ZPF) line for carbon-chromium-iron isopleth. The article illustrates the Gibbs...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006300
EISBN: 978-1-62708-179-5
... affects the eutectoid reaction in a similar way as the eutectic reaction. Figure 1(a) shows an isopleth Fe-C section of the stable Fe-Si-C phase diagram at 3.0 mass% Si, which has been limited to the eutectoid temperature range. It is seen that silicon leads to the formation of a three-phase field...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005402
EISBN: 978-1-62708-196-2
... triangular paper. Two other common diagrams of a ternary are an isopleth, that is, a temperature-composition section, with one constraint such as keeping the composition of one component constant, and a projection of the liquidus or solidus surface onto a two-dimensional Gibbs triangular paper. However...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006295
EISBN: 978-1-62708-179-5
... of the liquidus surface of the Fe-C-Si phase diagram in the iron-rich corner for the stable system. Source: Ref 12 Sectioning the Fe-C-Si three-dimensional diagram at constant silicon content leads to a so-called Fe-C isopleth section. The graphs in Fig. 13 ( Ref 25 , 26 ) allow comparing an isopleth...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005511
EISBN: 978-1-62708-197-9
..., ASM Handbook , 2009, a phase diagram is a graphical representation of the phase equilibria of materials in terms of temperature, composition, and pressure. It is normal to think of binary phase diagrams as plots of temperature versus composition at a constant pressure of 1 bar. In reality, many other...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005521
EISBN: 978-1-62708-197-9
... presented in Ref 19 . It is based on tracking the position with time of an isopleth of a chosen function. In the present case, the function is the signed geometric distance to the solid-liquid interface, and the “0” isopleth of this function is tracked. For that purpose, an expression of the velocity...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005206
EISBN: 978-1-62708-187-0
... the Gibbs energy to the phase diagram, as illustrated in Fig. 1 . The Gibbs energy functions of three phases, liquid (l), α, and β, are plotted as functions of the concentration, x B ( x A + x B = 1 for a binary system) for various fixed temperatures. The minimum of the Gibbs energy is given...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003085
EISBN: 978-1-62708-199-3
... in commercial applications, thus improving product predictability. This article describes different equilibrium phase diagrams (unary, binary, and ternary) and microstructures, description terms, and general principles of reading alloy phase diagrams. Further, the article discusses plotting schemes; areas...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006221
EISBN: 978-1-62708-163-4
... Abstract The application of phase diagrams is instrumental in solid-state transformations for the processing and heat treatment of alloys. A unary phase diagram plots the phase changes of one element as a function of temperature and pressure. This article discusses the unary system that can...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003060
EISBN: 978-1-62708-200-6
... a structure's critical regions Couple to a number of finite-element programs, including ABAQUS, ANSYS, COSMOS/M, MARC, and MSC/NASTRAN Fig. 5 Weibull plot of alumina three-point bend bars and biaxially loaded disks fractured in inert and water environments. The solid lines show CARES/LIFE...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006566
EISBN: 978-1-62708-290-7
... showing the influence of solidification rate and temperature gradient on the solidification microstructure. Source: Ref 40 Rapid heating and cooling cycles in an AM process manifest as sharp peaks with steep slopes in time-temperature plots, as measured by thermographic techniques ( Ref 41...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005426
EISBN: 978-1-62708-196-2
... = billion, one byte = eight bits). It ran at a computational speed of four gigaflops (“flops” = floating point operations per second) and required 80 days of computer time. A plot of ocean surface temperature obtained in this simulation is shown in Fig. 2 . Computers with maximum performance at one...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 June 2024
DOI: 10.31399/asm.hb.v12.9781627083874
EISBN: 978-1-62708-387-4
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002444
EISBN: 978-1-62708-194-8
...). It ran at a computational speed of four gigaflops (“flops” = floating point operations per second) and required 80 days of computer time. A plot of ocean surface temperature obtained in this simulation is shown in Fig. 2 . Computers with maximum performance at one teraflop (tera = trillion) are now...