EISBN: 978-1-62708-190-0
... relationship between the strain and the displacement gradient. The part of the nonlinearity parameter that is of particular interest in NDE is the material nonlinearity parameter (β m ), which is a measure of the material nonlinearity in the component being tested. The material nonlinearity parameter...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003241
EISBN: 978-1-62708-199-3
... Abstract This article reviews the various types of mechanical testing methods, including hardness testing; tension testing; compression testing; dynamic fracture testing; fracture toughness testing; fatigue life testing; fatigue crack growth testing; and creep, stress-rupture, and stress...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009007
EISBN: 978-1-62708-185-6
... indentation test plane-strain compression test ring compression test secondary-tension test tension test torsion test workability WORKABILITY is a complex property of a material, as indicated in the article “ Bulk Workability of Metals in this Volume.” It is difficult to isolate the intrinsic...
Book Chapter

By Peter J. Blau
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003242
EISBN: 978-1-62708-199-3
... Abstract Wear is mechanically-induced surface damage that results in the progressive removal of material. Because different types of wear occur in machinery, many different types of wear tests have been developed to evaluate its effects on materials and surface treatments. This article provides...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004017
EISBN: 978-1-62708-185-6
... article discusses the common testing techniques and process variables for workability prediction. It illustrates the simple and most widely used fracture criterion proposed by Cockcroft and Latham and provides a workability analysis using the fracture limit line. The article describes various workability...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003025
EISBN: 978-1-62708-200-6
... mechanical properties of engineering plastics. The testing methods for determining mechanical properties, including stress-strain test, modulus-directed tensile test, strength test, strength-directed tensile test, impact test, and dynamic mechanical test are discussed. crystallinity engineering...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003057
EISBN: 978-1-62708-200-6
... PROPERTIES OR CHARACTERISTICS of advanced ceramic materials may be divided into those that are intrinsic or inherent to the ceramic by nature and those that are extrinsic in nature, that is, related to a performance parameter. The purpose of testing is to provide a basis to evaluate materials properties...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005341
EISBN: 978-1-62708-187-0
... have high intrinsic value or high safety value. It is generally reasonable to test these parts at 100%. PCRT works most efficiently as an on-the-floor factory test. Depending on the circumstances, it can be used with premachined parts or machined parts. The potential limitations to the use of PCRT...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003026
EISBN: 978-1-62708-200-6
.... Because experimental isolation of the intrinsic breakdown process is problematic, intrinsic breakdown mechanisms are not completely understood ( Ref 9 ). The most useful practical tests of breakdown strength are therefore those in which sample preparation and geometry approximate the intended application...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003044
EISBN: 978-1-62708-200-6
...-deflection curve is linear to failure. If any nonlinearity occurs, these relationships must be modified. Such modifications can be found in ASTM D 790 ( Ref 24 ). In general, flexural strength is not considered an intrinsic property; however, the test is inexpensive to run and is usually considered a good...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005438
EISBN: 978-1-62708-196-2
... during software implementation planning to identify suitable programs, software components, and programming languages. It describes the validity tests used in model validation, including boundary-value tests, degenerate problem tests, sensitivity tests, and benchmarking. The article also presents an...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003028
EISBN: 978-1-62708-200-6
... effects on plastic materials, and the accelerated test methods that can be used to estimate the reaction of a plastic component during actual use. The article focuses on the determination of service temperature as it indicates the ability of a material to retain a certain property, when exposed to...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009011
EISBN: 978-1-62708-185-6
... Abstract This article discusses the equipment design, procedures, experimental considerations, and interpretation of the torsion tests used to establish workability. It describes the application of torsion testing to obtain flow-stress data and to gage fracture-controlled workability and flow...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005654
EISBN: 978-1-62708-198-6
... loading modes, cracking mode superposition, and surface area effects. The article describes the fundamentals of CF and SCC, testing methodology, and test findings from laboratory, in vivo, and retrieval studies. cardiovascular surgery corrosion fatigue corrosion fatigue testing dentistry...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009006
EISBN: 978-1-62708-185-6
... mechanisms. It discusses the empirical projections of absolute workability from various mechanical tests. The article concludes with a discussion on extrusion and drawing process design implications. drawing mechanical testing workability EXTRUSION AND WIRE DRAWING are very analogous processes...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005968
EISBN: 978-1-62708-166-5
... using properly standardized test coupons as the basis of a process capability study, one can separate out the variability due to intrinsic noise factors and arrive at the inherent process capability. However, extrinsic contributions should be kept in mind. Additionally, a GR&R (gage repeatability...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005652
EISBN: 978-1-62708-198-6
... metal ions from the bulk material and prevents corrosion of the material in contact with human tissues. Based on testing results of Laing ( Ref 1 ), it is clear that most of the alloying elements used to produce the alloys used in surgery are not intrinsically inert, but the formation of the passive...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003021
EISBN: 978-1-62708-200-6
... welding (vibration, spin, and ultrasonic), and electromagnetic welding (resistance, induction, dielectric, and microwave). It concludes with the evaluation of welds using destructive and nondestructive testing. adhesive bonding adhesives electromagnetic welding friction welding fusion welding...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... details postcoating application quality requirements, including measuring of dry-film thickness, assessing intercoat cleanliness, verifying minimum and maximum recoat intervals, performing holiday/pinhole detection, conducting cure/hardness testing, and assessing adhesion of the applied coating system...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
... Abstract Ceramic-matrix composites (CMCs) are being developed for a number of high-temperature and high-performance applications in industrial, aerospace, and energy conservation sectors. This article focuses on processing, fabrication, testing, and characterization methods of CMCs, namely...