Skip Nav Destination
Close Modal
Search Results for
intermetallic compound
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 555
Search Results for intermetallic compound
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 31 October 2011
Image
Published: 30 August 2021
Fig. 4 Copper-tin (Cu 6 Sn 5 ) and silver-tin (Ag 3 Sn) intermetallic compound morphology in a solder ball
More
Image
Published: 30 August 2021
Fig. 13 Typical growth kinetics of a copper-tin-base intermetallic compound. Source: Ref 31 . Courtesy of Springer Nature
More
Image
Published: 30 August 2021
Image
Published: 30 August 2021
Image
Published: 30 November 2018
Image
Published: 01 January 1993
Fig. 5 Effect of intermetallic compound thickness on room-temperature tensile strength of solder joints (copper/copper base metals)
More
Image
Published: 01 June 2024
Fig. 3 Effect of thermal aging on growth of copper-tin intermetallic compound layer. Cross section and top view at (a) 0 h aging. Original magnification: 3000×. (b) Original magnification: 6000×. (c) 600 h aging. Original magnification: 3000×. (d) Original magnification: 6000×. (e) 1000 h
More
Image
Published: 01 June 2024
Fig. 7 Intermetallic compound and morphology changes subject to thermal aging at 125 °C (255 °F). (a) Electroless nickel immersion gold (ENIG), 0 h. Original magnification: 6000×. (b) Organic solderability preservative (OSP), 0 h. Original magnification: 6000×. (c) ENIG, 500 h. Original
More
Image
Published: 01 June 2024
Image
Published: 01 June 2024
Fig. 12 Dominant solder joint failure modes. IMC, intermetallic compound; PCB, printed circuit board. Source: Ref 4
More
Image
Published: 01 June 2024
Fig. 16 Intermetallic compound (IMC) brittle failure during drop test and high-speed (HS) ball shear/pull tests. (a) IMC failure during drop test. PCB, printed circuit board. (b) IMC fracture failure during HS ball shear (500 mm/s, or 20 in./s). (c) IMC fracture failure during HS ball pull (50
More
Image
Published: 31 October 2011
Fig. 10 Composition of intermetallic compounds in the interface layer. (a) SPCC-A1050 at 1.5 kW, 150 MPa (22 ksi). (b) SPCC- A5052 at 1.5 kW, 150 MPa (22 ksi)
More
Image
Published: 30 August 2021
Fig. 14 Impact fracture energy of copper-tin intermetallic compounds. Source: Ref 26 . © 2013 IEEE. Reprinted, with permission, from IEEE Proceedings
More
Image
Published: 01 January 1996
Image
Published: 01 December 1998
Fig. 8 Hypothetical binary phase diagram showing three intermetallic line compounds and four melting reactions
More
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003164
EISBN: 978-1-62708-199-3
... Abstract Alloys based on ordered intermetallic compounds constitute a unique class of metallic material that form long-range ordered crystal structures below a critical temperature. Aluminides, a unique class of ordered intermetallic materials, possesses many attributes like low densities, high...
Abstract
Alloys based on ordered intermetallic compounds constitute a unique class of metallic material that form long-range ordered crystal structures below a critical temperature. Aluminides, a unique class of ordered intermetallic materials, possesses many attributes like low densities, high melting points, and good high-temperature strength that make them an attractive material for high-temperature structural application. This article discusses the properties, chemical composition, corrosion resistance, processing, fabrication, alloying effects and crystallographic data of nickel aluminides (Ni3Al and NiAl), iron aluminides (Fe3Al and FeAl) and titanium aluminides (alpha-2 alloys, orthorhombic alloys, and gamma alloys).
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004007
EISBN: 978-1-62708-185-6
... the hydrostatic extrusion of structural alloys, composites, brittle materials, and intermetallics or intermetallic compounds, with examples. It concludes with a discussion on the attempts made to extend the hydrostatic extrusion to higher temperatures. brittle materials composites hot hydrostatic...
Abstract
This article begins with a general review of the effects of changes in stress state on processing of materials. It describes the fundamentals of hydrostatic extrusion and reviews the various issues and benefits associated with hydrostatic extrusion. The article discusses the hydrostatic extrusion of structural alloys, composites, brittle materials, and intermetallics or intermetallic compounds, with examples. It concludes with a discussion on the attempts made to extend the hydrostatic extrusion to higher temperatures.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001043
EISBN: 978-1-62708-161-0
... Abstract Maraging steels comprise a special class of high-strength steels that differ from conventional steels in that they are hardened by a metallurgical reaction that does not involve carbon. Instead, these steels are strengthened by the precipitation of intermetallic compounds...
Abstract
Maraging steels comprise a special class of high-strength steels that differ from conventional steels in that they are hardened by a metallurgical reaction that does not involve carbon. Instead, these steels are strengthened by the precipitation of intermetallic compounds at temperatures of about 480 deg C. Commercial maraging steels are designed to provide specific levels of yield strength in the range of 1030 to 2420 MPa. However, some experimental maraging steels have yield strengths as high as 3450 MPa. These steels typically have very high nickel, cobalt, and molybdenum contents and very low carbon contents. This article outlines the processing of maraging steels: melting, hot working, cold working, machining, heat treating, surface treatment, and welding. It also covers mechanical and physical properties as well as tooling and aerospace applications, where maraging steels are extensively used.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003778
EISBN: 978-1-62708-177-1
... on etchants for tin and tin alloys in tabular form. It presents the procedure recommended for electron microscopy to determine the nature of the intermetallic compound formed by the reaction between tin or tin-lead coatings on various substrates. The article concludes with an illustration...
Abstract
This article describes the specimen preparation steps for tin and tin alloys, and for harder base metals which are coated with these materials with illustrations. The steps discussed include sectioning, mounting, grinding, polishing, and etching. The article provides information on etchants for tin and tin alloys in tabular form. It presents the procedure recommended for electron microscopy to determine the nature of the intermetallic compound formed by the reaction between tin or tin-lead coatings on various substrates. The article concludes with an illustration of the microstructures of tin-copper, tin-lead, tin-lead-cadmium, tin-antimony, tin-antimony-copper, tin-antimony-copper-lead, tin-silver, tin-indium, tin-zinc, and tin-zinc-copper systems.