Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004001
EISBN: 978-1-62708-185-6
... Abstract This article reviews the bulk deformation processes for various aluminide and silicide intermetallic alloys with emphasis on the gamma titanium aluminide alloys. It summarizes the understanding of microstructure evolution and fracture behavior during thermomechanical processing...
Image
Published: 01 January 2002
Fig. 57 Sigma (σ) phase in cast heat-resistant alloy HH, type II. Intermetallic phases, such as σ, can greatly reduce the ductility of many high-temperature alloys in service at temperatures from 480 to 955 °C (900 to 1750 °F). More
Image
Published: 01 December 2004
Fig. 40 50Sn-50In alloy. Structure is a eutectic of globular tin-rich intermetallic phase (light) in a matrix of dark indium-rich intermetallic. Etchant 1, Table 1 . 150× More
Image
Published: 01 December 2004
Fig. 9 Zn-0.025Fe alloy, hot graphite mold, slow cooling. Zeta-phase intermetallic compounds. Electrolytic polish. Electrolytic etch: etchant 6, Table 1 (short time). 200× More
Image
Published: 30 August 2021
Fig. 33 Sigma (σ) phase in cast heat-resistant alloy HH, type II. Intermetallic phases, such as σ, can greatly reduce the ductility of many high-temperature alloys in service at temperatures from 480 to 955 °C (900 to 1750 °F). More
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001102
EISBN: 978-1-62708-162-7
.... alloying effects environmental embrittlement fabrication iron aluminides intermetallic mechanical behavior metallurgical properties nickel aluminides silicides titanium aluminides ORDERED INTERMETALLIC compounds constitute a unique class of metallic materials that form long-range ordered...
Image
Published: 01 January 1990
Fig. 1 Atomic arrangements of conventional alloys and ordered intermetallic compounds. (a) Disordered crystal structure of a conventional alloy. (b) Long-range ordered crystal structure of an ordered intermetallic compound More
Image
Published: 01 December 1998
Fig. 1 Atomic arrangements of conventional alloys and ordered intermetallic compounds. (a) Disordered crystal structure of a conventional alloy. (b) Long-range ordered crystal structure of an ordered intermetallic compound More
Image
Published: 01 January 2003
Fig. 2 Schematic drawing of the cross section of a hot-dip coated sheet product showing the three features of all hot-dip coated sheet products—the outer coating layer, the intermetallic alloy bond zone, and the steel sheet substrate More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003164
EISBN: 978-1-62708-199-3
... Abstract Alloys based on ordered intermetallic compounds constitute a unique class of metallic material that form long-range ordered crystal structures below a critical temperature. Aluminides, a unique class of ordered intermetallic materials, possesses many attributes like low densities, high...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001416
EISBN: 978-1-62708-173-3
... Abstract This article focuses on the physical metallurgy and weldability of four families of titanium-base alloys, namely, near-alpha alloy, alpha-beta alloy, near-beta, or metastable-beta alloy, and titanium based intermetallics that include alpha-2, gamma, and orthorhombic systems...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003837
EISBN: 978-1-62708-183-2
... Abstract This article reviews the corrosion behavior of intermetallics for the modeling of the corrosion processes and for devising a strategy to create corrosion protective systems through alloy and coating design. Thermodynamic principles in the context of high-temperature corrosion...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003728
EISBN: 978-1-62708-177-1
... the β components of α + β alloys ( Ref 1 ). In this respect, lightweight titanium-aluminum intermetallic alloys have been extensively studied as potential high-temperature materials for structural applications ( Ref 6 , 7 , 8 , and 9 ) in the gas turbine industry, aeroengines and automotive...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003140
EISBN: 978-1-62708-199-3
... other transition metals. These elements have low solubility in α titanium and decrease the transformation temperature. They usually are added to alloys in combination with one or more of the β isomorphous elements to stabilize the β phase and prevent or minimize formation of intermetallic compounds...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003971
EISBN: 978-1-62708-185-6
... materials, such as intermetallic alloys and composites, have been developed. Furthermore, the advent of user-friendly computer codes and inexpensive computers has led to a revolution in the application of numerical methods for the design and control of a plethora of bulk-forming processes, thus leading...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005620
EISBN: 978-1-62708-174-0
... for rolling and postheating must take into consideration the possibility of intermetallic compound formation, eutectic melting, and/or porosity due to Kirkendall diffusion. The most common metals that are roll welded are low-carbon steels, aluminum and aluminum alloys, copper and copper alloys, d nickel. Low...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001419
EISBN: 978-1-62708-173-3
..., these alloy compositions are characterized by a wider freezing range (typically in excess of 300 °C, or 540 °F) than most aluminum alloys. Conventional I/M processing of these compositions produces equilibrium or near-equilibrium microstructures containing coarse Al 3 Fe-type primary intermetallic particles...
Image
Published: 01 December 1998
Fig. 18 Examples of characteristic eutectic microstructures in slowly cooled alloys. (a) 40Sn-50In alloy showing globules of tin-rich intermetallic phase (light) in a matrix of dark indium-rich intermetallic phase. 150×. (b) Al-13Si alloy showing an acicular structure consisting of short More
Image
Published: 01 December 2004
Fig. 8 Examples of characteristic eutectic microstructures in slowly cooled alloys. (a) 50Sn-50In alloy showing globules of tin-rich intermetallic phase (light) in a matrix of dark indium-rich intermetallic phase. Original magnification 150×. (b) Al-13Si alloy showing an acicular structure More
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0009239
EISBN: 978-1-62708-173-3
... intermetallics, and low ductility. The article reviews induction and torch brazing, infrared brazing, diffusion brazing, and brazing by heating with ion bombardment. It concludes by describing the design criteria and limitations of brazing. alpha-beta alloys brazing brittle intermetallics carbon steel...