Skip Nav Destination
Close Modal
By
Technical Publications Committee of the Porcelain Enamel Institute, Inc. , John C. Oliver, Douglas D. Giese, Jeffrey F. Wright, Ronald L. Allen ...
Search Results for
inorganic finishing
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 153 Search Results for
inorganic finishing
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003214
EISBN: 978-1-62708-199-3
... Abstract Finishing refers to a wide variety of processes that generally involve material removal in one form or another to generate surfaces with specific geometries, tolerances, and functional or decorative characteristics. This article discusses four major finishing methods, namely, abrasive...
Abstract
Finishing refers to a wide variety of processes that generally involve material removal in one form or another to generate surfaces with specific geometries, tolerances, and functional or decorative characteristics. This article discusses four major finishing methods, namely, abrasive machining, electropolishing, mass finishing, and shot peening. In each case, it describes subtypes, process variations, and the associated equipment.
Book Chapter
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001279
EISBN: 978-1-62708-170-2
.... These coatings are differentiated from paint by their inorganic composition and coating properties. They are fused to the metallic substrate at temperatures above 425 °C (800 °F) during the firing process. The most common applications for porcelain enamels are major appliances, water heater tanks...
Abstract
Porcelain enamels are glass coatings applied primarily to products or parts made of sheet steel, cast iron, and aluminum to improve appearance and to protect the metal surface. This article describes the types of porcelain enamels, and details enamel frits for these materials. It provides a list of steels suitable for porcelain enameling and discusses the most important factors considered in the selection of steel for porcelain enameling. The article briefly presents the preparation methods of these materials for porcelain enameling and covers the methods, and furnaces of porcelain enameling. It examines the role of coating thickness, firing time and temperature, metal substrate, and color on the performance of enameled surfaces. The article concludes with a discussion on the properties of enameled surfaces, factors considered in process control, and test procedures for evaluating the quality of enameled surfaces.
Book Chapter
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001308
EISBN: 978-1-62708-170-2
... Abstract Aluminum or aluminum alloy products have various types of finishes applied to their surfaces to enhance appearance or improve functional properties. This article discusses the procedures, considerations, and applications of various methods employed in the cleaning, finishing, and...
Abstract
Aluminum or aluminum alloy products have various types of finishes applied to their surfaces to enhance appearance or improve functional properties. This article discusses the procedures, considerations, and applications of various methods employed in the cleaning, finishing, and coating of aluminum. These include abrasive blast cleaning, barrel finishing, polishing, buffing, satin finishing, chemical cleaning, chemical brightening, electrolytic brightening, chemical etching, alkaline etching, acid etching, chemical conversion coating, electroplating, immersion plating, electroless plating, porcelain enameling, and shot peening.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005242
EISBN: 978-1-62708-187-0
... discussed. The article describes the methods of sand bonding with inorganic compounds. It provides a description of resin-bonded sand systems, namely, no-bake binder systems, heat-cured binder systems, and cold box binder systems. The article concludes with a discussion on the media used for expendable...
Abstract
This article reviews the basic types of mold aggregates and bonding methods for expendable molds and coremaking. It provides an overview of mold media and the basic types of sands and their properties. The most significant clays used in green sand operations, such as bentonites, are discussed. The article describes the methods of sand bonding with inorganic compounds. It provides a description of resin-bonded sand systems, namely, no-bake binder systems, heat-cured binder systems, and cold box binder systems. The article concludes with a discussion on the media used for expendable molds, namely, ceramic shells and rammed graphite, for casting reactive metals such as titanium or zirconium.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003139
EISBN: 978-1-62708-199-3
...-corrosion cracking and galvanic corrosion of magnesium alloys, as well as the surface protection of magnesium assemblies achieved by inorganic surface treatments. corrosion resistance environmental factors galvanic corrosion heavy metal impurities magnesium magnesium alloys magnesium assemblies...
Abstract
This article discusses the effects of heavy metal impurities, environmental factors, the surface condition (such as as-cast, treated, and painted), and the assembly practice on the corrosion resistance of a magnesium or a magnesium alloy part. It provides information on stress-corrosion cracking and galvanic corrosion of magnesium alloys, as well as the surface protection of magnesium assemblies achieved by inorganic surface treatments.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005241
EISBN: 978-1-62708-187-0
... Abstract Casting can be done with either expendable molds for one-time use or permanent molds for reuse many times. This article lists various methods used to fabricate expendable molds from permanent patterns. The methods include molding of sand with clay, inorganic binders, or organic resins...
Abstract
Casting can be done with either expendable molds for one-time use or permanent molds for reuse many times. This article lists various methods used to fabricate expendable molds from permanent patterns. The methods include molding of sand with clay, inorganic binders, or organic resins; shell molding of sand with a thin resin-bonded shell; no-bond vacuum molding of sand; plaster-mold casting; ceramic-mold casting; rammed graphite molding; and magnetic (no-bond) molding of ferrous shot. The article tabulates a general comparison of casting methods and discusses the basic requirements of foundry molds.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006051
EISBN: 978-1-62708-172-6
..., latex coatings, alkyds and other resins, which cure by oxidation, moisture-curing polyurethanes and inorganic zinc primers, and powder coatings. The article concludes with a discussion on the functions of the primer, intermediate coat, and topcoat in coating systems. chemical composition epoxy...
Abstract
A coating can be defined as a substance spread over a surface to provide protection or to serve decorative purposes. This article discusses two industrial coating components, namely, nonvolatile components such as the resin or binder, pigments, and any additives that may be incorporated into the formulation; and volatile components such as solvents, or water in emulsions and their composition. It provides general information on volatile organic compounds. The article describes the film-forming mechanisms of various coating types, namely, lacquers, chemically converting coatings, latex coatings, alkyds and other resins, which cure by oxidation, moisture-curing polyurethanes and inorganic zinc primers, and powder coatings. The article concludes with a discussion on the functions of the primer, intermediate coat, and topcoat in coating systems.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005354
EISBN: 978-1-62708-187-0
... information on the types of organic and inorganic no-bake systems is also provided in the article “Aggregates and Binders for Expendable Molds” in this Volume. Refractory coatings or washes are often necessary or desirable for chemically bonded cores and molds in order to improve surface finish and...
Abstract
No-bake sand molds are based on curing of inorganic or organic binders with either gaseous catalysts or liquid catalysts. This article reviews the major aspects of no-bake sand bonding in terms of coremaking, molding methods, and sand processing. It discusses the points to be noted in handling sand-resin mixtures for no-bake molds or cones and lists some advantages of no-bake air-set cores and molds. The article describes the process procedures, advantages, and disadvantages of gas curing and air-setting hardening of sodium silicates. It discusses the members of the air-setting organic binders, namely, furan no-bake resins, phenolic no-bake resins, and urethanes. The article provides an overview of gas-cured organic binders. It also illustrates the three commercial systems for sand reclamation: wet reclamation systems, dry reclamation systems, and thermal reclamation.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006759
EISBN: 978-1-62708-295-2
... failure analysis. It describes the general considerations for bulk and microscale chemical analysis in failure analysis, the most effective techniques to use for organic or inorganic materials, and examples of using these techniques. The article discusses the processes involved in the chemical analysis of...
Abstract
Chemical analysis is a critical part of any failure investigation. With the right planning and proper analytical equipment, a myriad of information can be obtained from a sample. This article presents a high-level introduction to techniques often used for chemical analysis during failure analysis. It describes the general considerations for bulk and microscale chemical analysis in failure analysis, the most effective techniques to use for organic or inorganic materials, and examples of using these techniques. The article discusses the processes involved in the chemical analysis of nonmetallics. Advances in chemical analysis methods for failure analysis are also covered.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005932
EISBN: 978-1-62708-166-5
... Abstract This article describes various quenchants, namely, water and inorganic salt solutions, polymers (polyvinyl alcohol, polyalkylene glycol, polyethyl oxazoline, polyvinyl pyrrolidone and sodium polyacrylates), quench oils, and molten salts, which are used for heat treatment of ferrous...
Abstract
This article describes various quenchants, namely, water and inorganic salt solutions, polymers (polyvinyl alcohol, polyalkylene glycol, polyethyl oxazoline, polyvinyl pyrrolidone and sodium polyacrylates), quench oils, and molten salts, which are used for heat treatment of ferrous alloys. It also provides information on the steps for controlling quenching performance for polymer quenchants and oils with an emphasis on measuring quenchant performance, safety measures, and oxidation.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001310
EISBN: 978-1-62708-170-2
.... This article focuses on mechanical finishing methods, namely, barrel tumbling, polishing, buffing, vibratory finishing, fiber brushing, and shot blasting. It provides useful information on process control and difficulties with chemical and anodic treatments of magnesium alloys. The use and applications...
Abstract
Surface treatments are applied to magnesium parts primarily to improve their appearance and corrosion resistance. Mechanical and chemical cleaning methods are used singly or in combination, depending on the specific application and product involved to ensure repetitive reliability. This article focuses on mechanical finishing methods, namely, barrel tumbling, polishing, buffing, vibratory finishing, fiber brushing, and shot blasting. It provides useful information on process control and difficulties with chemical and anodic treatments of magnesium alloys. The use and applications of plating and organic finishing of magnesium alloys are also reviewed. The article concludes with a description of health and safety precautions to be followed during the surface treatment process.
Book Chapter
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
... available from metal finishing suppliers. (b) 1.16 sp gr Table 2 Scale dip and bright dip conditions for copper-base metals These solutions remove scale that is not removed by sulfuric or hydrochloric acid solutions; lower concentrations of nitric acid and higher concentrations of sulfuric...
Abstract
The selection of surface treatments for copper and copper alloys is generally based on application requirements for appearance and corrosion resistance. This article describes cleaning, finishing, and coating processes for copper and copper alloys. These processes include pickling and bright dipping, abrasive blast cleaning, chemical and electrochemical cleaning, mass finishing, polishing and buffing, electroless plating, immersion plating, electroplating, passivation, coloring, and organic coatings.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
... Abstract This article discusses the classifications, compositions, properties, advantages, disadvantages, limitations, and applications of the most commonly used methods for surface engineering of carbon and alloy steels. These include cleaning methods, finishing methods, conversion coatings...
Abstract
This article discusses the classifications, compositions, properties, advantages, disadvantages, limitations, and applications of the most commonly used methods for surface engineering of carbon and alloy steels. These include cleaning methods, finishing methods, conversion coatings, hot-dip coating processes, electrogalvanizing, electroplating, metal cladding, organic coatings, zinc-rich coatings, porcelain enameling, thermal spraying, hardfacing, vapor-deposited coatings, surface modification, and surface hardening via heat treatment.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001246
EISBN: 978-1-62708-170-2
... Abstract Iron has been electroplated from a variety of electrolytes, whose bath parameters result in coatings that have widely divergent characteristics according to the specific characteristics desired in the finished product. This article provides an overview of the process description and...
Abstract
Iron has been electroplated from a variety of electrolytes, whose bath parameters result in coatings that have widely divergent characteristics according to the specific characteristics desired in the finished product. This article provides an overview of the process description and processing equipment and discusses the properties, advantages, limitations, and principal applications of iron plating. It also describes the environmental, health, and safety considerations of iron plating.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003132
EISBN: 978-1-62708-199-3
... Abstract This article discusses the applications and tensile properties of selected copper tube alloys, as well as the methods for producing copper tubular products, namely extrusion and rotary piercing. It explains the methods available for the finishing of copper tubular products, such as...
Abstract
This article discusses the applications and tensile properties of selected copper tube alloys, as well as the methods for producing copper tubular products, namely extrusion and rotary piercing. It explains the methods available for the finishing of copper tubular products, such as tube welding, cold drawing, and tube reducing. The article lists the standard dimensions and tolerances for several kinds of copper tubes and pipes in the ASTM specifications, along with other requirements for the tubular products.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001314
EISBN: 978-1-62708-170-2
... reduced oxide, sometimes followed by a flash pickle to brighten; and black or dark-colored surface requiring removal of adherent oxide film or scale. The article also reviews specialized pickling operations of nickel alloys and various cleaning and finishing operations, including grinding, polishing...
Abstract
Nickel alloys can be divided into four groups: high-nickel alloys, nickel-copper alloys, nickel-chromium alloys, and nickel-iron-chromium alloys. Alloys within each composition group that has similar surface conditions are pickled in the same solutions using the same procedures. This article discusses the procedures used for pickling nickel and nickel alloys. It discusses three different surface conditions for pickling these nickel alloys: bright annealed white surface requiring removal of tarnish by flash pickling; bright annealed oxidized surface requiring removal of a layer of reduced oxide, sometimes followed by a flash pickle to brighten; and black or dark-colored surface requiring removal of adherent oxide film or scale. The article also reviews specialized pickling operations of nickel alloys and various cleaning and finishing operations, including grinding, polishing, buffing, brushing, and blasting.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001321
EISBN: 978-1-62708-170-2
... Abstract This article describes selected U.S. environmental statutes and regulations that are pertinent to material surface finishers. It provides information on the applicability, requirements, and permitting conditions of the Clean Air Act, the Resources Conservation and Recovery Act, the...
Abstract
This article describes selected U.S. environmental statutes and regulations that are pertinent to material surface finishers. It provides information on the applicability, requirements, and permitting conditions of the Clean Air Act, the Resources Conservation and Recovery Act, the Superfund Amendments and Reauthorization Act, and the Clean Water Act.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006015
EISBN: 978-1-62708-172-6
... Abstract Powder coatings are widely used by manufacturers as a finish of choice to enhance the appearance and performance of their products. This article begins with a discussion on advantages and disadvantages of powder coatings. It describes the selection of coating-types and uses of powder...
Abstract
Powder coatings are widely used by manufacturers as a finish of choice to enhance the appearance and performance of their products. This article begins with a discussion on advantages and disadvantages of powder coatings. It describes the selection of coating-types and uses of powder coatings in appliance industries, furniture industries, computer industries, fixture industries, architectural industries, automotive industries, agriculture and construction equipment industries, recreational equipment industries, and general industries. Powder coating formulations consist of binder systems, pigments, extenders, and additives. The basic process flow for the manufacture of powder coatings consists of premix, extrusion, grinding, and packing. The article also provides information on application of powder coatings, including pretreatment, deposition, and curing as well as on troubleshooting, trends and challenges for the powder coatings.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003042
EISBN: 978-1-62708-200-6
... Abstract This article describes the use of conventional machining techniques, laser cutting and water-jet cutting for producing finished composite parts. It explains two representative polymer-matrix composites--graphite and aramid composites--and discusses the machining and drilling problems...
Abstract
This article describes the use of conventional machining techniques, laser cutting and water-jet cutting for producing finished composite parts. It explains two representative polymer-matrix composites--graphite and aramid composites--and discusses the machining and drilling problems such as delamination and fiber or resin pullout. The article describes machining and drilling techniques and the necessary tools and cutting parameters. It presents a description of laser cutting. The article also provides information on the advantages, disadvantages, cutting characteristics, and applications of water-jet cutting and abrasive water-jet cutting.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003022
EISBN: 978-1-62708-200-6
... parts which include tests that assess the quality of the finish, coating thickness, adhesion, and corrosion resistance, and gives a short note on service performance, which includes service condition classifications. coating thickness metallizing part design plastics plating quality assurance...
Abstract
The process of coating plastics with metals for functional purposes is called metallizing of plastics. This article discusses the metallizing of plastics, provides information on its history, and gives a short note on applications and adhesion properties of metallic coatings. It also discusses the selection of plastics for plating. This article also describes metallizing techniques, including plating (electrolytic or electroplating), vacuum metallizing and thermal spraying, and environmental considerations. The article discusses the quality assurance procedures for metallized plastic parts which include tests that assess the quality of the finish, coating thickness, adhesion, and corrosion resistance, and gives a short note on service performance, which includes service condition classifications.