1-20 of 181 Search Results for

infrared microscopy

Sort by
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002363
EISBN: 978-1-62708-193-1
... emission techniques, ultrasonic methods, eddy current techniques, infrared techniques, exoelectron methods, and gamma radiography. The article explains the microscopy methods used to determine fatigue crack initiation and propagation. These include electron microscopy, scanning tunneling microscopy, atomic...
Image
Published: 15 December 2019
Fig. 1 Flow charts of common techniques for characterization of glasses and ceramics. AAS, atomic absorption spectrometry; AES, Auger electron spectroscopy; EPMA, electron probe x-ray microanalysis; FTIR, Fourier transform infrared spectroscopy; IA, image analysis; IC, ion chromatography; ICP More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003710
EISBN: 978-1-62708-182-5
... failure analysis surface structure composition optical microscopy scanning electron microscopy scanning tunneling microscopy atomic force microscopy X-ray spectroscopy Auger electron spectroscopy X-ray photoelectron spectroscopy ion scattering spectroscopy reflectance Fourier transform infrared...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005685
EISBN: 978-1-62708-198-6
.... These methods include light microscopy, scanning electron microscopy, atomic force microscopy, energy-dispersive X-ray spectroscopy, Auger electron spectroscopy, secondary ion mass spectrometry, X-ray photoelectron spectroscopy, Fourier transform infrared spectroscopy, and Raman spectroscopy. atomic force...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0005693
EISBN: 978-1-62708-178-8
... ESCA electron spectroscopy for chemical analysis ESR electron spin resonance EXAFS extended x-ray absorption fine structure FIM field ion microscopy FNAA fast neutron activation analysis FMR ferromagnetic resonance FT-IR Fourier transform infrared...
Image
Published: 15 December 2019
; FTIR: Fourier-transform infrared spectrometry; RS: Raman spectroscopy; GC: gas chromatography; GC-MS: gas chromatography-mass spectrometry; LC: liquid chromatography; LC-MS: liquid chromatography-mass spectrometry; XRD: x-ray diffraction; TEM: transmission electron microscopy; OM: optical microscopy More
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006063
EISBN: 978-1-62708-172-6
... environments for coating failure analysis. chromatography differential scanning calorimetry electrochemical impedance spectroscopy Fourier transform infrared spectroscopy laboratory corrosion testing microscopic visual examination scanning electron microscopy-energy dispersive X-ray spectroscopy...
Image
Published: 15 December 2019
Fig. 1 Flow charts of common techniques for characterization of organic solids. AES: Auger electron spectroscopy; AFM: atomic force microscopy; COMB: high-temperature combustion; EFG: elemental and functional group analysis; EPMA: electron probe x-ray microanalysis; ESR: electron spin More
Image
Published: 15 December 2019
Fig. 1 Flow charts of common techniques for characterization of metals and alloys. AES: Auger electron spectroscopy; AFM: atomic force microscopy; COMB: high-temperature combustion; EDS: energy-dispersive x-ray spectroscopy; EFG: elemental and functional group analysis; EPMA: electron probe x More
Image
Published: 12 September 2022
Fig. 11 Powder characterization in the powder-bed fusion process. DSC, differential scanning calorimetry; TG, thermogravimetry; FTIR, Fourier transform infrared spectroscopy; EDX, energy-dispersive x-ray analysis; XRD, x-ray diffraction; AFM, atomic force microscopy More
Image
Published: 15 December 2019
Fig. 2 Images of polystyrene (PS)/polymethyl methacrylate (PMMA) block copolymer, a sample used to gage the performance of nanoinfrared techniques. Photo-induced force microscopy (PiFM) spectra correlate with the Fourier transform infrared (FTIR) spectra quite nicely. By tuning the excitation More
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006678
EISBN: 978-1-62708-213-6
... emission spectroscopy, high-temperature combustion, and inert gas fusion. This is followed by a section on techniques for determining the atomic structure of crystals, namely X-ray diffraction, neutron diffraction, and electron diffraction. Types of electron microscopies most commonly used...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006652
EISBN: 978-1-62708-213-6
... reaction after mixing to provide the hardened final product. In this example, the type of chemistry involved in the epoxy curing (the reaction between the two components) can be established by using Fourier transform infrared (FTIR) spectroscopic analysis of the uncured epoxy components as well...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005647
EISBN: 978-1-62708-174-0
... hot isostatic pressing HK Knoop hardness hp horsepower HR Rockwell hardness (requires scale designation, such as HRC for Rockwell C hardness) HREM high-resolution electron microscopy HSLA high-strength, low-alloy (steel) HSS high-speed steel(s) HTLA heat-treatable low-alloy...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006671
EISBN: 978-1-62708-213-6
..., electron probe x-ray microanalysis; FTIR, Fourier transform infrared spectroscopy; IA, image analysis; IC, ion chromatography; ICP-AES, inductively coupled plasma atomic emission spectroscopy; IR, infrared spectroscopy; LEISS, low-energy ion-scattering spectroscopy; NAA, neutron activation analysis; OES...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006748
EISBN: 978-1-62708-213-6
... Definitions of Terms Relating to Microscopy ,” E 175, Annual Book of ASTM Standards , Vol 14.01 , American Society for Testing and Materials , Philadelphia, PA , 1984 , p 215 – 219 • “ Standard Definitions of Terms Relating to Surface Analysis ,” E 673, Annual Book of ASTM Standards , Vol 03.06...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0005692
EISBN: 978-1-62708-178-8
... , p 12 – 48 • “Standard Definitions of Terms Relating to Microscopy,” E 175, Annual Book of ASTM Standards , Vol 14.01 , ASTM , Philadelphia , 1984 , p 215 – 219 • “Standard Definitions of Terms Relating to Surface Analysis,” E 673, Annual Book of ASTM Standards , Vol 03.06...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006662
EISBN: 978-1-62708-213-6
... Abstract Infrared (IR) spectra have been produced by transmission, that is, transmitting light through the sample, measuring the light intensity at the detector, and comparing it to the intensity obtained with no sample in the beam, all as a function of the infrared wavelength. This article...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006673
EISBN: 978-1-62708-213-6
... by Fourier transform infrared spectroscopy analysis. The relative loadings of various constituents within a plastic material, including polymers, plasticizers, additives, carbon black, mineral fillers, and glass reinforcement, can be assessed. The assessment of a plastic resin composition is illustrated...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0005663
EISBN: 978-1-62708-173-3
... expansion EXB exothermic brazing AFM atomic force microscopy CTOD crack tip opening displacement exp base of the natural logarithm CVD chemical vapor deposition EXW explosion welding AI artificial intelligence CVN Charpy V-notch (impact test or speci- f frequency AISC American Institute of Steel Construc...