1-14 of 14 Search Results for

infeed bar handling systems

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005849
EISBN: 978-1-62708-167-2
..., discharge chutes, pinch roll extractors, pick-n-place systems, and robots. billet pusher systems continuous conveyor systems dual pinch roll drive assemblies hot billet handling systems induction heating infeed bar handling systems infeed billet handling systems material handling equipment...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002142
EISBN: 978-1-62708-188-7
... that often the only fixture required for manual loading is a spring-loaded work stop to provide correct axial position. Lathes and Automatic Machines Radial infeed rolling can be done in lathes and automatic bar machines equipped with single-roll or double-roll radial threading attachments...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004012
EISBN: 978-1-62708-185-6
.... The dies in a three-die machine serve to locate the part so that often the only fixture required for manual loading is a spring-loaded work stop to provide correct axial position. Lathes and Automatic Machines Radial infeed rolling can be done in lathes and automatic bar machines equipped...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002151
EISBN: 978-1-62708-188-7
... applications, including floorstand, portable snagging, weld grinding, and most cutoff applications. In precision grinding, resin bonds are used in three situations: where system flexibility would break down a vitrified wheel (such as steel mill roll grinding and most centerless-bar grinding applications...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002186
EISBN: 978-1-62708-188-7
... and shaping, broaching, drilling, reaming, counterboring, milling, sawing, and grinding operations performed on magnesium. Safety measures related to machining, handling of chips and fines, and fire extinguishing are also discussed. boring broaching clamping cold working counterboring drilling...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003983
EISBN: 978-1-62708-185-6
... support. The carriage provides a means of attaching plain or antifriction workpiece holders and adapters, as well as a handle for manual feeding toward the swager. An adjustable stop is provided on the support bar to control the length of the swaged section and to reproduce accurate tapers. Roll-Feed...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003193
EISBN: 978-1-62708-199-3
..., standard marking systems, abrasives, and bonding types. It compares bonded wheel grinding with abrasive belt grinding. The article reviews the types of grinding fluids and discusses their importance in grinding operations. It describes the specific grinding processes and provides recommendations...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002145
EISBN: 978-1-62708-188-7
...: Depth of a tooth space below the pitch circle Diametral pitch: A measure of tooth size in the English system. In units, it is the number of teeth per inch of pitch diameter. As the tooth size increases, the diametral pitch decreases. Diametral pitches usually range from 25 to 1 Face width...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006422
EISBN: 978-1-62708-192-4
... lubricant and catch loose debris that might otherwise be rolled into the strip surface. Uniform, reproducible lubricant application is crucial in experiments aimed at lubricant evaluation. A simplified recirculating system ( Fig. 17 ) incorporating a pump, heater, mixer, spray bars, and a catch tray...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002185
EISBN: 978-1-62708-188-7
... beyond the 25% maximum cold reduction normally given leaded brass bars of most sizes. Fig. 5 Effect of cold work on the machinability of free-cutting brass (machinability scale non-standard) In drilling tests on a typical free-cutting brass rod to determine the effect of cold work...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002184
EISBN: 978-1-62708-188-7
..., broaching, reaming, tapping, milling, sawing, grinding, honing, and lapping. The article concludes with a discussion on drilling operations in automatic bar and chucking machines and drill presses. aluminum aluminum alloys boring broaching cutting force grinding high-silicon aluminum alloys...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002189
EISBN: 978-1-62708-188-7
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009015
EISBN: 978-1-62708-187-0
... continuously filled during pouring. Avoid abrupt changes in the direction of metal flow; gate and runner passages should be streamlined for minimum induced turbulence at angles or points of divergence in the system. Provide contoured transitions in gate, runner, and infeed cross sections at points...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.9781627081924