1-20 of 449 Search Results for

induction heating coils

Sort by
Image
Published: 01 November 2010
Fig. 28 Examples of circuit connections of induction heating coils (L) with fixed or variable capacitors (C). V , coil voltage. Source: Ref 1 More
Image
Published: 01 November 2010
Fig. 32 Multilayer induction heating coils. Courtesy of IHWT, England More
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005840
EISBN: 978-1-62708-167-2
..., and brazing and fabricating the copper coil winding for heating billets, bars, and slabs. The article describes refractory selection criteria and the methods of mounting and securing the induction coil winding, and presents general refractory installation guidelines for induction heating applications...
Image
Published: 09 June 2014
Fig. 3 Induction heating coil for hardening of undercarriage rollers. Source: Ref 1 More
Image
Published: 09 June 2014
Fig. 4 Thermal gradient through an induction heating coil More
Image
Published: 09 June 2014
Fig. 5 Cross sections of typical induction billet heating coils. S, induction coil; R, refractory insulation; G, guide rail. Source: Ref 5 , 6 More
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005913
EISBN: 978-1-62708-167-2
..., nanoparticles, induction heating setup, and magnetic field strength. hyperthermia induction heating coils magnetic field nanoparticles solenoid coils thermal gradient Induction heating is a convenient and flexible method to deliver high-strength magnetic fields to nanoparticles, resulting...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005849
EISBN: 978-1-62708-167-2
... to the induction heating system, every induction heating system has a mechanism for feeding the billets through the induction heating coils. Induction billet heaters are classified based on the type of materials handling system they use. The main categories of billet feeding systems are: Dual pinch roll...
Image
Published: 09 June 2014
Fig. 6 Assortment of copper tubes used for the design and manufacture of induction heating coils; includes rounds, squares, rectangles, ovals, and so on More
Image
Published: 01 January 2005
Fig. 12 Example of an 8000 ton isothermal forge press. Billet preheat chamber, transfer mechanisms, forge dies, and induction heating coils are all enclosed with a vacuum chamber. Courtesy of Pratt & Whitney More
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005843
EISBN: 978-1-62708-167-2
... of components, and testing the setup. frequency induction coils inductors load matching power supplies power supply circuit transformers TRANSFORMERS AND REACTORS for induction heating are discussed in the first half of this article as well as the following topics: initial considerations...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005839
EISBN: 978-1-62708-167-2
... Abstract This article provides information on single-shot and scanning, the two types of induction heat treating processes that are based on whether the induction coil is moving relative to the part during the heating process. It describes the effect of the frequency of induction heating...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005854
EISBN: 978-1-62708-167-2
... Abstract Induction heating system control is straightforward after the design and application of the coil and power supply required for the job. This article provides an overview of the basic components of an induction heating system, including a machine controller (computer or programmable...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005846
EISBN: 978-1-62708-167-2
..., and linear coils. It provides information on the role of magnetic flux controllers for whole-body and local area mass-heating applications, continuous induction tube welding, seam-annealing inductors, and various induction melting systems, namely, channel-type, crucible-type, and cold crucible systems...
Image
Published: 30 September 2014
Fig. 48 Longitudinal heating coil, single shot with quench. Source: Induction Tooling More
Image
Published: 01 August 2013
Fig. 3 Induction coil with an offset used to provide heating uniformity More
Image
Published: 01 August 2013
Fig. 28 Adjustment (coil characterization) of induction heating patterns for several parts by varying the coupling distance or turn spacing. Source: Ref 19 More
Image
Published: 09 June 2014
Fig. 4 Infrared multiple-coil induction heating system More
Image
Published: 01 January 2000
Fig. 11 Adjustable work coil fixture for direct induction heating in elevated-temperature fatigue testing More
Image
Published: 01 November 2010