1-20 of 381 Search Results for

induction heating coil

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005840
EISBN: 978-1-62708-167-2
... that is used to heat bar ends. Courtesy of Pillar Induction Fig. 7 Heavy-wall tubing used in construction of induction coils Fig. 12 Low-frequency coil design in which the induction coil winding is compressed between end plates using long rods with threads and nuts. Courtesy of Ajax Tocco...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005839
EISBN: 978-1-62708-167-2
... of quick-change adapters. Courtesy of Capital Induction Fig. 27 Temperature distribution in the induction coil with 1 mm (0.048 in.) wall thickness, 10 kHz frequency, 5000 A current, and low-pressure cooling Fig. 28 Temperature dynamics during heating at critical points with 1 mm (0.048...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005846
EISBN: 978-1-62708-167-2
... Fig. 1 Magnetic circuit in a single turn coil with magnetic flux concentrator heating cylindrical part from the outside: Φ = total. Source: Ref 3 Fig. 13 Schematic of channel-type induction melting furnace. Source: Ref 13 Fig. 16 Comparison of power density in the melt...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005913
EISBN: 978-1-62708-167-2
..., namely, nanoparticles, induction heating setup, and magnetic field strength. hyperthermia induction heating coils magnetic field nanoparticles solenoid coils thermal gradient Induction heating is a convenient and flexible method to deliver high-strength magnetic fields to nanoparticles...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005516
EISBN: 978-1-62708-197-9
... 16 10 600 1112 192 66 47 30 23 14.9 1500 2732 218 75 53 33 26 17 Source: Ref 1 Fig. 34 Inductor for heating metal plates and strips. Courtesy of Inductoheat, Inc. Fig. 35 Unique 6000 kW/110 Hz induction coil provides heating of the world's largest steel...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005849
EISBN: 978-1-62708-167-2
... Handling Systems Although the first step to every system is the handling of raw material for delivery to the induction heating system, every induction heating system has a mechanism for feeding the billets through the induction heating coils. Induction billet heaters are classified based on the type...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005854
EISBN: 978-1-62708-167-2
...Abstract Abstract Induction heating system control is straightforward after the design and application of the coil and power supply required for the job. This article provides an overview of the basic components of an induction heating system, including a machine controller (computer...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005897
EISBN: 978-1-62708-167-2
... the critical parameters: workpiece power estimation; estimation of electrical and thermal efficiency of the coil; and frequency selection for heating solid cylinders, tubes, pipes, slabs, plates, strips, and rectangular workpieces. electrical efficiency frequency induction coils induction hardening...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005843
EISBN: 978-1-62708-167-2
... Technology for Medium and High Frequency Applications , Proc. of the 1st Int. Induction Heating Seminar , São Paulo, Brazil , 1995 11. Rudnev V. , Cook R. , Loveless D. , and Black M. , Induction Heat Treatment: Basic Principles, Computation, Coil Construction, and Design...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005842
EISBN: 978-1-62708-167-2
... induction hardening magnetic flux concentrators solenoid coils THE LIFE OF INDUCTION COILS has a certain ending and uncertain timing. The goal of this article is to provide theoretical explanations and practical recommendations that would allow induction heating practitioners and designers...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005924
EISBN: 978-1-62708-166-5
... temperature-control system. IR, infrared. Source: Ref 7 Fig. 14 Schematic circuit diagrams of low- to medium-frequency heat stations illustrating capacitor and transformer adjustments when using (a) an autotransformer for high-impedance induction coils and (b) an isolation transformer for low...
Book Chapter

By J.F. Libsch
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001387
EISBN: 978-1-62708-173-3
... frequent applications ( Ref 5 ). The schematics show the placement of brazing alloy preforms and coil-part arrangements. Joint Parameters Effect of Thermal Expansion on Stress In induction brazing, the heating function is essentially independent of the operator once the generator, coil...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005888
EISBN: 978-1-62708-167-2
... Example of an induction bar/billet heating system that uses four large-size inverters supplying power to 12 inline coils. Courtesy of Inductotherm Heating & Welding Ltd., UK Fig. 22 Conventional surface-to-core temperature profiles of induction system for heating 64 mm (2.5 in.) diameter...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005841
EISBN: 978-1-62708-167-2
..., to aid in pulling the braze alloy into the joint. Inductors (commonly called induction coils or coils) that are used for brazing are similar in many ways to inductors used for induction heat treating. The general differences between inductors designed for heat treating and inductors designed...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003200
EISBN: 978-1-62708-199-3
... and induced currents produced by various induction coils Abstract Abstract This article discusses the fundamentals and applications of localized heat treating methods: induction hardening and tempering, laser surface transformation hardening, and electron-beam heat treatment. The article provides...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005850
EISBN: 978-1-62708-167-2
... induction heating coils power supplies programmable logic controllers quenching MAINTENANCE OF INDUCTION heating systems has long been ignored due to the assumption that “everything is fine as long as good workpieces are produced.” However, there are high costs associated with ignoring routine...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005761
EISBN: 978-1-62708-165-8
... through hardening of steel parts by induction ( Ref 19 ) Section size Material Frequency (a) , Hz Power (b) , kW Total heating time, s Scan time Work temperature Production rate Inductor input (c) Entering coil Leaving coil mm in. s/cm s/in. °C °F °C °F kg/h lb/h kW/cm 2...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005838
EISBN: 978-1-62708-167-2
.... Fig. 18 Heating coil current Fig. 19 Gears processed with simultaneous dual frequency. Courtesy of Inductoheat, Inc. Fig. 29 Induction power supply. Courtesy of Radyne Corporation Fig. 30 Control board. Courtesy of Radyne Corporation Fig. 4 Typical capacitors...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005891
EISBN: 978-1-62708-167-2
... tightly wound turns Fig. 7 Results of computer simulation show an electromagnetic end effect that manifests itself by a distortion of the electromagnetic field at end regions of induction coil. Fig. 8 Normalized surface power density distribution along the length of a heated bar using...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005868
EISBN: 978-1-62708-167-2
... Fig. 1 Typical undercarriage components that are induction hardened Fig. 2 Single-shot induction-hardening system used for track pins. Source: Ref 1 Fig. 3 Induction heating coil for hardening of undercarriage rollers. Source: Ref 1 Fig. 4 Immersion quench...