Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006450
EISBN: 978-1-62708-190-0
..., bridge unbalance system, induction bridge system, and through transmission system. The article concludes with a discussion on the inspection of aircraft structural and engine components. aircraft structures bridge unbalance system coil impedance eddy-current inspection electrical conductivity...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005838
EISBN: 978-1-62708-167-2
... switching devices, namely, silicon-controlled rectifiers, insulated-gate bipolar transistors, and metal-oxide semiconductor field-effect transistors. The article also provides information on frequency-multiplication harmonic-induction power supplies, namely, push-pull and half-bridge inverters and full...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005836
EISBN: 978-1-62708-167-2
...-calculations, human analysis-decisions, multiple system arrangements, and zone control systems for power supply selection. It provides information on the maintenance of induction power supplies, detailing the safety precautions to be taken and the need for routine inspection and servicing. capacitors...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003234
EISBN: 978-1-62708-199-3
... of bridge system is an induction bridge, in which the power signal is transformer coupled into an inspection coil and a reference coil. In addition, the entire inductance-balance system is placed in the probe, as shown in Fig. 12 . The probe consists of a large transmitter (or driver) coil and two small...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005846
EISBN: 978-1-62708-167-2
... Abstract Magnetic flux controllers are materials other than the copper coil that are used in induction systems to alter the flow of the magnetic field. This article describes the effects of magnetic flux controllers on common coil styles, namely, outer diameter coils, inner diameter coils...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005911
EISBN: 978-1-62708-167-2
... augers or shears cutting a viscous stream. For lenses, Gearing invented a precision technique for gobbing glass using induction heating of crucibles and nozzles along with a balance beam weighing system. Controlling the pressure head in the working crucible and synchronizing the heating and cooling...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005899
EISBN: 978-1-62708-167-2
... Abstract This article provides a detailed discussion on the components of a high-performance induction crucible furnace system, namely, furnace body, power supply, and peripheral components. The furnace body contains refractory lining, coil and transformer yokes, and tilting frame and furnace...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006337
EISBN: 978-1-62708-179-5
...—consisting of the furnaces themselves (for the cupola, including holding furnace), the charge makeup, charging and dedusting systems, and for foundations and construction work—are markedly lower for an induction plant. These usually are on the order of half of cupola furnace costs. In terms of operating...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005196
EISBN: 978-1-62708-187-0
... and water cooling systems for induction furnaces. Furnace operators can increase the power supply utilization by the use of mechanical skimmers. The article describes the various lining materials used in induction furnaces, namely, silica, alumina, and magnesia. The crucible wall scrapers, ramming mixes...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005843
EISBN: 978-1-62708-167-2
... Transformers and reactors are critical components in induction heating power supplies and heat stations. With modern power supplies using very efficient semiconductors, the efficiency of the power supply and the heating system are determined largely by the transformers and reactors that are used. A power...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005904
EISBN: 978-1-62708-167-2
... from renewable sources rises. Characteristic features of the two principal melting systems in iron foundries Table 1 Characteristic features of the two principal melting systems in iron foundries Feature Induction furnace Cupola furnace Chemical composition and tapping temperature...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003655
EISBN: 978-1-62708-182-5
... Abstract Corrosion monitoring is important in the operation of modern industrial plants and in the use and maintenance of expensive assets such as bridges and aircrafts, because the damage caused by corrosion and the rate of the deterioration can be huge and the risks devastating. This article...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005840
EISBN: 978-1-62708-167-2
..., bars, and slabs is one of the best applications for this technology, which often is used for warm forming, hot forging, and metal processing. This technology, now widely used in modern induction heating systems, has attained an established position in the industrial workplace and is likely to further...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005924
EISBN: 978-1-62708-166-5
... Abstract Induction heating has many different applications, such as melting, heating stock for forging, and heat treating. This article begins with a discussion on the types of power supplies, namely, solid-state power supplies and oscillator tubes. It provides information on system elements...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005850
EISBN: 978-1-62708-167-2
..., computer systems, water cooling systems, fixtures and machines, air-operated or pneumatic devices, coils, and quench systems. It also presents simple rules that need to be applied while moving the equipment from one location to another. fixtures hardness test equipment hardness testing induction...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005905
EISBN: 978-1-62708-167-2
... stoppage times, the furnace is cooled to room temperature and heated again for restart with a burner run by programmable logic controllers. After tapping, the alloyed melt is transferred from the induction furnace into a ladle furnace, soon to be made ready to pour in a vacuum oxygen decarburization system...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001746
EISBN: 978-1-62708-178-8
... provide vary- The detector is a basic Wheatstone bridge required to provide thorough reduction of the balanced under a helium or oxygen flow. sample. In high-frequency furnace systems, ing results, depending on the amount of inductive capabilities of the material must be surface corrosion. The system...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003039
EISBN: 978-1-62708-200-6
... design factors, and techniques to produce aerodynamic surfaces, improve surface smoothness, and avoid slipping and bridging of filament. The article discusses tooling and the equipment used in the filament winding process, namely, mandrel design, winding machines, tensioners, and ovens. curing...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006445
EISBN: 978-1-62708-190-0
... of discrete parts, a second coil containing a reference can be added to the system; this configuration is called a magnetic bridge comparator. Magnetic Bridge Comparator Testing When a ferromagnetic part is placed in the core of a coil with an alternating current, a unique set of harmonics...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003832
EISBN: 978-1-62708-183-2
... to coat steel bridges rather than TSA. The reasons cited for this are that TSZ is lower in cost and somewhat easier to spray than aluminum or Al-5Mg. The TSZ is also said to be more forgiving of the surface preparation quality. A typical coating system consists of 100 μm (4 mils) of thermal-sprayed zinc...