Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006166
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data hydrogen binary system phase data THIS ARTICLE includes systems where hydrogen is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006209
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data tantalum binary system THIS ARTICLE includes systems where tantalum is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006216
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data vanadium binary system THIS ARTICLE includes systems where vanadium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006208
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data strontium binary system THIS ARTICLE includes systems where strontium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006188
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data neodymium binary system phase data THIS ARTICLE includes systems where neodymium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006215
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data uranium binary system THIS ARTICLE includes systems where uranium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006173
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data lanthanum binary system phase data THIS ARTICLE includes systems where lanthanum is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006187
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data niobium binary system phase data THIS ARTICLE includes systems where niobium is the first-named element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006213
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data phase data titanium binary system THIS ARTICLE includes systems where titanium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006193
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data palladium binary system phase data THIS ARTICLE includes systems where palladium is the first-named...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006189
EISBN: 978-1-62708-163-4
... system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase. binary phase diagrams crystallographic data nickel binary system phase data THIS ARTICLE includes systems where nickel is the first-named element...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002388
EISBN: 978-1-62708-193-1
... mechanisms for SCC. It discusses the materials, environmental, and mechanical factors that control hydrogen embrittlement and SCC behavior of different engineering materials with emphasis on carbon and low-alloy steels, high-strength steels, stainless steels, nickel-base alloys, aluminum alloys, and titanium...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005439
EISBN: 978-1-62708-196-2
... is the constant diffusivity assumption. However, the constant D solutions tend to be robust, and variations in D of 10% would likely be insignificant compared to scatter in experimental data. In the following, four standard solutions to Fick's second law for binary single-phase systems are given...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003836
EISBN: 978-1-62708-183-2
... hydrogen embrittlement and stress-corrosion cracking. hydrogen embrittlement stress-corrosion cracking liquid phase quenching transition metal-metal binary alloys transition metal-metalloid alloys amorphous simple metal-transition metal-rare earth metal alloys AMORPHOUS, or glassy, metal...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003837
EISBN: 978-1-62708-183-2
... Abstract This article reviews the corrosion behavior of intermetallics for the modeling of the corrosion processes and for devising a strategy to create corrosion protective systems through alloy and coating design. It discusses the high-temperature corrosion properties of intermetallics...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005903
EISBN: 978-1-62708-167-2
... for the individual groups of alloys: The binary systems detailed in Fig. 35 to 38 provide an initial reference to the properties of the alloys ( Ref 35 ). The influence of the different alloying metals is described in ( Ref 37 ). The hydrogen solubility of copper and copper alloy melts needs to be considered...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003675
EISBN: 978-1-62708-182-5
... Abstract This article begins with a discussion on the corrosion characteristics of unalloyed magnesium and two major magnesium alloy systems. It shows the effects of iron and 13 other elements on the saltwater corrosion performance of magnesium in binary alloys with increasing levels...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006221
EISBN: 978-1-62708-163-4
... exist as a solid, liquid, and/or gas, depending on the specific combination of temperature and pressure. It describes the accomplishment of conversion between weight percentage and atomic percentage in a binary system by the use of formulas. The article analyzes the effects of alloying on melting...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003620
EISBN: 978-1-62708-182-5
... is obtained in certain binary alloy systems; for example, in the gold alloy and platinum alloy systems, only the alloying element is dissolved. For less noble systems, such as copper-zinc, both elements may undergo dissolution. One of the first mechanisms proposed for the dezincification of brass...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005192
EISBN: 978-1-62708-187-0
... are considerably faster than for nitrogen. If equilibrium between the metal and the gas bubbles leaving the system is assumed, it is possible to calculate the amount of hydrogen that can be removed by gas bubbling from thermodynamic considerations alone. The equations are developed similarly to those for steel...