... Abstract This article focuses on heat treating of the most important H-series and low-alloy hot-work tool steels, namely, normalizing, annealing, stress relieving, preheating, austenitizing, quenching, tempering, and surface hardening. It describes the heat-treating procedure for hot-work tools...
Image
Published: 01 January 2005
Fig. 4 Hot hardnesses of AISI hot-work tool steels. Measurements were made after holding at the test temperature for 30 min. Source: Ref 2 More
Image
Published: 01 December 1998
Fig. 5 Hot hardnesses of AISI hot-work tool steels. Measurements were made after holding at the test temperature for 30 min. More
Image
Published: 01 October 2014
Fig. 1 Tempering curves for the most common hot-work tool steels. Tempering curves are obtained after hardening small (25 mm or 1 in.) specimens of all materials with the usual hardening temperature: 1020 °C for H13, TENAX300 (brand name of low-silicon H11), and VHSUPER (brand name of high More
Image
Published: 01 October 2014
Fig. 8a Effect of temperature on hardness of chromium hot-work tool steels More
Image
Published: 01 October 2014
Fig. 8b Effect of temperature on hardness of tungsten hot-work tool steels More
Image
Published: 01 October 2014
Fig. 8c Effect of temperature on hardness of molybdenum hot-work tool steels More
Image
Published: 01 January 2005
Fig. 5 Resistance of AISI hot-work tool steels to softening during 10 h elevated-temperature exposure as measured by room-temperature hardness. Unless otherwise specified by values in parentheses, initial hardness of all specimens was 49 HRC. Source: Ref 3 More
Image
Published: 01 January 2005
Fig. 17 Amount of wear of hot work tool steels as a function of the number of forgings. Equivalent steels are in parentheses. Source: Ref 29 More
Image
Published: 01 December 1998
Fig. 6 Resistance of AISI hot-work tool steels to softening during 10 h elevated-temperature exposure as measured by room-temperature hardness. Unless otherwise specified by values in parentheses, initial hardness of all specimens was 49 HRC. More
Image
Published: 30 September 2015
Fig. 43 True specific heat of low alloy and hot working tool steels. Squares, low alloy tool steels with 1% ≤ Cr ≤ 2.4% and 0.4% ≤ Mo ≤ 1%; circles, hot working tool steels with around 5% Cr, 1% ≤ Mo ≤ 3% and 0.4% ≤ V ≤ 1.1% More
Image
Published: 01 December 2004
Fig. 31 AISI H13 chromium hot-worked tool steel, spheroidize annealed. 4% picral. 1000× More
Image
Published: 01 January 2002
Fig. 25 Runner block made from a proprietary hot work tool steel that was used to die cast aluminum transmission case covers. Macrograph shows the worn out surface of the die. 0.25×. Close-up views of areas 1 and 2 are shown in Fig. 26 . More
Image
Published: 01 January 2002
Fig. 48 Runner block made from a proprietary hot-work tool steel that was used to die cast aluminum transmission case covers. Macrograph shows the worn out surface of the die. 0.25×. Close-up views of areas 1 and 2 are shown in Fig. 49 . More
Image
Published: 01 December 1998
Fig. 6 Effect of tempering temperature on hardness of type H26 hot-work tool steel for two different tempering temperatures More
Image
Published: 30 August 2021
Fig. 48 Runner block made from a proprietary hot work tool steel that was used to die cast aluminum transmission case covers. Macrograph shows the worn-out surface of the die. Original magnification: 0.25×. Close-up views of areas 1 and 2 are shown in Fig. 49 . More
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001042
EISBN: 978-1-62708-161-0
... Abstract The powder metallurgy (P/M) process has been used primarily for the production of advanced high-speed tool steels. However, the P/M process is also being applied to the manufacture of improved cold-work and hot-work tool steels. The basic heat treatments for P/M high-speed tool steels...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006417
EISBN: 978-1-62708-192-4
... Abstract Tool steels are carbon, alloy, and high-speed steels that can be hardened and tempered to high hardness and strength values. This article discusses the classifications of commonly used tool steels: water-hardening tool steels, shock-resisting tool steels, cold-work tool steels, and hot...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003975
EISBN: 978-1-62708-185-6
... fatigue, and mechanical fatigue. The article describes heat treating practices commonly employed for chromium- and tungsten-base AISI hot-work tool steels. It discusses the fabrication of impression dies, and the advantages and disadvantages of cast dies. The article concludes with a discussion...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003202
EISBN: 978-1-62708-199-3
..., austenitizing, quenching, preheating, and tempering commonly employed in certain steels. These are water-hardening tool steels, shock-resisting tool steels, oil-hardening cold-work tool steels, medium-alloy air-hardening cold-work tool steels, high-carbon high-chromium cold-work tool steels, hot-work tool...