Skip Nav Destination
Close Modal
By
David L. Bourell, Joseph J. Beaman, Jr., Donald Klosterman, Ian Gibson, Amit Bandyopadhyay
Search Results for
hot melts
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1509
Search Results for hot melts
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 01 January 2001
Fig. 3 The fused deposition modeling (FDM) hot melt extrusion process. Courtesy of Penn State University
More
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006039
EISBN: 978-1-62708-172-6
... Abstract Bitumen for coating usage can best be categorized as two fundamental but very different types: asphalts and coal tars. This article provides a detailed discussion on asphalt and coal tar hot-melt applications; asphalt and coal tar emulsions; asphalt and coal tar cutbacks; and coal tar...
Abstract
Bitumen for coating usage can best be categorized as two fundamental but very different types: asphalts and coal tars. This article provides a detailed discussion on asphalt and coal tar hot-melt applications; asphalt and coal tar emulsions; asphalt and coal tar cutbacks; and coal tar epoxies. It reviews the similarities between asphaltic and coal tar coatings and discusses the health and environmental concerns of these materials.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003047
EISBN: 978-1-62708-200-6
... conditions. It then focuses on the characteristics, types, and properties of the five groups of adhesives, such as structural, hot melt, pressure sensitive, water based, ultraviolet, and electron beam cured adhesives. The article also discusses the functions and applications of adhesive modifiers, including...
Abstract
This article begins with an overview of the fundamentals of adhesive technology, including functions, limitations, adhesive joint types, and the key factors in the selection of adhesives, including application, type of joint, process limitation, mechanical requirement, and service conditions. It then focuses on the characteristics, types, and properties of the five groups of adhesives, such as structural, hot melt, pressure sensitive, water based, ultraviolet, and electron beam cured adhesives. The article also discusses the functions and applications of adhesive modifiers, including fillers, adhesion promoters, tackifiers, and tougheners. It gives a short note on functions of primers and primerless bonding. Applications of adhesives in automotive, aerospace, electronics, electrical, medical, sports, and construction sectors are also described. Finally, the article describes the steps in adhesive bonding, including storage and handling of adhesives, bonding preparation, adhesive application, tooling, and curing.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003366
EISBN: 978-1-62708-195-5
... Abstract This article describes the chemistry of phenolic resins and reviews their characteristics and properties for various composites fabrication processes. The fabrication processes include solution/hot-melt process, pultrusion, vacuum infusion, filament winding, sheet molding, and hand lay...
Abstract
This article describes the chemistry of phenolic resins and reviews their characteristics and properties for various composites fabrication processes. The fabrication processes include solution/hot-melt process, pultrusion, vacuum infusion, filament winding, sheet molding, and hand lay-up. The article illustrates the manufacturing process of phenolic honeycomb and provides information on the applications of phenolic composites.
Book Chapter
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003397
EISBN: 978-1-62708-195-5
... Abstract This article reviews various rapid prototyping (RP) processes such as stereolithography, powder sintering, hot melt extrusion, sheet lamination, solid ground curing, and three-dimensional printing. It discusses the various material prototypes produced by RP technology. The list...
Abstract
This article reviews various rapid prototyping (RP) processes such as stereolithography, powder sintering, hot melt extrusion, sheet lamination, solid ground curing, and three-dimensional printing. It discusses the various material prototypes produced by RP technology. The list of materials includes particulate and fiber-reinforced polymers, ceramic-matrix composites, and metal-matrix composites. The article also provides information on freeform-fabrication techniques for composite part lay-up.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005672
EISBN: 978-1-62708-198-6
... of curable adhesives used for medical device assemblies, including acrylics, cyanoacrylates, epoxies, urethanes, and silicones. Other forms of adhesives, such as hot melts, bioadhesives, and pressure-sensitive adhesives, are also discussed. The typical characteristics and applications of biocompatible...
Abstract
This article provides an overview of curing techniques, adhesive chemistries, surface preparation, adhesive selection, and medical applications of adhesives. The curing techniques are classified into moisture, irradiation, heat, and anaerobic. The article highlights the common types of curable adhesives used for medical device assemblies, including acrylics, cyanoacrylates, epoxies, urethanes, and silicones. Other forms of adhesives, such as hot melts, bioadhesives, and pressure-sensitive adhesives, are also discussed. The typical characteristics and applications of biocompatible medical device adhesives are listed in a table. The article concludes with a section on the selection of materials for medical adhesives.
Image
in Wrought and P/M Superalloys
> Properties and Selection: Irons, Steels, and High-Performance Alloys
Published: 01 January 1990
Image
Published: 01 June 2016
Fig. 10 Transformation diagram for vacuum-melted and hot-forged Inconel 718 bar. Source: Ref 12
More
Image
Published: 01 June 2016
Fig. 20 Transformation diagram for vacuum-melted and hot-forged Inconel 718 bar. Source: Ref 12
More
Image
Published: 01 January 1987
Fig. 104 Hot cracking of an electron beam weld due to accidental melting of the copper backing plate. Note the extensive intergranular cracking and the grain-boundary copper film. (a) 4 ×. (b) 13 ×. (c) 68 ×. (d) 340 ×
More
Image
in Metallography and Microstructures of Refractory Metals and Alloys
> Metallography and Microstructures
Published: 01 December 2004
Fig. 11 Niobium alloy C-103 sheet, 1 mm (0.040 in.) thick. Arc melted, hot extruded, warm rolled, and annealed. Cold rolled to finished size. Final annealed in vacuum at 1290 °C (2350 °F) for 1 h. Longitudinal section showing fully recrystallized structure. ASTM grain size 7. Etchant: ASTM 163
More
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003017
EISBN: 978-1-62708-200-6
..., and polyurethane. Additives Pigments are added to powdered resins by either dry blending or hot-melt compounding to obtain a colored part. Dry blending of very fine powdered pigments with powdered resin can give fair color dispersion and acceptable color appearance for many applications. Dry blending...
Abstract
Rotational molding is a simple but unique process that has the capability of producing small to large hollow items with very uniform wall thicknesses. Providing an overview of the operating principles of rotational molding, this article discusses the key selection factors, including function and property requirements for resins and additives; size, shape, design, and cost of molded parts; equipment type and size; and the type of mold to be used. Commonly used molds include cast aluminum, fabricated sheet metal, nickel deposit, machined aluminum, silicone, fiberglass, and prototype molds.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.9781627082075
EISBN: 978-1-62708-207-5
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005299
EISBN: 978-1-62708-187-0
... characteristics, melting practices, melt treatment, and feeding of the molten steel into the mold used in steel foundries. It discusses the features of melting furnaces used in direct arc melting and induction melting. It reviews factors such as wall thickness and designing for avoidance of hot spots. The article...
Abstract
Sand mold and permanent mold casting are the major methods for shape casting of steels, with production closely split among green sand, chemically bonded sand, and permanent mold processes. This article describes key aspects of the steel casting process, including steel solidification characteristics, melting practices, melt treatment, and feeding of the molten steel into the mold used in steel foundries. It discusses the features of melting furnaces used in direct arc melting and induction melting. It reviews factors such as wall thickness and designing for avoidance of hot spots. The article explains the sand casting and permanent mold casting of steel. The process design and casting of thin sections are also discussed.
Book Chapter
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003784
EISBN: 978-1-62708-177-1
... will be established somewhere between the hot melt and the cold wall. The solidification of the casting will then proceed inward, with a more or less uniform isothermal front. The grains that nucleated on the mold wall will elongate in the direction of heat flow, as shown in Fig. 9 , resulting in a columnar grain...
Abstract
Pure metals normally solidify into polycrystalline masses, but it is relatively easy to produce single crystals by directional solidification from the melt. This article illustrates the dislocations present in a metal crystal, which is often polygonized into sub-boundaries during grain growth after solidification. It provides a description of small-angle and large-angle grain boundaries of polycrystalline metals.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005267
EISBN: 978-1-62708-187-0
... Abstract This article describes the melting process of casting metals used in hot chamber die casting. It discusses the design and capabilities of injection components, such as gooseneck, plunger, and cylinder. The article reviews the distinctions between hot and cold chamber processes...
Abstract
This article describes the melting process of casting metals used in hot chamber die casting. It discusses the design and capabilities of injection components, such as gooseneck, plunger, and cylinder. The article reviews the distinctions between hot and cold chamber processes. An example of a typical runner, gate and overflow configuration for faucet fixture casting is shown. Temperature control for die casting is also discussed. The article explains some ejection and post-processing techniques used for the hot chamber die casting: robotics, recycling, and fluxing.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001399
EISBN: 978-1-62708-173-3
... Abstract Hot gas soldering is a process that is commonly used in applications where the workpiece thermal mass is small and the melting temperature of the solder is relatively low. This article describes the characteristics of hot gas heating that are critical to its effectiveness in soldering...
Abstract
Hot gas soldering is a process that is commonly used in applications where the workpiece thermal mass is small and the melting temperature of the solder is relatively low. This article describes the characteristics of hot gas heating that are critical to its effectiveness in soldering. These characteristics include the focus of gas flow, gas flow rates (velocity and volume), gas temperature, and typical gas media. The article explains the thermal profile of a component being soldered and the temperature across adjacent components, which helps to understand time-temperature relationship. It concludes with a discussion on reliability concerns and processing concerns when using hot gas soldering in electronics assembly.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006519
EISBN: 978-1-62708-207-5
... assembled by wax welding using a hot iron or spatula or a small gas flame. The wax at the interface between two components is quickly melted, and the components are pressed together until the wax resolidifies. The joint is then smoothed over. A hot melt adhesive can be used instead of, or in addition...
Abstract
Investment casting, in which molten metal is poured into hot molds, allows for the production of aluminum parts with extremely thin sections, knife edges and sharp detail. This article describes the various steps in the investment casting process, including patternmaking and dimensioning, the design and manufacture of shell molds, melting and casting methods, and postcasting operations such as knockout, core removal, and cleaning. It also addresses a wide range of design considerations, discusses casting defects, and provides several design examples.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005307
EISBN: 978-1-62708-187-0
... the magnesium content, and greater flux additions can make the magnesium disappear completely. Consequently, it is necessary to control temperatures continuously, to flux properly, and to check the analysis. Melt Processing Furnaces In the past, the standard furnace at the hot chamber zinc die casting...
Abstract
This article describes the control of alloy composition and impurity levels in die casting of zinc alloys based on agitation, use of foundry scrap, and melt temperature and fluxing. It reviews the process considerations for the melt processing of the zinc alloys. The process considerations include the usage of furnaces and launder system, scrap return, inclusions in zinc alloys, fluxing of zinc alloys, and galvanizing fluxes. The article discusses the materials and lubricant selection, casting and die temperature control, and trimming process used in hot chamber die casting for zinc alloys. It also reviews other casting processes for zinc alloys, such as sand casting, permanent mold casting, plaster mold casting, squeeze casting, and semisolid casting.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001007
EISBN: 978-1-62708-161-0
... Abstract This article describes ironmaking and steelmaking practices (melt or liquid processing, including hot metal desulfurization) and discusses the evolution of these processes and their effects on steel properties. The physical chemistry of steelmaking may appear deceptively simple...
Abstract
This article describes ironmaking and steelmaking practices (melt or liquid processing, including hot metal desulfurization) and discusses the evolution of these processes and their effects on steel properties. The physical chemistry of steelmaking may appear deceptively simple for integrated steel mill operations where ore from the ground is converted into steel. The various refining steps that occur in steelmaking are reviewed. The article also describes solid processing of steel, with emphasis on hot and cold rolling, thermomechanical processing, and annealing of flat steel products.