1-20 of 457

Search Results for hot dip coating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 2003
Fig. 1 Basic arrangement of the coating bath in a continuous hot-dip coating operation More
Image
Published: 01 January 1994
Fig. 3 Schematic of pot region in a typical continuous hot dip coating line More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003688
EISBN: 978-1-62708-182-5
... Abstract This article describes the basic principles, processing steps, and benefits of continuous hot dip coatings. It provides useful information on the principal types of coatings applied in the hot-dip process. The types of coatings include galvanized coatings, galvannealed coatings, 55Al...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001270
EISBN: 978-1-62708-170-2
... considered in this article include metal coatings, such as zinc coatings, and alloy coatings, such as zinc-iron, types 1 and 2 aluminum, Zn-5AI, Zn-55AI, and lead-tin coatings. aluminum coatings continuous hot dip coatings ferrous metals lead-tin alloycoatings microstructure steel sheet surface...
Image
Published: 01 January 2003
Fig. 10 Microstructure of the coating and alloy layer of a hot-dip coated type 1 aluminized steel sheet More
Image
Published: 01 January 2003
Fig. 11 Microstructure of the coating and alloy layer of hot-dip coated type 2 aluminized sheet More
Image
Published: 01 January 1994
Fig. 8 Corrosion losses of hot dip coatings in the industrial environment of Bethlehem, PA. Source: Ref 18 More
Image
Published: 01 January 2003
Fig. 2 Schematic drawing of the cross section of a hot-dip coated sheet product showing the three features of all hot-dip coated sheet products—the outer coating layer, the intermetallic alloy bond zone, and the steel sheet substrate More
Image
Published: 01 December 1998
Fig. 2 Corrosion losses of hot-dip coatings in the industrial environment of Bethlehem, PA More
Image
Published: 01 January 1997
Fig. 2 Corrosion losses of hot dip coatings in the industrial environment of Bethlehem, PA. Source: Ref 13 More
Image
Published: 01 January 1990
Fig. 4 Photomicrograph of a typical hot dip galvanized coating. The molten zinc is interlocked into the steel by the alloy reaction, which forms zinc-iron layers and creates a metallurgical bond. 250× More
Image
Published: 01 August 2013
Fig. 6 Schematic diagram of the pot region of a continuous hot dip metal coating line. Schematic redrawn based on Ref 2 and 3 More
Image
Published: 01 January 1994
Fig. 1 Photomicrograph of typical hot dip galvanized coating. The molten zinc is interlocked into the steel by the alloy reaction, which forms zinc-iron layers and creates a metallurgical bond. See Table 3 for properties of alloy layers. 250× More
Image
Published: 01 January 1994
Fig. 4 Typical hot dip galvanized coating. Note the gradual transition from layer to layer, which results in a strong bond between base metal and coating. More
Image
Published: 01 January 1994
Fig. 5 Service life versus coating thickness for hot dip galvanized steel in various atmospheres. Source: Ref 8 More
Image
Published: 01 January 1994
Fig. 6 Time to first maintenance versus coating thickness for hot dip galvanized coatings in seawater immersion and sea spray exposures. Source: Ref 11 More
Image
Published: 01 January 2003
Fig. 2 Service life versus coating thickness for hot dip galvanized steel in various atmospheres. Service life is defined as the time to 5% rusting of the steel surface. More
Image
Published: 01 January 2003
Fig. 3 Time to first maintenance versus coating thickness for hot dip galvanized coatings in seawater immersion and sea spray exposures. Source: Ref 13 More
Image
Published: 01 December 1998
Fig. 1 Typical hot-dip galvanized coating. Note the gradual transition from layer to layer, which results in a strong bond between base metal and coating. More
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001272
EISBN: 978-1-62708-170-2