1-9 of 9 Search Results for

horizontal broaching

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001231
EISBN: 978-1-62708-170-2
... Abstract This article focuses on precision and ultraprecision finish machining techniques that make use of defined cutting edges, such as polycrystalline diamond and cubic boron nitride compacts. The techniques are finish turning, finish broaching, finish milling, and finish drilling...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003189
EISBN: 978-1-62708-199-3
... variations in the tool geometry and workpiece material will change the severity of the machining operation. For heavy-duty machining operations (such as tapping or broaching), medium- or heavy-duty cutting oils are generally used. Horizontal broaching of steel usually requires a heavier bodied or more...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001233
EISBN: 978-1-62708-170-2
... Simple cavities 2.2 0.085 19 × 10 3 mm 2 (30 in. 2 ) faces 1.3 0.050 Broaching (angled ECM) 7.6 0.300 Accurate estimates of feed rates usually require pilot testing in the desired ECM configuration. Electrolyte conductivity also affects resistance across the gap. Increasing the...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
... cores. Hydraulic wax injection machines are sized according to their clamping force capability, with models ranging in capacity from 9.1 to 363 Mgf (10 to 400 tonf) or more. Machines for manual or semiautomatic operation generally have horizontal platens that clamp the die closed (one stationary, one...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003988
EISBN: 978-1-62708-185-6
... such as fracture toughness and fatigue strength. The lateral flow also imparts some mechanical anisotropy due to grain flow. The stress state during hot repress powder forging consists of a small difference between vertical and horizontal stresses, which results in very little metal movement in the...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005323
EISBN: 978-1-62708-187-0
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.9781627081863
EISBN: 978-1-62708-186-3
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001243
EISBN: 978-1-62708-170-2
... work should be hung as nearly vertical as possible, with the lower edge of the work tilted from the horizontal to permit runoff at a corner rather than a whole edge. When recessed areas cannot be racked to allow proper runoff, provision should be made for drain holes or perhaps tilting of the rack when...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.9781627081979
EISBN: 978-1-62708-197-9