1-20 of 103 Search Results for

high-performance liquid chromatography

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 30 September 2015
Fig. 35 Ion chromatography high-performance liquid chromatography technique. Source: Ref 11 More
Image
Published: 30 September 2015
Fig. 33 High-performance liquid chromatography separation of components. Source: Ref 10 More
Image
Published: 30 September 2015
Fig. 34 (a) High-performance liquid chromatography equipment. (b) Example of data generated by this technique. Courtesy of KTA-Tator, Inc. More
Image
Published: 15 May 2022
Fig. 2 (a) High-performance liquid chromatography chromatogram from isocratic separation of TPA, MHET and BHET. (b) Formation of halos on agar plates containing PET, BHET, and PCL. Images were taken after incubation with purified and recombinant PET30 enzyme for 24 hours (unpublished data More
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006636
EISBN: 978-1-62708-213-6
... Abstract This article describes high-performance liquid chromatography and ultra-high-performance liquid chromatography that are used to separate and quantify the chemical components in any sample that can be dissolved in a liquid. This includes pharmaceutical drugs, medicinal plant extracts...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001776
EISBN: 978-1-62708-178-8
..., and describes the experimental procedure of and sample preparation for GC/MS. The article also discusses complementary techniques, such as high-performance liquid chromatography/mass spectrometry and mass spectrometry/mass spectrometry, and concludes with the applications of GC/MS. chemical analysis gas...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003432
EISBN: 978-1-62708-195-5
... to control the rate of reaction. The article describes the component material tests, mixed resin system tests, and prepreg tests for the resin system. These tests include high-performance liquid chromatography, infrared spectroscopy, and gel permeation chromatography. The article contains a table that lists...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001777
EISBN: 978-1-62708-178-8
... the conditions necessary for high-speed analysis. Modern liquid column chromatography, now called high-performance liquid chromatography (HPLC) or simply liquid chromatography (LC), was made possible by technical advances in equipment, columns, and column packing materials. As a result of these advances, LC...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006063
EISBN: 978-1-62708-172-6
... attached to GC-MS instruments for coating analysis. A GC-MS instrument is shown in Fig. 32 . Fig. 32 Gas chromatography-mass spectroscopy instrument. Courtesy of KTA-Tator, Inc. High-Performance Liquid Chromatography (HPLC) High-performance liquid chromatography (HPLC) comprises a wide...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006945
EISBN: 978-1-62708-395-9
... polyethylene heat-de ection temperature high-impact polystyrene high-strength sheet molding compound high-performance liquid chromatography high-pressure polyethylene high-speed liquid chromatography International Electrotechnical Commission butyl rubber (or isobutylene-isoprene rubber) infrared; synthetic...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006849
EISBN: 978-1-62708-395-9
... to contrast one against another. Molecular Weight Determination from Viscosity The principal methods of molecular weight (MW) determination are based on viscosity measurements and chromatography. The latter includes gel permeation chromatography (GPC) and high-performance liquid chromatography (HPLC...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006652
EISBN: 978-1-62708-213-6
... Abstract This article introduces various analytical techniques commonly used in the characterization of organic solids and liquids and discusses the challenges in performing the analysis, with examples. Some general advice in approaching a material analysis is also provided. organic...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0005693
EISBN: 978-1-62708-178-8
... (spectroscopy) GC gas chromatography GC-IR gas chromatography-infrared (spectroscopy) GC/MS gas chromatography/mass spectrometry GFAAS graphite furnace atomic absorption spectrometry HPLC high-performance liquid chromatography IC ion chromatography ICP-AES...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006659
EISBN: 978-1-62708-213-6
... is wound into a coil and housed in a temperature-controlled oven. The column is coated with a stationary phase that is a solid (or a liquid supported on a solid). Chromatography also requires a mobile phase, which can be a liquid or a gas that flows past the stationary phase and carries the components...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001778
EISBN: 978-1-62708-178-8
... chromatography and are equipped with spectrophotometric detectors. Conductivity detectors have been designed to attach to existing high-performance liquid chromatographs, and columns packed with the proper ion exchange resins are commercially available. An instrument designed solely for single-column ion...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006630
EISBN: 978-1-62708-213-6
... chromatographic media ( Ref 17 ). While C18 bonded phase silica is the most common reversed phase material used in high-performance liquid chromatography (HPLC), the extreme pH conditions of IC make such materials unsuitable for use in IC. Instead, the most common chromatographic material used in ion pair...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0006515
EISBN: 978-1-62708-200-6
... stress-intensity ETFE ethylene tetrafluoroethylene eV electron volt HM high modulus factor EVA ethylene vinyl acetate HMC high-strength molding compound kg kilogram hp horsepower f fiber kIn kilometer HP high performance I focal length; frequency kN kilonewton In normal load HPLC high-performance liquid...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001745
EISBN: 978-1-62708-178-8
... include Shpol'skii spectrometry ( Ref 17 ) and Fourier transform/NMR spectroscopy ( Ref 18 ). A suitable alternative to spectroscopic methods is gas chromatography (for the more volatile hydrocarbons) or high-performance liquid chromatography (HPLC) (for the polynuclear aromatic hydrocarbons). Gas...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003441
EISBN: 978-1-62708-195-5
... Ply thickness Fiber volume HPLC, high-performance liquid chromatography; GPC, gel permeation chromatography; RDS, rheometric dynamic scanning; DSC, differential scanning calorimetry; ARC, accelerated rate calorimeter; TGA, thermogravimetric analysis A typical BMI could contain a bis F...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006678
EISBN: 978-1-62708-213-6
... … Gas chromatography/mass spectrometry N N V • V V V V … … V V V V … High-temperature combustion N … … … … … N N … … N N N … … Image analysis … … … … … … … • • … … … … … • Inductively coupled plasma mass spectrometry...