DOI: 10.31399/asm.hb.mhde2.a0003202
EISBN: 978-1-62708-199-3
..., austenitizing, quenching, preheating, and tempering commonly employed in certain steels. These are water-hardening tool steels, shock-resisting tool steels, oil-hardening cold-work tool steels, medium-alloy air-hardening cold-work tool steels, high-carbon high-chromium cold-work tool steels, hot-work tool...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005973
EISBN: 978-1-62708-168-9
... high-chromium tool steels, and high-vanadium-powder metallurgy tool steels. The article also describes the properties, types, nominal compositions and designations of these cold-work tool steels. air-hardening cold work tool steel carbon content chromium hardenability hardening hardness...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003114
EISBN: 978-1-62708-199-3
... blast or by interrupted quenching in hot oil. High-Carbon, High-Chromium, Cold-Work Steels High-carbon, high-chromium, cold-work steels (group D) contain 1.50 to 2.35% C and 12% Cr. With the exception of type D3, they also contain 1% Mo. All group D tool steels except type D3 are air hardening...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001041
EISBN: 978-1-62708-161-0
... tools, massive sections should be hardened by cooling in an air blast or by interrupted quenching in hot oil. High-Carbon, High-Chromium, Cold-Work Steels High-carbon, high-chromium, cold-work steels (group D) contain 1.50 to 2.35% C and 12% Cr; with the exception of type D3, they also contain 1...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005946
EISBN: 978-1-62708-168-9
... and low-alloyed (water- and oil-hardening, shock-resistant) cold work tool steels: W-, S-, O-, L-, as well as 6F-type Medium- and high-alloy (air-hardening, high-carbon and high-chromium) cold work tool steels: A-, D- (including powder metallurgy and new ∼8% Cr steels), as well as 6F-type Hot work...