1-20 of 608

Search Results for high strength sand-casting alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006588
EISBN: 978-1-62708-210-5
... Abstract Alloy 713.0 is an aluminum-based casting alloy that ages at room temperature to provide high-strength sand and permanent-mold castings. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006589
EISBN: 978-1-62708-210-5
... Abstract Alloys 771.0 and 772.0 are high-strength, shock-resistant, aluminum sand-casting alloys that develop a high combination of physical and mechanical properties in the as-cast and room-temperature-aged conditions. This datasheet provides information on key alloy metallurgy, processing...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006568
EISBN: 978-1-62708-210-5
... impact energy hardness curves high-strength casting alloys mechanical properties physical properties Alloys 356.0 and A356.0 ( Table 1 ) are used in sand and permanent mold casting and provide excellent strength with good elongation and excellent corrosion resistance. The alloys provide...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006567
EISBN: 978-1-62708-210-5
..., and application characteristics of these 3xxx series alloys. aluminum alloy 355.0 aluminum alloy C355.0 fabrication characteristics heat treatment high-strength alloys mechanical properties physical properties Used in sand and permanent mold (PM) casting, alloys 355.0 and C355.0 ( Table 1...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006580
EISBN: 978-1-62708-210-5
... silicon content of 5 wt% with various limits on iron, copper, manganese and magnesium ( Table 1 ). They are hypoeutectic AI-Si binary alloys with high ductility, very good corrosion resistance, good machinability, but only fair castability, and low strength. The alloys are used in castings where above...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
... thinner than those obtainable by sand or permanent mold casting. High mechanical properties and resistance to fatigue can be developed in die castings without heat treatment because of the fine microstructures produced by the rapid solidification. Alloys most frequently used in die casting differ...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006586
EISBN: 978-1-62708-210-5
... alloy. fabrication characteristics highly stressed castings mechanical properties natural-aging aluminum alloys physical properties sand casting Alloy 710.0 ( Table 1 ) is a natural-aging aluminum alloy produced by sand casting. It develops high-mechanical properties without a quenching...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006558
EISBN: 978-1-62708-210-5
... Typical tensile properties of separately cast test bars of alloy 242.0-T571 at elevated temperature, after 10 4 hours of exposure Temperature Tensile strength Yield strength Elongation in 50 mm (2 in.), % °C °F MPa ksi MPa ksi Sand cast 24 75 220 32 205 30 0.5 150 300...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
... casting, is also included. alloying elements aluminum casting alloys high-pressure die casting low-pressure permanent mold casting permanent mold casting green sand casting investment casting castability ALUMINUM CASTINGS have played an integral role in the growth of the aluminum...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006533
EISBN: 978-1-62708-207-5
... periods. Chemical Binders Chemical binders, which are resins that can be used to glue the sand grains together, are more common in the foundry industry, and aluminum castings use many types of chemical binders. The advantages of the chemical binder systems include high strength, ease of handling...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006577
EISBN: 978-1-62708-210-5
... have excellent wear resistance coupled with good mechanical properties, high hardness, and low coefficients of expansion, high thermal conductivity, good elevated temperature strength and hardness, and very good castability. Corrosion resistance is fair. It is used mainly as a substitute for gray cast...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006584
EISBN: 978-1-62708-210-5
... aluminum alloy 520.0 magnesium sand-casting alloys mechanical properties physical properties Alloy 520.0 contains nominally 10% magnesium ( Table 1 ) and is typically sand cast. It is characterized by an excellent combination of machinability, strength, ductility and resistance to corrosion...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006562
EISBN: 978-1-62708-210-5
... alloys improve ductility, tensile strength, and fatigue life. These alloys offer good strength in the as-cast condition and they are often used this way. However, it is possible to increase strength considerably by heat treatment. In applications which see high temperatures, as in engine components...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006559
EISBN: 978-1-62708-210-5
... Abstract Alloy 295.0 is an Al-Cu-Si alloy suitable for sand casting requiring high strength with ductility and toughness. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003134
EISBN: 978-1-62708-199-3
... to the case with which an alloy responds to ordinary foundry practice without requiring special techniques for gating, risering, melting, sand conditioning, or any of the other factors involved in making good castings. High fluidity often ensures good castability, but it is not solely responsible...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006578
EISBN: 978-1-62708-210-5
... 0.20 Al bal bal bal Typical mechanical properties of separately cast test bars of the 391 type alloys Table 2 Typical mechanical properties of separately cast test bars of the 391 type alloys Alloy Casting method and temper Tensile strength, (MPa (ksi) Yield strength, (MPa (ksi...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
...-copper alloys can and have been successfully used to produce high-strength and high-ductility castings. More exacting casting techniques are also helpful and required when casting other single-phase aluminum casting alloys or alloy systems. In terms of alloy additions, manganese in small amounts may...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006569
EISBN: 978-1-62708-210-5
... characteristics of Al-Si-Mg high-strength casting alloys. aluminum alloy 357.0 aluminum-silicon-magnesium alloys fabrication characteristics high-strength casting alloys mechanical properties physical properties Alloy 357.0 is similar to alloy 356.0, but it has a larger amount of magnesium, which...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001062
EISBN: 978-1-62708-162-7
... others (total) max, bal Al Consequence of Exceeding Impurity Limits High iron or silicon decreases tensile properties. Applications Typical Uses Sand castings, permanent mold and investment castings. Structural casting members, aerospace housings, electrical transmission line fittings...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006561
EISBN: 978-1-62708-210-5
... Abstract Alloy 308.0 is an Al-Si-Cu alloy used in sand and permanent mold casting. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of this alloy. aluminum alloy 308.0 cast...