1-20 of 1330 Search Results for

heat-resistant titanium-base alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003728
EISBN: 978-1-62708-177-1
... Abstract This article describes the development of heat-resistant titanium-base alloys and their classification into several microstructure categories based on their strengthening mechanisms. It explains the phase transformation in titanium-aluminum-base alloys and two peritectic reactions...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001430
EISBN: 978-1-62708-173-3
... Abstract This article discusses the weldability characteristics of cobalt-base corrosion-resistant (CR) alloys, titanium-base CR alloys, zirconium-base CR alloys, and tantalum-base CR alloys that assist in the selection of suitable alloy and welding method for producing high-quality welds...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001416
EISBN: 978-1-62708-173-3
... Abstract This article focuses on the physical metallurgy and weldability of four families of titanium-base alloys, namely, near-alpha alloy, alpha-beta alloy, near-beta, or metastable-beta alloy, and titanium based intermetallics that include alpha-2, gamma, and orthorhombic systems...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003623
EISBN: 978-1-62708-182-5
.... It also reviews the considerations for selected nonferrous alloy systems such as aluminum, titanium, tantalum, and nickel. corrosion resistance alloy composition shielding molten hot metal surface welding parameter weldments nonferrous alloy system aluminum titanium tantalum nickel...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003814
EISBN: 978-1-62708-183-2
... easily be categorized by elemental base. aluminum copper corrosion resistance nickel nonferrous metals titanium NONFERROUS METALS AND ALLOYS are widely used to resist corrosion. At one end of the spectrum, they are used for water piping and food preparation. At the other end...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003160
EISBN: 978-1-62708-199-3
... will recover its shape upon heating above its transformation temperatures. Examples of martensitic devices include vibration dampers, bendable surgical tools for open heart surgery, and highly fatigue resistant wires. Copper-Base Alloys Compositions and Properties Commercial copper-base shape memory...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004003
EISBN: 978-1-62708-185-6
... Processing As with nickel-base superalloys, TMP routes have been developed to provide dual (and graded) microstructures in alpha-beta titanium alloys ( Ref 31 , 38 ). Most of these methods comprise local heating of selected regions of a part above the beta transus followed by controlled cooling...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001492
EISBN: 978-1-62708-173-3
... types of engineering materials considered in the selection of a brazing process. The engineering materials include low-carbon steels, low-alloy steels, and tool steels; cast irons; aluminum alloys; copper and copper alloys; nickel-base alloys; heat-resistant alloys; titanium and titanium alloys...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001080
EISBN: 978-1-62708-162-7
... Abstract Titanium has been recognized as an element with good mechanical and physical properties, alloying characteristics, and corrosion resistance. Providing an outline of general characteristics and types of titanium alloys, this article discusses the contemporary technology of titanium...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001453
EISBN: 978-1-62708-173-3
... the elements at the surface Nickel Flashing Certain heat-resistant alloys that are used as base metals in brazed assemblies—particularly nickel-base alloys containing high percentages of aluminum and titanium (such as Inconel 718)—may require a surface pretreatment to ensure maintenance...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001456
EISBN: 978-1-62708-173-3
... brazed with Ti-28V-4Be, was resistant to potassium vapor and liquid exposed for 1000 h at 815 °C (1500 °F). Honeycomb structures of Nb alloys were evaluated using Pd-30Cu and Ti-11Cr-13V-3Al brazing filler alloys. There was some erosion with the palladium alloy, but the titanium-base alloy produced...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001415
EISBN: 978-1-62708-173-3
... metallurgy titanium titanium alloys welding defects weldability TITANIUM is a low-density element (approximately 60% of the density of steel) that can be highly modified by alloying and deformation processing. Titanium is nonmagnetic and has good heat transfer properties. Its coefficient of thermal...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0009239
EISBN: 978-1-62708-173-3
..., properties, and potential heat treatment of titanium base alloys are presented in tables. The article provides information on brazed joints of titanium with carbon steels, as well as ceramics and graphite. It discusses the risks involved in titanium brazing, including erosion of base metal, brittle...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003210
EISBN: 978-1-62708-199-3
... such as diffusion and exothermic brazing. The article explains joint design, filler materials, fuel gases, equipment, and fluxes in the brazing methods. The article also describes the brazing of steels, stainless steels, cast irons, heat-resistant alloys, aluminum alloys, copper and copper alloys, and titanium...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005644
EISBN: 978-1-62708-174-0
...-hardened alloys. Susceptible to heat-affected zone cracking Titanium alloys Commercially pure grades and alpha alloys TIG, MIG, electron beam, resistance pressure, flash butt Weld in annealed condition Stress relieve 400–650 °C (750–1200 °F) Highly reactive, requires good shielding. No filler...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001428
EISBN: 978-1-62708-173-3
... their respective carbides. Although chromium depletion may occur in the HAZ of welds, as it does with the iron-base alloys in the absence of titanium or columbium, it is only in extremely corrosive media that corrosion resistance is impaired. Manganese Manganese was considered to be relatively unimportant...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005884
EISBN: 978-1-62708-167-2
..., this class of metals has good corrosion resistance. The ability to resist corrosion comes from the formation of an adherent chromium oxide film on the surface of the metal. This film is very thin but it prevents the degradation of the base iron that is normally encountered in other ferrous-based alloys...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003184
EISBN: 978-1-62708-199-3
... Abstract This article reviews specific processing characteristics and forging-related properties of commonly forged families of metals and alloys, including carbon and alloy steels, stainless steels, heat-resistant alloys (iron, cobalt, and nickel base alloys), aluminum alloys, copper...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006406
EISBN: 978-1-62708-192-4
... of the various constituents in the case can be modified by changes in the base alloy content, carbon content, and thermal treatment. It is possible to optimize the martensite/austenite/carbide ratio to achieve maximum wear resistance for particular environments. Fig. 3 Micrograph of a high-carbon (≈0.85...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003140
EISBN: 978-1-62708-199-3
...%. Titanium alloys have been employed in submarine hulls and submersible research vehicles. Because of favorable heat-transfer behavior, thermal stability, and corrosion resistance, titanium is being used in heat exchangers for power generation. Corrosion resistance also is a factor in the selection...