1-20 of 669 Search Results for

heat-resistant gray iron

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006344
EISBN: 978-1-62708-179-5
... used heat-resistant gray irons suitable for elevated-temperature service are presented in a table. cast iron chemical composition compacted graphite iron cooling rate ductile iron foundry gray iron heat-resistant gray iron malleable iron mechanical properties notch sensitivity...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006308
EISBN: 978-1-62708-179-5
... characteristics and machinability of a gray iron casting. The article also presents typical mechanical properties of heat-resistant gray irons in a table. It concludes with information on the automotive application of alloy cast irons. carbon ductility elasticity gray iron gray iron casting heat...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001006
EISBN: 978-1-62708-161-0
... irons, and heat-resistant cast irons. This article discusses abrasion-resistant chilled and white irons, high-alloy corrosion-resistant irons, and medium-alloy and high-alloy heat-resistant gray and ductile irons. The article outlines in a list the approximate ranges of alloy content for various types...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006348
EISBN: 978-1-62708-179-5
... to poor tolerances or may be operated with occasional lubricant starvation or without maintenance. For good wear resistance, gray cast iron should be pearlitic with randomly distributed graphite flakes. Cast irons have been heat treated to obtain martensitic structures for use as cylinder liners...
Book Chapter

Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006416
EISBN: 978-1-62708-192-4
... they may be made to poor tolerances or may be operated with occasional lubricant starvation or without maintenance. For good wear resistance, gray cast iron should be pearlitic with randomly distributed graphite flakes. Cast irons have been heat treated to obtain martensitic structures for use as cylinder...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001303
EISBN: 978-1-62708-170-2
...-chromium iron 1.2–4.0 0.3–1.5 0.15 0.15 0.5–3.0 5.0 12–35 4.0 3.0 M,A Nickel-chromium gray iron (g) 3.0 0.5–1.5 0.08 0.12 1.0–2.8 13.5–36 1.5–6.0 1.0 7.5 A Nickel-chromium ductile iron (h) 3.0 0.7–4.5 0.08 0.12 1.0–3.0 18–36 1.0–5.5 1.0 … A Heat-resistant gray...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005970
EISBN: 978-1-62708-168-9
..., including austenitic gray irons and austenitic ductile irons. It also provides a discussion on the heat treatment of high-silicon irons for heat resisting and corrosion resisting applications. austenitic ductile iron austenitic gray iron corrosion resistance heat treatment high-alloy graphitic...
Book: Casting
Series: ASM Handbook