Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003196
EISBN: 978-1-62708-199-3
... Abstract This article describes the heat treating (stress relieving, normalizing, annealing, quenching, tempering, martempering, austempering, and age hardening) of different types of steels, including ultrahigh-strength steels, maraging steels, and powder metallurgy steels. Tabulating the...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005782
EISBN: 978-1-62708-165-8
... Abstract Stress-relief heat treating of steel is the uniform heating of a structure to a suitable temperature below the transformation range, holding at this temperature for a predetermined period of time, followed by uniform cooling. This article provides information on the sources of residual...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003195
EISBN: 978-1-62708-199-3
... Abstract This article presents an outline of the physical metallurgical principles that are associated with heat treating of steels. It describes the iron-carbon phase diagram and various types of transformation diagrams, including isothermal transformation diagrams, continuous heating...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001279
EISBN: 978-1-62708-170-2
... permanent deformation or creep of steel due to its own weight during enamel firing. The sag resistance of steel is related to its strength at elevated temperatures and to the temperature at which the steel starts to transform from ferrite to austenite on heating. In general, the higher the strength and the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
... Abstract Heat treating of stainless steel produces changes in physical condition, mechanical properties, and residual stress level and restores maximum corrosion resistance when that property has been adversely affected by previous fabrication or heating. This article focuses on annealing of...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003202
EISBN: 978-1-62708-199-3
... Abstract All tool steels are heat treated to develop specific combinations of wear resistance, resistance to deformation or breaking under loads, and resistance to softening at elevated temperature. This article describes recommended heat treating practices, such as normalizing, annealing...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.9781627081689
EISBN: 978-1-62708-168-9
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006269
EISBN: 978-1-62708-169-6
... atoms such as molybdenum and aluminum was observed during plasma nitriding of titanium α + β alloys ( Ref 16 , 64 , 65 ). The high nitriding temperature of titanium α + β alloys permits the use of it in lieu of the heat treating processes such as quenching and aging as well as cyclic treatment ( Ref...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006250
EISBN: 978-1-62708-169-6
... hardened by heat treatment. Only a relatively small portion of the total number of nonferrous alloys responds significantly to hardening by heat treatment (see also the article “Heat Treatable Nonferrous Alloys” in this Volume). The most common heat treating procedure for hardening of nonferrous alloys...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003201
EISBN: 978-1-62708-199-3
... Abstract Cast irons may be compared with steels in their reactions to hardening. However, because cast irons (except white iron) contain graphite and substantially higher percentages of silicon, they require higher austenitizing temperatures. This article describes the effect of heat treatment...