1-20 of 239 Search Results for

heat treatable steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005645
EISBN: 978-1-62708-174-0
... of heat treatable steels, namely, low-alloy steels and ultra high-strength steels. carbon steel heat treatable steel interpass temperature low-alloy steels pipe welds postweld heat treatment preheat temperature pressure vessels ultra high-strength steels Recommended preheat and interpass...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001404
EISBN: 978-1-62708-173-3
... steels. The article describes six general classes of the metal: low-carbon steels, high-strength low-alloy steels, quenched-and-tempered steels, heat-treatable low-alloy steels, thermal-mechanical-controlled processing steels, and chromium-molybdenum steels. It concludes with an illustration of steels...
Image
Published: 01 January 2005
Fig. 22 Tensile-strength losses for (a) low-carbon steel and (b) representative non-heat-treatable aluminum alloys at several atmospheric exposure sites. Strength losses of the aluminum alloys are less than one-tenth that of the low-carbon steel More
Image
Published: 15 June 2019
Fig. 22 Tensile strength losses for (a) low-carbon steel and (b) representative non-heat-treatable aluminum alloys at several atmospheric exposure sites. Strength losses of the aluminum alloys are less than one-tenth that of the low-carbon steel. More
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001447
EISBN: 978-1-62708-173-3
... near the bond line and may also act as dry lubricants that reduce frictional heating. Heat-treatable steels also can be friction welded. The rapid quenching of the weld area can present hardenability problems and a subsequent tempering or annealing procedure may be required. Hardenable steels...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001455
EISBN: 978-1-62708-173-3
... Abstract Aluminum, a commonly used base material for brazing, can be easily fabricated by most manufacturing methods, such as machining, forming, and stamping. This article outlines non-heat-treatable wrought alloys typically used as base metals for the brazing process. It highlights chloride...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005596
EISBN: 978-1-62708-174-0
... directional properties near the bondline and may also act as dry lubricants that reduce frictional heating. Heat treatable steels also can be friction welded. The rapid quenching of the weld area can present hardenability concerns, and a subsequent tempering or annealing procedure may be required. Hardenable...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006529
EISBN: 978-1-62708-207-5
... alloys that can be brazed as base metals are listed in Table 1 . These include non-heat treatable and heat-treatable wrought alloys, as well as some casting alloys. Non-heat-treatable alloys include high-purity aluminums and those with low additions of alloying elements. Table 2 provides major...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001417
EISBN: 978-1-62708-173-3
... Abstract Aluminum alloys, particularly the heat-treatable alloys, are sensitive to weld cracking. Anticipation of these characteristics and general knowledge of these materials assist in selection of suitable method for welding heat-treatable aluminum alloys. This article provides a general...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006510
EISBN: 978-1-62708-207-5
..., mainly in the general factors associated with service weldability (fitness). The article also provides a discussion on the selection and weldability of non-heat-treatable aluminum alloys, heat treatable aluminum alloys, aluminum-lithium alloys, and aluminum metal-matrix composites. aluminum alloys...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006528
EISBN: 978-1-62708-207-5
... treatable. Because of its higher strength, 6061 alloy has better handling characteristics before and during porcelain enameling, and it is stronger after porcelain enameling. The non-heat-treatable alloys are easier to form before porcelain enameling and are used for small parts for which the amount...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006509
EISBN: 978-1-62708-207-5
... reflectors 2 xxx Al-Cu-(Mg, Li) Heat treatable 2024, 2219, 2618, 2090 The major alloying element is copper or copper with magnesium or lithium. Provides mechanical properties similar to mild steel but has limited corrosion resistance and is especially prone to intergranular corrosion. Typical...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001436
EISBN: 978-1-62708-173-3
... when heated; and its wide range of mechanical properties and melting temperatures that result from alloying with other metals. Various property values are provided in Tables 1 , 2 , 3 , and 4 . Composition, physical properties, and weldability of selected non-heat-treatable wrought aluminum...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005887
EISBN: 978-1-62708-167-2
... properties similar to mild steel Limited corrosion resistance and especially prone to intergranular corrosion Examples: 2024, 2219, 2618, 2090 3<italic>xxx</italic> Series—Al-Mn(-Mg) Alloys Non-heat-treatable alloys containing manganese as the major alloying element. Trace elements...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001433
EISBN: 978-1-62708-173-3
... describes the various categories of low-alloy steels, such as high-strength low-alloy (HSLA) structural steels, high-strength low-alloy quenched and tempered(HSLA Q&amp;T) structural steels, low-alloy steels for pressure vessels and piping, medium-carbon heat-treatable (quenched and tempered) low-alloy...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006274
EISBN: 978-1-62708-169-6
..., cobalt alloys, zinc alloys, and heat treatable silver alloys, gold alloys, lead alloys, and tin alloys. It also provides a detailed discussion on the effects due to precipitation and transformation processes in these non-ferrous alloys. aluminum alloys copper copper alloys heat treatment...
Image
Published: 01 January 1994
, and M1A Solution Type of solution Constituents Amount, g/L (oz/gal) Operating temperature, °C (°F) Cycle time, min Tank material 1 Alkaline cleaner (a) (a) 88–100 (190–212) 3–10 Low-carbon steel 2 Cold rinse Water … Ambient (b) Low-carbon steel 3 Acid pickle (c More
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005963
EISBN: 978-1-62708-168-9
... )/2 Low-Alloyed Boron Steel Boron, in the presence of C-Mn-Mo-Cr, increases the hardenability to many times that of unalloyed steel ( Ref 18 ). Many grades in these categories are heat treatable boron-containing steels ( Table 4 ) with improved hardness and wear properties. The critical...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006285
EISBN: 978-1-62708-169-6
...) after working or between successive stages of working or customer forming processes. In principle, all deformed aluminum alloys lose some of their (strain-hardening) strength when heated or tested at higher temperatures (&gt;200 °C, or 390 °F). However, there are specific differences for heat treatable...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005266
EISBN: 978-1-62708-187-0
... casting is a term commonly used to refer to a die casting process in which liquid alloy is cast without turbulence and gas entrapment and subsequently held at high pressure throughout the freezing cycle to yield high-quality heat treatable components. Direct squeeze casting originally was developed...