Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006128
EISBN: 978-1-62708-175-7
..., austenitizing, and vacuum heat treatment. It explains the result of these tempering processes with HSS M2 grade of HATS. austenitizing heat treatment high-potential high-alloy tool steels martensitic microstructure salt bath heat treatment secondary-hardening high-alloy tool steel tempering vacuum...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003762
EISBN: 978-1-62708-177-1
.... carbonitrided steel carburized steel case hardening steel etching grinding metallography microstructure mounting nitrided steel polishing sectioning specimen preparation DIFFUSION of alloying elements for surface hardening of steels includes various thermochemical treatments ( Table 1...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005771
EISBN: 978-1-62708-165-8
... Abstract Surface hardening improves the wear resistance of steel parts. This article focuses exclusively on the methods that involve surface and subsurface modification without any intentional buildup or increase in part dimensions. These include diffusion methods, such as carburizing...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005788
EISBN: 978-1-62708-165-8
... Abstract Inverse hardening a steel of adequate hardenability requires a workpiece of sufficiently large cross section, an appropriate cooling medium, and the right quenching conditions. This article explains the Temperature Gradient Quenching Analysis System (TGQAS), which can measure, record...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005817
EISBN: 978-1-62708-165-8
... Abstract Electron beam hardening (EBH), with some special characteristics in comparison to other heat treatment technologies, allows beam deflection frequencies of up to 100 kHz. This article illustrates the principles of different thermal electron beam technologies, including beam-deflection...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005807
EISBN: 978-1-62708-165-8
... Abstract Flame hardening is a heat treating process in which a thin surface shell of a steel part is heated rapidly to a temperature above the critical temperatures of the steel. The versatility of flame-hardening equipment and the wide range of heating conditions obtainable with gas burners...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005773
EISBN: 978-1-62708-165-8
... carbide coating, and low-temperature salt bath nitride coating. carbides coating fluidized-beds hardening nitrides nucleation salt baths steel surface hardening Introduction The thermoreactive deposition and diffusion (TRD) process is a heat-treatment-based method to form coatings...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005761
EISBN: 978-1-62708-165-8
... in a workpiece is explained, with emphasis on the skin effect. The article discusses typical procedures for induction hardening of steel, namely, austenitizing and quenching to form martensite either on the surface (case hardening) or through the entire section (through hardening). It briefly describes induction...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005808
EISBN: 978-1-62708-165-8
... Abstract Laser surface hardening is a noncontact process that provides a chemically inert and clean environment as well as flexible integration with operating systems. This article provides a brief discussion on the various conventional surface-modification techniques to enhance the surface...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005864
EISBN: 978-1-62708-167-2
... Abstract This article describes the common types of automotive and truck axle shafts. It provides information on steels used for induction-hardened shafts, and on the manufacturing and induction hardening methods of axle shafts. The article discusses the effects of case depth, shaft length...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005865
EISBN: 978-1-62708-167-2
... Abstract Induction heat treatment is a common method for hardening and tempering of crankshafts, which are necessary components in almost every internal combustion engine for cars, trucks, and machinery, as well as pumps, compressors, and other devices. Similar to crankshafts, camshafts also...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005868
EISBN: 978-1-62708-167-2
... Abstract Induction heat treating is used in the off-road machinery industry for hardening steel and cast iron components used in a wide range of applications. This article focuses on the usage of induction hardening components in the industry, and discusses the basic requirements of steel...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005869
EISBN: 978-1-62708-167-2
... Abstract Induction hardening of geared parts used in aeronautic and aerospace industry is an important technology because of its one-piece flow, repeatability, energy efficiency, and tighter control of surface distortion than conventional carburizing. This article describes the requirements...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005867
EISBN: 978-1-62708-167-2
... Abstract Induction hardening is a prominent method in the gear manufacturing industry due to its ability of selectively hardening portions of a gear such as the flanks, roots, and/or tips of teeth with desired hardness, wearing resistance, and contact fatigue strength without affecting...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005859
EISBN: 978-1-62708-167-2
... Abstract This article focuses on induction hardening process for heat treating operations specifically designed to result in proper microstructure/property combinations in either localized or in the final parts. It briefly reviews the heat treating basics for conventional heat treating...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005863
EISBN: 978-1-62708-167-2
... Abstract Induction hardening of steel components is the most common application of induction heat treatment of steel. This article provides a detailed account of electromagnetic and thermal aspects of metallurgy of induction hardening of steels. It describes induction hardening techniques...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006268
EISBN: 978-1-62708-169-6
... Abstract This article describes the effects of alloying and heat treatment on the metastable transition precipitates that occur in age hardenable aluminum alloys. Early precipitation stages are less well understood than later ones. This article details the aging sequence and characteristics...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005934
EISBN: 978-1-62708-166-5
... Abstract Successful hardening depends on the hardenability of steel composition, the geometry of parts, the quenching system, and on the heat treating process used. This article provides a brief overview of the computation and use of quench factor analysis (QFA) to quantify as-quenched hardness...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005951
EISBN: 978-1-62708-168-9
... Abstract Case hardening involves various methods and each method has unique characteristics and different considerations in the selection of steels  This article reviews the various grades of carburizing steels, carbonitriding steels, nitriding steels, and steels for induction, or flame...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005959
EISBN: 978-1-62708-168-9
... Abstract Low-temperature surface hardening is mostly applied to austenitic stainless steels when a combination of excellent corrosion performance and wear performance is required. This article provides a brief history of low-temperature surface hardening of stainless steel, followed...