1-20 of 150 Search Results for

grinders

Sort by
Image
Published: 01 January 1989
Fig. 22 Use of the wheel face in double-disk grinders to machine the surface while the workpieces, sandwiched between two abrasive disks (top and side view of each setup is shown), traverse along a straight line or in an arcuate path. (a) Parts to be machined are pushed in and retracted More
Image
Published: 01 January 1989
Fig. 25 Creep-feed grinders with ball-screw drives to ensure rigidity More
Image
Published: 01 December 1998
Fig. 5 Single and dual belt grinders for rough grinding More
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003169
EISBN: 978-1-62708-199-3
... Abstract Ores, which consist of the primary valuable mineral, predominant gangue content, valuable by-products, and detrimental impurities, are extracted and directed to mineral processing. This article describes the mineral processing facilities, such as crushers, grinders, concentrators...
Image
Published: 01 January 1987
Fig. 29 Fatigue fracture of sand-cast gray iron bread-crumb grinder. The ASTM A159 part was machined and hot dip galvanized after casting. Also, a lockpin hole (not visible) was drilled through the casting in a region containing type C, size 3 graphite flakes. Cause of failure was traced More
Image
Published: 01 January 1994
Fig. 16 Schematic of backstand grinder having coated abrasive belts for use in off-hand rough grinding operations More
Image
Published: 01 August 2013
Fig. 2 Surface grinder for flat surfaces More
Image
Published: 01 August 2013
Fig. 3 Cylindrical or outer-diameter grinder used on outer diameters of cylinders between centers More
Image
Published: 01 August 2013
Fig. 4 Centerless grinder for grinding outer diameters of cylinders without the use of centers More
Image
Published: 01 August 2013
Fig. 5 Internal or inner-diameter grinder for grinding the inner diameters of cylinders with a small wheel on a shaft at high revolutions per minute More
Image
Published: 01 August 2013
Fig. 6 Jig grinder used for intricate shapes and holes with high degree of accuracy More
Image
Published: 01 August 2013
Fig. 30 Schematic of a metallographic grinder. Source: Ref 31 More
Image
Published: 01 January 1989
Fig. 12 Effect of speed ratio on a creep-feed grinder. Going from positive to negative roll per wheel speed direction increases the normal force and the power. Workpiece was 4340 steel at 50 HRC. It was ground with a 38A801-D25VX514 abrasive wheel dressed with a 30/40 mesh reverse-plated More
Image
Published: 01 January 1989
Fig. 16 Front view (a) and side view (b) of a backstand grinder having coated abrasive belts for use in offhand rough grinding operations More
Image
Published: 01 January 1989
Fig. 36 Universal center-type grinder equipped for grinding a steep taper More
Image
Published: 01 December 2004
Fig. 23 A portable handheld disk sander/grinder. Thin abrasive cut-off wheels can be used to remove a “boat” sample. More
Image
Published: 31 August 2017
Fig. 23 Fatigue fracture of sand cast gray iron bread crumb grinder. The ASTM A159 part was machined and hot dip galvanized after casting. Also, a lock pin hole (not visible) was drilled through the casting in a region containing type C, size 3 graphite flakes. Cause of failure was traced More
Image
Published: 01 December 1998
Fig. 6 Laboratory flush mounted semi-automatic grinder/polisher system More
Image
Published: 01 December 1998
Fig. 11 An automatic single-specimen grinder/polisher More
Image
Published: 01 December 1998
Fig. 12 A semi-automatic grinder/polisher More