... Abstract This article provides background information on the chemistry, coating properties, resin types, applications techniques, and performance characteristics of fluoroethylene vinyl ether (FEVE) resins. It describes the formulation methods of FEVE resins, namely, solvent-based coating...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003213
EISBN: 978-1-62708-199-3
... Abstract Metal surfaces must often be cleaned before subsequent operations to remove unwanted substances such as pigmented drawing compounds, unpigmented oil and grease, chips and cutting fluids, polishing and buffing compounds, rust and scale, and miscellaneous contaminants. The article...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... installation of the protective coating/lining system. Prior to beginning surface-preparation operations, many specifications will require a presurface-preparation inspection to verify the correction of fabrication defects and removal of surface contamination such as grease, oil, cutting compounds, lubricants...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... Abstract This article reviews the steps involved in presurface-preparation inspection: substrate replacement; removal of weld spatter, rounding of sharp edges, and grinding of slivers/laminations; and removal of rust scale, grease, oil, and chemical (soluble salt) contamination. It focuses on...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001221
EISBN: 978-1-62708-170-2
... Abstract This article describes the basic attributes of the most widely used metal surface cleaning processes to remove pigmented drawing compounds, unpigmented oil and grease, chips, cutting fluids, polishing and buffing compounds, rust and scale from steel parts, and residues and lapping...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006044
EISBN: 978-1-62708-172-6
... structure and properties when they are formulated into coatings, and how they are being used in coatings. The main discussion points are the differences between solventborne and waterborne technologies and some of the challenges in formulating and applying waterborne acrylic coatings. The article describes...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006015
EISBN: 978-1-62708-172-6
... coatings in appliance industries, furniture industries, computer industries, fixture industries, architectural industries, automotive industries, agriculture and construction equipment industries, recreational equipment industries, and general industries. Powder coating formulations consist of binder...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006008
EISBN: 978-1-62708-172-6
... coating due to the many potential factors that may be involved. These could include formulation, surface preparation, application, drying and curing times and conditions, and environmental exposure, with more than one contributing factor often being involved. Failures and defects can manifest themselves...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003809
EISBN: 978-1-62708-183-2
... corrosion protection of steel structures are discussed, as are the prepainting process, the primary differences between prepaint formulations, the essential considerations about part design, and the selection criteria for the appropriate paint system. More detailed information on organic coating materials...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001227
EISBN: 978-1-62708-170-2
... process in which a solution of a mineral acid, organic acid, or acid salt, in combination with a wetting agent and detergent, is used to remove oxide, shop soil, oil, grease, and other contaminants from metal surfaces, with or without the application of heat. The distinction between acid cleaning and acid...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001276
EISBN: 978-1-62708-170-2
...-containing materials. A rust-preventive compound can consist of only one or a combination of these four basic parts: a carrier, a film former, polar materials, and specialty additives. For example, the rust protection offered by film formers, such as grease, petrolatum, and low-melting...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006014
EISBN: 978-1-62708-172-6
...) 500-03 surface-preparation descriptions Standard Title Description NAPF 500-03-01 “Solvent Cleaning” Shall result in the surface being free of all oil, small deposits of asphalt paint, grease, soil, drawing and cutting s, and other soluble contaminants from iron surfaces. NAPF 500-03...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
... Rough polishing Cloth (a) 2100 23 80-grit silicon carbide 29 None or light application of grease stick Final polishing Cloth (a) 2100 30 220-grit Al 2 O 3 49 Grease stick Spot polishing Cloth (a) 2100 46 220-grit Al 2 O 3 77 Grease stick General buffing Spiral-sewn...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003221
EISBN: 978-1-62708-199-3
... organic finishes. Anodic coatings are porous and provide no corrosion protection unless sealed with a paint. NICKEL ALLOYS do not require special techniques or precautions for removing shop soils such as soap, drawing compound, oil, grease, cutting fluid, and polishing compound. Oxide...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001226
EISBN: 978-1-62708-170-2
...) to remove a variety of contaminants from parts immersed in aqueous media. The contaminants can be dirt, oil, grease, buffing/polishing compounds, and mold release agents, just to name a few. Materials that can be cleaned include metals, glass, ceramics, and so on. Ultrasonic agitation can be used...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001273
EISBN: 978-1-62708-170-2
... constituents added to render the grease soluble. Proprietary cleaners are recommended because they are formulated to deal with specific types of contaminants and basis metal. The temperature of alkaline solutions should not be below 85 °C (185 °F). A simple 5% sodium hydroxide solution at 80 to 90 °C (185 to...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001315
EISBN: 978-1-62708-170-2
..., or dipped in, the hot solvent and then subjected to vapor degreasing to remove the last traces of grease and compound. This method is effective provided that adequate measures are taken to remove the fine abrasive and metallic particles from the parts ( Ref 5 ). Emulsion cleaners can be used to...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003048
EISBN: 978-1-62708-200-6
... solutions to typical engineering sealant problems. Although adhesives and sealants are often formulated from the same types of polymeric materials, they are usually designed to have different properties. Adhesives typically have high tensile and shear strengths and are used to replace or...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003047
EISBN: 978-1-62708-200-6
... joints between dissimilar metals. They may also act as vibration dampers. The mechanical damping characteristics of an adhesive can be changed by formulation. However, changing such a property in an adhesive generally produces change in other properties of the joint, such as tensile or shear strength...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001222
EISBN: 978-1-62708-170-2
... of metals. Soils removed by alkaline cleaning include oils, grease, waxes, metallic fines, and dirt. Alkaline cleaners are applied by either spray or immersion facilities and are usually followed by a warm water rinse. A properly cleaned metal surface optimizes the performance of a coating that is...