1-20 of 420 Search Results for

grain boundaries

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005422
EISBN: 978-1-62708-196-2
... Abstract This article reviews network models and their applications for the simulation of various physical phenomena related to grain-boundary migration. It discusses the steps involved in the implementation of two and three-dimensional network models, namely, acquisition and discretization of...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004018
EISBN: 978-1-62708-185-6
... Abstract Plastic deformation can occur in metals from various mechanisms, such as slip, twinning, diffusion creep, grain-boundary sliding, grain rotation, and deformation-induced phase transformations. This article emphasizes on the mechanism of slip and twinning under cold working conditions...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003995
EISBN: 978-1-62708-185-6
... effectively stop recrystallization by pinning the austenite grain boundaries. Thus, strain is accumulated in the subsequent passes. If a large amount of strain is accumulated, the austenite grains become greatly elongated, hence the term “pancaked” austenite. Perhaps more important than this morphological...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003993
EISBN: 978-1-62708-185-6
...) it is common, in forgings, to process precipitation-hardening superalloys within a restricted temperature range so that not all of the precipitating elements are in solution during forging, thus causing pinning of grain boundaries and restriction of grain growth. The forging conditions must be chosen...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000601
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of pure irons and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the grain-boundary cavitation; slip lines; intergranular...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000607
EISBN: 978-1-62708-181-8
...-type spring, railroad rail, and seamless drill pipe. driveshaft fatigue crack propagation fatigue fracture fractograph grain boundaries high-carbon steel hydrogen embrittlement microstructure springs Fig. 245 Surface of a fatigue fracture that occurred, after 732 h of service, in...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000608
EISBN: 978-1-62708-181-8
... horizontal tail-actuator shafts, bucket elevators, aircraft propellers, helicopter bolts, air flasks, tie rod ball studs, and spiral gears. aircraft landing gears alloy steel corrosion fatigue crack nucleation crankshafts ductile fracture fatigue fracture fractograph grain boundaries hydrogen...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005428
EISBN: 978-1-62708-196-2
... Abstract The misorientation of a boundary of a growing grain is defined not only by its crystallography but also by the crystallography of the grain into which it is growing. This article focuses on the Monte Carlo Potts model that is typically used to model grain growth, Zener-Smith pinning...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004020
EISBN: 978-1-62708-185-6
... in fine-grain metals has encompassed many ideas, such as the diffusional creep, dislocation creep with diffusional accommodation at grain boundaries, and concepts of grain-mantle deformation. The article concludes with information on the kinetics of superplastic deformation processes, including low...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000617
EISBN: 978-1-62708-181-8
... fracture, grain boundaries, notch and fatigue precrack, dimpled rupture, and fatigue striations of these alloys. fractograph intergranular fracture nickel alloys Fig. 867 Surface of a fracture in a bend-test specimen of Nickel 201 containing 0.02% C, 0.35% Mn, 0.01% S, 0.35% Si, 0.25% Cu...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000613
EISBN: 978-1-62708-181-8
...-overload fractures, impact fractures, microstructure, quench cracking, brittle-in-service failure, hydrogen embrittlement, stress-corrosion cracking, and grain-boundary cracking of tool steel components. These components include diesel engine injector plungers, rivet-heading tools, circular saw blades, and...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000621
EISBN: 978-1-62708-181-8
..., tension-overload fracture surface, ductile fracture, cone-shaped fracture surface, intergranular crack propagation, transgranular crack propagation, stress-corrosion cracking, hydrogen damage, and grain-boundary separation of these alloys. Fractographs are also provided for a forged aircraft main-landing...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000610
EISBN: 978-1-62708-181-8
... candy fracture, cleavage fracture, brittle fracture, high-cycle fatigue fracture, fatigue striations, hydrogen-embrittlement failure, creep crack propagation, fatigue crack nucleation, intergranular creep fracture, torsional overload fracture, stress-corrosion cracking, and grain-boundary damage of...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006777
EISBN: 978-1-62708-295-2
... Abstract This article briefly reviews the factors that influence the occurrence of intergranular (IG) fractures. Because the appearance of IG fractures is often very similar, the principal focus is placed on the various metallurgical or environmental factors that cause grain boundaries to...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006781
EISBN: 978-1-62708-295-2
..., temperature-assisted grain-boundary evolution, and temperature-driven surface oxidation, among other things. This article discusses some of the major aspects and challenges of dealing with TMF life prediction. It describes the damage mechanisms of TMF and covers various experimental techniques to promote TMF...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004019
EISBN: 978-1-62708-185-6
... lower energy level. All three processes involve diffusion and thus depend on thermal activation to cause rearrangement of dislocations and grain boundaries. The mechanisms of recovery and recrystallization also depend on the extent of plastic deformation (either during hot working or by cold work prior...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005207
EISBN: 978-1-62708-187-0
... observed between Al 3 Ti and aluminum. For TiB 2 and aluminum, the reported results differ on detection of a consistent orientation relationship, as noted in Table 1 . In addition, boride particles have often been observed to be located at grain boundaries rather than within grain centers, which suggests...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003248
EISBN: 978-1-62708-199-3
... grain size, austenite grain size, and prior-austenite grain size. Each type presents particular problems associated with revealing these boundaries so that an accurate rating can be obtained ( Ref 5 ). To complicate matters, a variety of parameters are utilized to define grain size: Average grain...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005403
EISBN: 978-1-62708-196-2
... phenomenological approach, the mesoscale (or grain scale) models take the basic physical mechanisms into account, that is, strain hardening and dynamic recovery, nucleation, grain-boundary migration, and the associated softening effects. Their main advantage, however, is to predict both flow stress and...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005432
EISBN: 978-1-62708-196-2
... neighborhood definitions. (a) von Neumann neighborhood. Note the strong dependence of the orientation of grain boundaries on the neighborhood definition. (b) Modified-Moore neighborhood. Simulations times are arbitrary time steps. In many cases, a CA simulation of recrystallization uses periodic boundary...