1-20 of 167 Search Results for

gas-lubricated bearings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001273
EISBN: 978-1-62708-170-2
... steel pressing or bushing, or a bronze or iron casting. The bonded bimetal material is shaped and machined to make plain, fluid film lubricated bearings for a wide variety of automotive, industrial, and marine applications. Babbitt is used in small bearings for high-volume applications, such as...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
... along z -axis under Hertzian contact Fig. 5 Subsurface stress under rolling contact The life prediction of rolling-element bearings is based on a statistical analysis of bearing tests performed in a controlled environment (e.g., full-film lubrication, dust free). Given that the...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003134
EISBN: 978-1-62708-199-3
... properties; one example of such an alloy is C94700 (88Cu-5Sn-2Zn-5Ni). Copper alloys have long been used for bearings because of their combination of moderate-to-high strength, corrosion resistance, and self-lubrication properties. The choice of an alloy depends on the required corrosion resistance and...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003061
EISBN: 978-1-62708-200-6
... valve components, rolling elements and bearings, paper and wire manufacturing, biomedical implants, heat exchangers, adiabatic diesel engines, advanced gas turbines, and aerospace applications. advanced ceramics aerospace applications mineral processing equipment structural applications...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003091
EISBN: 978-1-62708-199-3
... Abstract This article presents a detailed account on the process flow, composition, alternative sources, and the advancement of ironmaking, steelmaking and secondary steelmaking practices. Some steels, such as bearing steels, heat-resistant steels, ultrahigh strength missile and aircraft steels...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001227
EISBN: 978-1-62708-170-2
.... Electrolytic acid cleaning followed the alkaline treatment to ensure removal of the phosphate coating and residual lubricant. Because of scrubbing action by the gas evolved at the work surface, the electrolytic bath assisted in removing adherent solid particles that were the residue of a polishing compound...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003818
EISBN: 978-1-62708-183-2
... behavior on soft solders, pewter, bearing alloys, tin-copper alloys, and tin-silver alloys. It reviews the influence of corrosion on immersion tin coating, tin-cadmium alloy coatings, tin-cobalt coatings, tin-copper coatings, tin-lead coatings, tin-nickel coatings, and tin-zinc coatings. The general...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005665
EISBN: 978-1-62708-198-6
... Abstract This article highlights corrosion resistance and ion release from main transition metallic bearings that are used as medical devices. It discusses the main issues associated with the in vivo presence of ions and their biocompatibility during the exposure of patients to different...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003135
EISBN: 978-1-62708-199-3
... industry dates back to the 1920s, when commercial porous bronze bearings were developed independently in the research laboratories of General Motors Corp. and Bound-Brook Oilless Bearing Co. These self-lubricating bearings still account for the major portion of P/M copper and copper alloy applications...
Book Chapter

By Peter J. Blau
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003242
EISBN: 978-1-62708-199-3
... by three independent methods. Tests involved sliding polished aluminum bronze blocks against a rotating bearing steel ring in argon gas. Wear was assessed by weight change, the depth of the wear scar (using a mechanical stylus), and optical microscope measurement of the width of the wear scar. Four...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001276
EISBN: 978-1-62708-170-2
... furniture, and bearing industries, products are used not only as rust preventives, but as lubricants. In the steel industry, a rust-preventive compound is put on the surface of steel that has been pickled after hot rolling. This compound, which is usually compatible with the cold-rolling oil, sometimes...
Book Chapter

By David V. Neff
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005353
EISBN: 978-1-62708-187-0
...) , the rounded porosity would suggest gas evolution during final stages of solidification and hence could very well be caused by hydrogen, However, further microscopic investigation may be necessary, since this porosity may also be caused by entrapped air or lubricant decomposition. In actual practice...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005678
EISBN: 978-1-62708-198-6
... synovial joint exhibits the features of many engineering plain bearings. It consists of layers of bearing material (articular cartilage) ted on relatively hard bones forming the skeletal frame ( Fig. 1 ). The lubricant (synovial fluid) is a water-based fluid containing an additive (hyaluronic acid) that...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003219
EISBN: 978-1-62708-199-3
... protection and aluminum and silver as solid lubricants. Electron beam/physical vapor deposition (EB/PVD) is widely used in the gas turbine industry for applying MCrAlY metallic coatings on turbine blades and vanes for oxidation and corrosion protection. Zirconia thermal barrier coatings (TBCs) can also be...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006789
EISBN: 978-1-62708-295-2
... propellers; high-speed lubricated sliding bearings Corrosive wear Wear conjoint with corrosion, as in a metal bushing versus a shaft immersed in water Rolling wear occurs when two bodies roll one over the other. Some sliding always occurs in the contact region. Wear may occur by rolling-sliding...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
... characteristic reddish-brown debris of ferric oxide, which, when mixed with oil or grease, produces debris that is often referred to as “blood,” “cocoa,” or “red mud.” Hence, in components that are lubricated so that ordinary corrosion is not likely to occur, the presence of reddish-brown debris is indicative of...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004006
EISBN: 978-1-62708-185-6
... Abstract Hot extrusion is a process in which wrought parts are formed by forcing a heated billet through a shaped die opening. This article discusses nonlubricated and lubricated hot extrusion. The two nonlubricated hot extrusion methods are forward or direct extrusion and backward or indirect...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003012
EISBN: 978-1-62708-200-6
... Abstract Additives for plastics and elastomers are used to increase the ease of processing and to improve the properties of the final product. Additives improve processing characteristics by increasing lubricity and by stabilizing the polymer. Additives that improve properties include those...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0005586
EISBN: 978-1-62708-170-2
... austenite on cooling ARE activated reactive evaporation ARIP activated reactive ion plating ARP Aerospace Recommended Practice ASLE American Society of Lubrication Engineers (former name of STLE) ASM American Society for Metals (now ASM International) ASME American...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005258
EISBN: 978-1-62708-187-0
... produce selectively graded composite castings such as graphite or silicon carbide particulates segregating the inner surfaces of copper alloy bearings and bushings to provide lubrication and/or wear resistance of the inner surface while maintaining high strength and toughness of the outer shell. Similar...