1-20 of 341 Search Results for

gas tungsten arc cutting

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005176
EISBN: 978-1-62708-186-3
.... It concludes with information on the seldom-used electric arc cutting methods, such as shielded metal arc cutting, gas metal arc cutting, and gas tungsten arc cutting. air carbon arc cutting arc cutting electric arc cutting ferrous metals gas metal arc cutting gas tungsten arc cutting gouging...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005647
EISBN: 978-1-62708-174-0
... FRW friction welding FS furnace soldering ft foot FW flash welding g gram g acceleration due to gravity gf gram force GMA gas metal arc GMAC gas metal arc cutting GMAW gas metal arc welding GPa gigapascal GTA gas tungsten arc GTAC gas tungsten arc...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0005663
EISBN: 978-1-62708-173-3
... to produce NACE National Association of Corrosion En- gf gram force GMA gas-metal arc stress-corrosion cracking gineers GMAC gas-metal arc cutting km kilometer NASA National Aeronautics and Space Ad- GMAW gas-metal arc welding kN kilonewton GPa gigapascal kPa kilopascal ministration GTA gas-tungsten arc ksi...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005646
EISBN: 978-1-62708-174-0
... A nonstandard term for cutting tip. cutting tip The part of an oxygen cutting torch from which the gases issue. cutting torch (arc) A device used in air carbon arc cutting, gas tungsten arc cutting, and plasma arc cutting to control the position of the electrode, to transfer current, and to con- trol the ow...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.9781627081740
EISBN: 978-1-62708-174-0
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005643
EISBN: 978-1-62708-174-0
... metal welding, small-diameter pipe Gas cutting Oxyacetylene/oxygen flame … Oxygen jet injected through flame oxidizes and ejects metal along the cutting line Oxygen Carbon and low-alloy steel … Cutting and bevelling plate for welding; general engineering applications Gas tungsten arc...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.9781627081733
EISBN: 978-1-62708-173-3
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005590
EISBN: 978-1-62708-174-0
... Abstract The gas tungsten arc welding (GTAW) process derives the heat for welding from an electric arc established between a tungsten electrode and the part to be welded. This article provides a discussion on the basic operation principles, advantages, disadvantages, limitations...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001484
EISBN: 978-1-62708-173-3
... Abstract Plasma arc cutting (PAC) is an erosion process that utilizes a constricted arc in the form of a high-velocity jet of ionized gas to melt and sever metal in a narrow, localized area. This article discusses the process description, equipment, gases, operating sequence, process...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001356
EISBN: 978-1-62708-173-3
... Abstract The melting temperature necessary to weld materials in the gas-tungsten arc welding (GTAW) process is obtained by maintaining an arc between a tungsten alloy electrode and a workpiece. This article discusses the advantages and limitations and applications of the GTAW process...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006515
EISBN: 978-1-62708-207-5
... ALUMINUM AND ITS ALLOYS can be welded by several methods. The primary methods used are the gas-shielded arc welding processes, mainly gas tungsten arc welding (GTAW) and gas metal arc welding (GMAW). Other arc welding processes include arc stud welding, plasma arc welding, and shielded metal arc...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006133
EISBN: 978-1-62708-175-7
... are relatively easy to machine while tungsten and rhenium are much more difficult. A prime advantage of WHAs over pure tungsten is their ability to be machined to complex geometries using common metalworking tools and techniques. Cutting forces are generally higher for machining refractory metals than...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001441
EISBN: 978-1-62708-173-3
... Abstract Zirconium and its alloys are available in two general categories: commercial grade and reactor grade. This article discusses the welding processes that can be used for welding any of the zirconium alloys. These include gas-tungsten arc welding (GTAW), gas-metal arc welding (GMAW...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006561
EISBN: 978-1-62708-210-5
... oil in milling, sawing, and drilling. Joining Gas or electric-arc welding can be applied. For gas welding, an oxyhydrogen flame is preferred. Inert-gas shielded-metallic arc welding is preferred, using either a non-consumable tungsten electrode or a consumable electrode. The use of flux-coated...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005174
EISBN: 978-1-62708-186-3
... arc cutting, and laser cutting. The article concludes with information on the advantages of abrasive waterjet cutting, which is an alternative to laser cutting, gas cutting, and plasma cutting. abrasive waterjet cutting band saws electric arc cutting gas cutting laser cutting mechanical...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005635
EISBN: 978-1-62708-174-0
... arc and flux cored arc welding … … Less than 60  7 … … …  60–160 10 11 … … 160–250 10 12 … … 250–500 10 14 Gas tungsten arc welding … … Less than 50  8 10 … …  50–150  8 12 … … 150–500 10 14 Air carbon arc cutting  Light … … Less than 500 10...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006391
EISBN: 978-1-62708-192-4
... processes. The arc welding processes include shielding metal arc welding, gas metal arc welding/flux cored arc welding, gas tungsten arc welding, submerged arc welding, and plasma transferred arc welding. The article also reviews various factors influencing the selection of the appropriate hardfacing...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005712
EISBN: 978-1-62708-171-9
...-corrosion Hydrotransport screens, crusher teeth, cutting edges Tungsten carbide cermets HVOF Low-stress abrasion, erosion-corrosion Pumps (a) GMAW, gas metal arc welding; SAW, submerged arc welding; FCAW, flux-cored arc welding; PTAW, plasma-transferred arc welding; HVOF, high-velocity oxyfuel...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005622
EISBN: 978-1-62708-174-0
... Abstract Penetration-enhanced gas tungsten arc welding (GTAW) processes have been referred to variously as flux tungsten inert gas (TIG), A-TIG, and GTAW with a penetration-enhancing compound. This article provides a discussion on the principles of operation, advantages, disadvantages...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001487
EISBN: 978-1-62708-173-3
... bonding arc welding brazing compressed gas handling cutting electric shock electrical safety electron-beam welding explosion welding eye protection face protection friction welding high-frequency welding laser-beam welding oxyfuel gas welding protective clothing resistance welding safety...