1-20 of 544 Search Results for

galvanic properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001268
EISBN: 978-1-62708-170-2
..., metallic dust or powder, promoter or accelerator chemicals, and water. It offers a straightforward alternative method for achieving desired mechanical and galvanic properties with an extremely low risk of hydrogen embrittlement. This article provides a detailed description of the equipment, process steps...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003689
EISBN: 978-1-62708-182-5
...Properties of alloy layers to hot dip galvanized steels Table 1 Properties of alloy layers to hot dip galvanized steels Layer Alloy Iron, % Melting point Crystal structure Diamond pyramid microhardness (vickers scale) Alloy characteristics °C °F Eta Zinc 0.03 419 787...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001272
EISBN: 978-1-62708-170-2
... 3.27 55.30 17.0 Source: Ref 1 Properties of alloy layers of a hot dip galvanizing coating Table 3 Properties of alloy layers of a hot dip galvanizing coating Layer (a) Composition Hardness, DPN Iron, % Melting Temperature °C °F Eta Zn 70 0 454 850 Zeta FeZn...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001077
EISBN: 978-1-62708-162-7
... incorporated into ASTM B 750 ( Table 2 ) and Galvalume into ASTM A 792. Additional information on strip galvanizing is available in the article “Precoated Steel Sheet” in Properties and Selection: Irons, Steels, and High-Performance Alloys, Volume 1 of ASM Handbook, formerly 10th Edition Metals Handbook...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003137
EISBN: 978-1-62708-199-3
...Guide to corrosion of copper alloys Table 1 Guide to corrosion of copper alloys Form of attack Characteristics Preventive measures General thinning Uniform metal removal Select proper alloy for environmental conditions based on weight loss data Galvanic corrosion Corrosion...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003216
EISBN: 978-1-62708-199-3
... to by a variety of names, including peen plating, impact plating, and mechanical galvanizing. Mechanical plating often can solve engineering, economic, and pollution-related plating problems. It offers a straightforward alternative method for achieving desired mechanical and galvanic properties with an extremely...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001462
EISBN: 978-1-62708-173-3
... with a TSC Fig. 8 Plot of service life versus coating thickness as a function of selected environments for a 90/10 aluminum metal-matrix composite with a TSC Galvanic Properties Thermite Sparking Hazard <xref rid="a0001462-ref5" ref-type="bibr">(Ref 5...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003830
EISBN: 978-1-62708-183-2
... Testing Corrosion Rate Prediction Galvanic Action Pitting Intergranular Corrosion Wet-Storage Stain Coating Processes Postgalvanizing Surface Treatment Zinc has electrochemical properties that are important in the production and applications of zinc, including electrowinning...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003216
EISBN: 978-1-62708-199-3
... and is referred to by a variety of names, including peen plating, impact plating, and mechanical galvanizing. Mechanical plating often can solve engineering, economic, and pollution-related plating problems. It offers a straightforward alternative method for achieving desired mechanical and galvanic properties...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003678
EISBN: 978-1-62708-182-5
... sequences in different industries Industry Typical process sequence Car, truck Cleaning, water rinsing, activating, zinc phosphating, water rinsing, sealing, water rinsing, drying Galvanizing line Activating, zinc phosphating, water rinsing, drying Coil coating line Cleaning, water...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003144
EISBN: 978-1-62708-199-3
... Application Thousand metric tonnes Percentage (a) Galvanizing 654 54% Zinc alloy castings 229 18.9% Brasses 155 12.8% Zinc oxide 80 6.4% Miscellaneous (b) 92 7.6% Total 1210 100% (a) Percentages are rounded; columns may not add up to 100%. (b) Includes...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003826
EISBN: 978-1-62708-183-2
... properties corrosion corrosion resistance crevice corrosion galvanic corrosion hafnium hafnium alloys hafnium-tantalum alloys hafnium-zirconium alloys hydrochloric acid mechanical properties nitric acid physical properties pitting corrosion sulfuric acid water alkalis ...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003823
EISBN: 978-1-62708-183-2
... SHE, standard hydrogen electrode Galvanic series in seawater Table 7 Galvanic series in seawater Cathodic (noble) Platinum Gold Graphite Titanium Silver Zirconium Type 316, 317 stainless steels (passive) Type 304 stainless steel (passive) Type 410 stainless...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001276
EISBN: 978-1-62708-170-2
... metal surface military specifications petrolatum compounds physical properties removable coatings rust-preventive compounds safety precautions water-based dry films RUST-PREVENTIVE COMPOUNDS are removable coatings that are used to protect the surfaces of iron, steel, coated or galvanized...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001012
EISBN: 978-1-62708-161-0
... 100 4 40 150 6 6 250 10 69 (a) Service life is defined as time to about 5% red rust. Source: Ref 4 Properties of alloy layers of hot dip galvanized steels Table 5 Properties of alloy layers of hot dip galvanized steels Layer Alloy Iron, % Melting point Crystal...
Book Chapter

By Allan B. Dove
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001017
EISBN: 978-1-62708-161-0
... 2.40 &gt;3.02 to 3.61 &gt;0.119 to 0.142 260 0.85 520 1.70 780 2.55 &gt;3.61 to 4.75 &gt;0.142 to 0.187 270 0.90 550 1.80 820 2.70 &gt;4.75 &gt;0.187 310 1.00 610 2.00 920 3.00 (a) Uncoated wire surface Mechanical properties of galvanized bridge wire used...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001270
EISBN: 978-1-62708-170-2
... ), the corrosion loss is approximately linear with time at an average rate of about 2 μm/year ( Ref 18 ). Near-linear behavior is also observed in marine and rural environments. The sacrificial properties of zinc coatings derive from the position of zinc relative to steel in the galvanic series. The corrosion...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006049
EISBN: 978-1-62708-172-6
...-rich coatings, and discusses the concerns regarding zinc-rich coatings. corrosion rate electrical properties inorganic binders mechanical properties porosity zinc-dust pigment zinc-rich coatings THE USE OF ZINC in corrosion-protective coatings is due to its higher galvanic activity...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003663
EISBN: 978-1-62708-182-5
... for material degradation by weight loss and other corrosion measurements as well as by degradation of such mechanical properties as ultimate tensile strength. A third atmospheric galvanic-corrosion test has been used extensively by ASTM International but has not been standardized. This test ( Ref 12...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003839
EISBN: 978-1-62708-183-2
... Galvanic current density l Liquid state MMC Metal-matrix composite MPT Mixed-potential theory PVD Physical vapor deposition s Solid state SCE Standard calomel electrode σ Standard deviation SiC MF Silicon carbide monofilament SiC MF E SiC MF electrode...