Published: 01 January 1990
Fig. 1 Parts that required different forming characteristics in the steel sheet More
Image
Published: 01 January 2006
Fig. 16 Stretch-forming characteristics of 1.0 mm (0.040 in.) thick copper alloys. Elongation values for a given percentage of cold reduction indicate the remaining capacity for stretch forming in a single operation. Source: Ref 3 More
Image
Published: 01 January 2006
Fig. 28 Illustration of thinning characteristics in the blow forming of an unlubricated part of rectangular cross section and semi-infinite length More
Image
Published: 30 September 2015
Fig. 8 Atomization design characteristics: α, angle formed by free falling molten metal and impinging gas; A , distance between molten metal and gas nozzle More
Image
Published: 01 January 2000
Fig. 5 Experimental pressure-load characteristic of indentations formed in work-hardened mild steel by a hard spherical indenter. Yield stress of steel, Y = 77 kg/mm 2 . Ball diameter is 10 mm. The broken line is the theoretical result for elastic deformation. OL, elastic region; LM, elastic More
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001031
EISBN: 978-1-62708-161-0
... the properties of complicated shapes, and various simulative forming tests. The mechanical properties of steel sheet that influence its forming characteristics, either directly or indirectly, can be measured by uniaxial tension testing. The article covers the effects of steel composition, steelmaking practices...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006720
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, processing effects on physical and mechanical properties, and fabrication characteristics of electrical bus conductor aluminum alloys 6101 and 6201 along with standard temper designations. Machining and forming characteristics...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001089
EISBN: 978-1-62708-162-7
..., and chemical properties; electronic configurations; crystal structures, and explains the alloy forming characteristics of rare earth elements. The article concludes by describing the various applications of commercial-grade rare earth elements and commercial alloys, which incorporates rare earth elements...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005143
EISBN: 978-1-62708-186-3
... Abstract This article reviews the general characteristics of copper and copper alloys and explains how these characteristics affect the behavior of strip in different types of forming operations. These forming operations include blanking, piercing, bending, drawing and stretch forming, spinning...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006693
EISBN: 978-1-62708-210-5
... section of tensile-test specimen. Where a range of values appears in this column, the specified minimum elongation varies with thickness of the mill product. Fabrication Characteristics Aluminum 5005 has excellent forming characteristics, particularly in the 0, H12, and H32 tempers. It can...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006712
EISBN: 978-1-62708-210-5
... on mechanical properties, and fabrication characteristics of this 6xxx series alloy. automotive sheet alloy 6022 corrosion resistance dent resistance fabrication characteristics formability mechanical properties thermal exposure Alloy 6022-T4 is widely used in the U.S. in auto outer panel...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005145
EISBN: 978-1-62708-186-3
... in engineering applications. These iron alloys also have forming characteristics similar to the nickel and cobalt alloys. Depending on the specific alloy, one or more of the following strengthening mechanisms is used in the nickel and cobalt alloys: solid-solution strengthening, precipitation hardening...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003974
EISBN: 978-1-62708-185-6
.... Process Requirements and Forging Machines The behavior and characteristics of the forming machine influence: The flow stress and workability of the deforming material The temperatures in the material and in the tools, especially in hot forming The load and energy requirements for a given...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006702
EISBN: 978-1-62708-210-5
... Up through 5.000 290 42 131 19 16 H112 Up through 13 Up through 5.000 290 42 131 19 12 H311 Up through 13 Up through 5.000 303 44 172 25 12 (a) Area limitation of up through 207 cm 2 (32 in. 2 ) Fabrication Characteristics The extent of cold forming...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006704
EISBN: 978-1-62708-210-5
... to energy efficiency in modern buildings, enabling lower-wattage lights to provide the same amount of light. Fabrication Characteristics Alloys are readily formed in both the annealed and H25 tempers ( Table 6 ). Forming characteristics are similar to 3003. Other fabrication characteristics include...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005147
EISBN: 978-1-62708-186-3
... Abstract This article discusses many of the processes and related considerations involved in the forming of superplastic sheet metal parts. It reviews the requirements for superplasticity and describes the characteristics of superplastic metals. The characterization of superplastic behavior...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003972
EISBN: 978-1-62708-185-6
... on product design while taking advantage of the benefits of deformation processing. deformation manufacturing process product design THE OBJECTIVE of mechanical part design is to specify the geometric details, materials, and surface characteristics that meet the performance requirements...
Image
Published: 01 January 2005
Fig. 5 Four degrees of susceptibility to seaming during thread rolling. (a) Negative susceptibility to form seams. Metal flow adjacent to the die surface is slower than in the middle of the roll form. This is characteristic of metals having a relatively high coefficient of friction More
Image
Published: 01 January 1989
Fig. 5 Four degrees of susceptibility to seaming during thread rolling. (A) Negative susceptibility to form seams. Metal flow adjacent to the die surface is slower than in the middle of the roll form. This is characteristic of metals having a relatively high coefficient of friction More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006719
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, fabrication characteristics, processing effects on physical and mechanical properties, product specifications, and applications of medium-strength structural aluminum alloy 6082. The fabrication characteristics of alloy 6082...