1-20 of 199 Search Results for

foil-fiber-foil process

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
...-reinforced titanium composites magnesium matrix composites copper matrix composites superalloy matrix composites foil-fiber-foil process green tape process metal wire process METAL-MATRIX COMPOSITES (MMCs) are a class of materials with a wide variety of structural, wear, and thermal management...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009085
EISBN: 978-1-62708-177-1
..., including polarized light, bright- and dark-field illumination, and epi-fluorescence. The damage characteristics depend on many factors, including the type of lightning strike protection material on the surface (expanded foil or interwoven wire), the polymer matrix, the fiber type and volume, the lay-up...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003414
EISBN: 978-1-62708-195-5
...) pressure on the resin inlet, vacuum infusion with a thin foil as one mold half, and only vacuum on the resin outlet. But what about a vacuum infusion process with one stiff mold half and a semirigid glass-fiber/polyester second mold half? To speed up the process, one can apply pressure on the inlet (e.g...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000625
EISBN: 978-1-62708-181-8
... in an aluminum alloy 6061 matrix. Fiber diameter: 110 μm. Composite was fabricated by diffusion bonding alternating layers of metal foils and aligned fiber arrays for 30 min at 69 MPa (10 ksi) and 480 °C (895 °F). Tensile strength of the metal-matrix composite was in close agreement with rule-of-mixture values...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006574
EISBN: 978-1-62708-290-7
..., and computer numerical control (CNC) machining operations to create three-dimensional (3D) metal parts ( Ref 1 , 2 ). The process uses metal foils, including tapes, as feedstock and lays down layers side by side and on top of each other, creating a 3D part. With intermittent CNC machining, intricate features...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
.... Fabrication processes for aluminum/boron composites are based on hot-press diffusion bonding of alternating layers of aluminum foil and boron fiber mats (foil-fiber-foil processing) or plasma spraying methods. Selected properties of aluminum/boron composites are given in Table 10 . Room-temperature...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004018
EISBN: 978-1-62708-185-6
... to the directions of metal flow during deformation processing. If fibering is present, flow lines will often be visible on a macroetched section. Fibering often is associated with anisotropic mechanical properties. Figure 19 shows fibering in an Fe-2.5Si flat-rolled electrical sheet. Fig. 19 Fibering...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002465
EISBN: 978-1-62708-194-8
.... Source: Ref 1 , 2 Resin, carbon, or metal matrix, with or without fillers, can be added to the reinforcement fibers or woven fabric as a partially staged resin (partially solidified, stabilized, or cured liquid resin) or as a metal sheet or foil or powder form, or matrix material can be added...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001416
EISBN: 978-1-62708-173-3
... consists of a conventional Ti-6Al-4V or Ti-6242 matrix with layers of continuous silicon-carbide fibers. The layers can be either unidirectional or cross-ply. Two manufacturing techniques can be used: a foil/fiber/foil approach, in which layers of monolithic foil and fiber sets are either vacuum hot...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005639
EISBN: 978-1-62708-174-0
..., weld speed of 1 m/s (3.3 ft/s), and 40 µm thick stainless steel foil. Source: Ref 23 Process Description Suitable Equipment As of this writing (2011), microjoining electron beam welders are just becoming commercially available. Most work to date has been done with converted scanning...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006488
EISBN: 978-1-62708-207-5
... of continuously reinforced composites include diffusion bonding of matrix foils and fiber tapes (foil-fiber-foil method), plasma spraying fiber tapes with the matrix, and coating the fiber by physical vapor deposition with the matrix. Metal-Matrix Composite Solidification Processing...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003839
EISBN: 978-1-62708-183-2
...-bonded B MF -foil and foil-foil interface regions ( Ref 28 , 51 , 52 ). Graphite/Aluminum MMCs Graphite/aluminum MMCs with continuous fiber graphite are known to have high specific tensile strength and stiffness in the direction of the fiber axis, but limitations of shear, compression...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006572
EISBN: 978-1-62708-290-7
..., this is used to bond layers or embed particles and fibers to make composites, typically resulting in a microstructure similar to that of the starting material; however, grain refinement can occur at interfaces between foil layers ( Ref 2 ). Fig. 2 (a) Schematic of the ultrasonic additive manufacturing...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006518
EISBN: 978-1-62708-207-5
... strength in the transverse direction. If this dual-fiber texture is lost by recrystallization, strength in the longitudinal direction decreases to that in the transverse directions. Flat-Rolled Products Flat-rolled products include plate, sheet, and foil. These products are semifabricated...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003614
EISBN: 978-1-62708-182-5
... by the corrosion products of filiform corrosion. Note the void spaces between the paperboard fibers that can entrap water. Scanning electron microscopy. 650× Figure 11 shows typical flaws in PVC coating applied by a chromium-plated gravure. The tendency to follow flaws in the coated foil, such as hills...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001057
EISBN: 978-1-62708-162-7
... production of aluminum and classification system for cast and wrought aluminum alloys. It talks about various manufactured forms of aluminum and its alloys, which are classified into standardized products such as sheet, plate, foil, rod, bar, wire, tube, pipe, and structural forms, and engineered products...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003407
EISBN: 978-1-62708-195-5
..., because excessive deflection can lead to loss of performance. As with the rigs, this drives the design toward the use of carbon-fiber reinforcements. Design Process The design process is not entirely an “engineering” exercise. In addition to the loading scenarios and strength or stiffness criteria...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004177
EISBN: 978-1-62708-184-9
... 12 ). The development of more mobile thermal spray equipment with high deposition efficiency is likely to increase the use of TSA in the chemical process industry. Aluminum Foil Wrapping of Stainless Steel Pipe This technique is widely used in Europe by end users and engineering companies...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005619
EISBN: 978-1-62708-174-0
... resulted in a new manufacturing process known as ultrasonic consolidation (UC). By continuously welding layers of metal foil to previously deposited material, during which the profile for each layer is created by contour milling, UC is able to build up complex, multifunctional, three-dimensional (3-D...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003125
EISBN: 978-1-62708-199-3
... sheet that will be drawn. If texture is not random, ears form during the drawing process. In extruded or drawn rod or bar, the texture is a dual-fiber texture in which almost all grains are aligned so that the grain directions are either [001] or [111]. In heat-treatable alloys, texture has the most...