Skip Nav Destination
Close Modal
Search Results for
fluorinated epoxy resin
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 88 Search Results for
fluorinated epoxy resin
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Image
Published: 30 September 2015
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006077
EISBN: 978-1-62708-172-6
... Novolac resin epoxy phosphate ester resin epoxy resins fluorinated epoxy resin ketimines phenolic co-polymers phosphorus-containing epoxy resin polyamides polyoxyalkylene amines waterborne epoxy resin EPOXY COATING SYSTEMS are the workhorses of the corrosion-protection industry...
Abstract
This article provides a detailed discussion on the principal classes and curatives of epoxy resins used in the coatings industry. The principal classes are bisphenol A epoxy, bisphenol F epoxy, epoxy phenol novolac, cycloaliphatic epoxies, epoxy acrylate, brominated bisphenol-A-based epoxy, phosphorus-containing epoxy, fluorinated epoxies, epoxy esters, epoxy phosphate esters, and waterborne epoxy. The principal curatives are amines, amine adducts, cyanoethylated amines, ketimines, polyoxyalkylene amines, cycloaliphatic amines, aromatic amines, polyamides, amido amines, and dicyandiamides. Other curatives include polyester co-polymers, phenolic co-polymers, melamine and urea formaldehyde co-polymer resins, phosphate flame retardants, ultraviolet and electron beam curing of epoxy resins, Mannich bases, Mannich-based adducts, and anhydrides. The article concludes by discussing the concerns regarding the use of epoxy coatings.
Image
in Nondestructive Testing of Composites (Polymer- and Metal-Matrix Composites)[1]
> Nondestructive Evaluation of Materials
Published: 01 August 2018
Fig. 39 Comparison of pulsed thermography. (a) X-ray. (b) Through-transmission ultrasound. (c) Images of a carbon/epoxy five-ply laminate with aluminum core. Intentional defects include (top to bottom) synthetic fluorine-containing resin inserts in the laminate, synthetic fluorine-containing
More
Image
Published: 01 January 2001
Fig. 39 Comparison of pulsed thermography. (a) X-ray. (b) Through-transmission ultrasound. (c) Images of a carbon/ epoxy 5-ply laminate with aluminum core. Intentional defects include (top to bottom) synthetic fluorine- containing resin inserts in the laminate, synthetic fluorine-containing
More
Book Chapter
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003364
EISBN: 978-1-62708-195-5
... of an addition-cure matrix resin combined with epoxy-like autoclave processing. The BMI matrix composites provide the highest composite mechanical properties available through 177 °C (350 °F)/wet with damage tolerance equivalent to the best epoxies. Certain BMIs are capable of extended service at 230 to 290 °C...
Abstract
This article discusses bismaleimide (BMI) chemistry and the use of BMI in composites. An analysis of the applications illustrates how the advantages of BMIs have been exploited and perhaps suggests how these advantages might be extended to other applications. The article describes the mechanical properties of BMI composites. BMIs suitable for resin transfer molding processing are provided. The article concludes with information on the elevated-temperature applications of 5250-4 BMI system.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006041
EISBN: 978-1-62708-172-6
... of fluoropolymer resins were studied before the FEVE resins were chosen as the most viable candidate. Some of the important criteria were solvent solubility, hydroxyl (–OH) functionality, reasonable glass transition temperature ( T g ) properties, and an adequate presence of fluorine in the polymer backbone...
Abstract
This article provides background information on the chemistry, coating properties, resin types, applications techniques, and performance characteristics of fluoroethylene vinyl ether (FEVE) resins. It describes the formulation methods of FEVE resins, namely, solvent-based coating formulations, water-based coating formulations, and powder coating formulations. The basic concerns to be addressed when formulating and using FEVE coatings are also discussed. The article concludes with a section on health and related safety regulations.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003367
EISBN: 978-1-62708-195-5
... Abstract Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins...
Abstract
Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins. It describes the processing procedures for the cyanate ester resins and provides information on properties for selected applications, such as space applications, radomes, and printed circuit boards.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003692
EISBN: 978-1-62708-182-5
... coatings, and as coating materials in the original equipment manufacturer (OEM) markets. Fine powders produced from high-molecular-weight resins of the thermoplastic vinyl and fluorinated hydrocarbon families, or from thermoset resins of the epoxy and polyester families, are applied to the surface...
Abstract
This article discusses the coating systems categorized by the generic type of binder or resin and grouped according to the curing or hardening mechanism inherent within that generic type. It focuses on the properties, advantages, and limitations of various autooxidative cross-linked resins, thermoplastic resins, and cross-linked thermosetting resins. The autooxidative cross-linked resins include alkyd resins and epoxy esters. The article examines the two types of coatings based on thermoplastic resins: those deposited by evaporation of a solvent, commonly called lacquers, and those deposited by evaporation of water, a class of coatings called water-borne coatings. The coatings that chemically cross link by copolymerization, including epoxies, unsaturated polyesters, urethanes, high-temperature curing silicones, and phenolic linings, are also described.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005672
EISBN: 978-1-62708-198-6
... chemistry includes an oxirane ring, which can functionalize a wide range of monomers or prepolymers. Epoxy adhesives are typically two-part systems (resin and hardener) that cure at room temperature upon mixing. Other cure systems include one-part premixes that use heat cure and one- or two-component UV...
Abstract
This article provides an overview of curing techniques, adhesive chemistries, surface preparation, adhesive selection, and medical applications of adhesives. The curing techniques are classified into moisture, irradiation, heat, and anaerobic. The article highlights the common types of curable adhesives used for medical device assemblies, including acrylics, cyanoacrylates, epoxies, urethanes, and silicones. Other forms of adhesives, such as hot melts, bioadhesives, and pressure-sensitive adhesives, are also discussed. The typical characteristics and applications of biocompatible medical device adhesives are listed in a table. The article concludes with a section on the selection of materials for medical adhesives.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006031
EISBN: 978-1-62708-172-6
... for coatings, namely, PVDF, polyvinyl fluoride, and polytetrafluoroethylene. It focuses on general properties, polymerization, resin types, coating formulation, technology of organic coatings, coating properties, and health and related safety considerations of PVDF. The article describes the application...
Abstract
Polyvinylidene fluoride (PVDF)-based coatings are typically used in outdoor applications that require exceptionally high performance and excellent long-term exterior durability with little maintenance. This article provides a background of three fluoropolymers most commonly used for coatings, namely, PVDF, polyvinyl fluoride, and polytetrafluoroethylene. It focuses on general properties, polymerization, resin types, coating formulation, technology of organic coatings, coating properties, and health and related safety considerations of PVDF. The article describes the application and typical end uses of PVDF-based coatings and the opportunities for improvement in PVDF-based coatings as with all organic coatings.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004181
EISBN: 978-1-62708-184-9
..., polysulfone, polyphenylene sulfide, and polyphenylsulfone, are resistant to HCl. Nonresistant thermoplastics include such polyimides as nylon and methacrylates. Reinforced Thermoset Plastics Reinforced thermoset plastics for HCl service include polyester, epoxy, phenolic, and furan resins. Polyester...
Abstract
Hydrochloric acid (HCl) may contain traces of impurities that will change the aggressiveness of the solution. This article discusses the effects of impurities such as fluorides, ferric salts, cupric salts, chlorine, and organic solvents, in HCl. It describes the corrosion resistance of various metals and alloys in HCl, including carbon and alloy steels, austenitic stainless steels, standard ferritic stainless steels, nickel and nickel alloys, copper and copper alloys, corrosion-resistant cast iron, zirconium, titanium and titanium alloys, tantalum and its alloys, and noble metals. The article illustrates the effect of HCl on nonmetallic materials such as natural rubber, neoprene, thermoplastics, and reinforced thermoset plastics. It also tabulates the corrosion of various metals in dry hydrogen chloride.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004125
EISBN: 978-1-62708-184-9
... are performed in accordance with MIL-A-8625. Primer Epoxy resins are commonly used as binders in high-performance primers due to their exceptional adhesion and chemical resistance. The solvent-borne epoxy primer is manufactured and packaged as a two-component epoxy/polyamide system. One component...
Abstract
This article describes the protective coatings technology used in naval aircrafts. It reviews the future needs and trends of the protective coatings technology based on advancing technology, environmental concerns, and operational requirements. The article discusses the standard finishing systems for aircrafts: the surface pretreatment system, primer, topcoat, advanced-performance topcoat, self-priming topcoat, and specialty coatings. It presents safe compliant solutions to environmental problems associated with the protective coatings technology. These solutions include the use of environmental regulations and hazardous materials, nonchromated pretreatments, waterborne technology, high-solids technology, and touch-up paints. The article also deals with the use of electrodeposition coatings, powder coatings, adhesive films, paint application equipment, and non-chromated sealants in the protective coatings technology.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003047
EISBN: 978-1-62708-200-6
...: Hybrids: Rubber-toughened epoxy, silicone, high-temperature polymers Thermoset polymers: Epoxy, phenolic, polyester, acrylic Rubbery thermosets: Polyether urethanes, polyester urethanes Thermoplastics: Polyamide, polyester Elastomers: Neoprene, nitrile rubber, styrene-butadiene block...
Abstract
This article begins with an overview of the fundamentals of adhesive technology, including functions, limitations, adhesive joint types, and the key factors in the selection of adhesives, including application, type of joint, process limitation, mechanical requirement, and service conditions. It then focuses on the characteristics, types, and properties of the five groups of adhesives, such as structural, hot melt, pressure sensitive, water based, ultraviolet, and electron beam cured adhesives. The article also discusses the functions and applications of adhesive modifiers, including fillers, adhesion promoters, tackifiers, and tougheners. It gives a short note on functions of primers and primerless bonding. Applications of adhesives in automotive, aerospace, electronics, electrical, medical, sports, and construction sectors are also described. Finally, the article describes the steps in adhesive bonding, including storage and handling of adhesives, bonding preparation, adhesive application, tooling, and curing.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006492
EISBN: 978-1-62708-207-5
... The conversion coatings most commonly used are chromates, chrome phosphates, trivalent chromates, or nonchromates. The prime coats and topcoats consist of pigmented organic resins of a number of commonly used paints, including epoxies, polyurethanes, polyesters, alkyds, acrylics, polyvinylidene fluorides...
Abstract
Although aluminum alloys are inherently corrosion resistant, there are many operating environments where they require additional protection. This article describes the conditions under which aluminum is prone to corrode and explains how to prevent it through the addition of conversion coatings and paints. It addresses some of the more common corrosion mechanisms, including corrosion driven by pH extremes, pitting corrosion, crevice corrosion, galvanic corrosion, and filiform corrosion. The article also describes in-plant as well as field application procedures for cleaning and coating, and discusses the advantages and limitations of the various materials and chemicals used.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003023
EISBN: 978-1-62708-200-6
... Coefficient of thermal expansion, 10 −6 /°C °C °F °C °F W/m · K Btu/ft · h · °F Allyl diglycol carbonate 60–90 140–190 100 212 0.2 0.115–0.120 80–140 Bismaleimide resins … … 315 (a) 230 (b) 600 (a) 450 (b) … … 30–50 Epoxy resins 45–290 115–550 120–290...
Abstract
Thermal analysis provides a powerful tool for researchers and engineers in determining both unknown and reproducible behavioral properties of polymer molecules. This article covers the thermal analysis and thermal properties of engineering plastics with respect to chemical composition, chain configuration, conformation of the base polymers, processing of the base polymers with or without additives; and the response to chemical, physical, and mechanical stresses of base polymers as unfilled, shaped articles or as components of composite structures. It also describes thermal analysis techniques, including differential scanning calorimetry, thermogravimetric analysis, thermomechanical analysis, and rheological analysis. This article also summarizes the basic thermal properties used in the application of engineering plastics, such as thermal conductivity, temperature resistance, thermal expansion, specific heat, and the determination of glass transition temperatures. It concludes with a discussion of the thermal and related properties of nine thermostat resin systems divided into three groups by low, medium, and high service temperature capabilities.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006015
EISBN: 978-1-62708-172-6
..., and in powder coatings the choice of binder is limited to binder systems that are solid at ambient temperatures. A review of common binder system chemistries follows. Epoxies Epoxies used in powder coatings are thermoset polymers formed from the reaction of a mixture consisting of epoxy resin...
Abstract
Powder coatings are widely used by manufacturers as a finish of choice to enhance the appearance and performance of their products. This article begins with a discussion on advantages and disadvantages of powder coatings. It describes the selection of coating-types and uses of powder coatings in appliance industries, furniture industries, computer industries, fixture industries, architectural industries, automotive industries, agriculture and construction equipment industries, recreational equipment industries, and general industries. Powder coating formulations consist of binder systems, pigments, extenders, and additives. The basic process flow for the manufacture of powder coatings consists of premix, extrusion, grinding, and packing. The article also provides information on application of powder coatings, including pretreatment, deposition, and curing as well as on troubleshooting, trends and challenges for the powder coatings.
Book Chapter
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
...-bonding resin coatings Table 5 Relative effectiveness of fusion-bonding resin coatings Effectiveness (a) Vinyl Cellulose Epoxy Nylon Chlorinated polyether Polyethylene Exterior durability E VG F F F F Salt spray resistance E G VG VG F F Water resistance E VG G...
Abstract
Coating of cast irons is done to improve appearance and resistance to degradation due to corrosion, erosion, and wear. This article describes inorganic coating methods commonly applied to cast irons. The coating methods include plating, hot dip coating, conversion coating, diffusion coating, cladding, porcelain enameling, and thermal spray. Organic coatings have a wide variety of properties, but their primary use is for corrosion resistance combined with a pleasing colored appearance. The article discusses the various types of organic coatings applied to cast irons. Practically any degree of smoothness or roughness and requirement for color and gloss can be filled by organic coatings. The article describes abrasive blast cleaning, abrasive waterjet cleaning and finishing, vibratory finishing, barrel finishing, and shot peening for processing iron castings.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006028
EISBN: 978-1-62708-172-6
... are being sought. In 1983, it was found that a primer composed of an acrylic copolymer, an epoxy resin, a silica sol, and a trialkoxysilane compound provides superior paintability, degrease resistance, and corrosion resistance after paint coating ( Ref 15 ). Twelve years later, it was found that an SBT...
Abstract
This article focuses on those areas of coatings technology where silicon-based technology (SBT) is the primary enabling technology and where SBT is used as an additive to provide unique properties to the coating film. It describes the chemistry and the uses of alkoxy silanes. The uses of silicates, siliconates, silicone fluids, and silicone resins in coatings are reviewed. The article discusses the various applications of SBT, namely, primers, heat-resistant coatings, industrial maintenance coatings, hygienic coatings, and abrasion-resistant coatings, and for marine biofouling control. It also provides information on the benefits of silicon-base additives.
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005841
EISBN: 978-1-62708-167-2
... the power supply to the desired resonant frequency. Sufficient electrical insulation is required between coil leads to prevent arcing and corona. Typically, synthetic fluorine-containing resin or some other temperature-resistant and highly electrically resistant polymer sheet material is used...
Abstract
Inductors used for brazing can be machined from solid copper shapes or fabricated out of copper tubing, depending on the size and complexity of the braze joint geometry to be heated. This article provides information on inductors (coils) that are generally classified as solenoid, channel (slot), pancake, hairpin, butterfly, split-return, or internal coils. It discusses the variables pertinent to the design of inductors for brazing, soldering, or heat treating. The article presents various considerations for designing inductors for brazing of dissimilar materials that present a unique challenge in the field of induction brazing.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003001
EISBN: 978-1-62708-200-6
... Polyphenylene sulfide 500 533 Alkyd, reinforced 450 505 Felt, tetrafluoroethylene fluorocarbon 450 505 Melamine, reinforced 430 494 Diallyl phthalate 400 478 Epoxy amine coating 400 478 Fluorocarbon, fluorinated ethylene propylene 400 478 Fluorocarbon...