1-20 of 210 Search Results for

flexural test

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003330
EISBN: 978-1-62708-176-4
... Block compression Limited by end crushing to low-strength composites unless end reinforcement is used 3 Sandwich beam specimen test methods ASTM D 3410 Method C-flexure Large specimen. Expensive to fabricate. Simple fixture. Reliable results if specimen is properly designed to prevent core...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003044
EISBN: 978-1-62708-200-6
.... The article also discusses the test procedures, recommended configurations, test specimen considerations, and safety requirements considered in the four major types of mechanical testing of polymer-matrix composites: tensile test, compression test, flexural test, and shear test. compression test...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003256
EISBN: 978-1-62708-176-4
... testing of ceramics Terminology C 1145 Standard Definition of Terms Relating to Advanced Ceramics C 1286 Standard System for Classification of Advanced Ceramics Properties and performance (monolithic) C 1161 Standard Test Method for Flexural Strength of Advanced Ceramics at Ambient...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003443
EISBN: 978-1-62708-195-5
...Selected standards for lamina and laminate mechanical testing Table 1 Selected standards for lamina and laminate mechanical testing Designation Title ASTM standards (a) C 393 Standard Test Method for Flexural Properties of Sandwich Constructions D 638 Standard Test Method...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003312
EISBN: 978-1-62708-176-4
...Methods for determining apparent fracture toughness using small test specimens Table 1 Methods for determining apparent fracture toughness using small test specimens Method Description Calibrations Uncertainties or difficulties Single-edge precracked beam (SEPB) A flexural test...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003321
EISBN: 978-1-62708-176-4
... Majesty's Stationary Office , London , 1989 5. Quinn G.D. and Morrell R. , “Design Data for Engineering Ceramics: A Review of the Flexure Test,” J. Am. Ceram. Soc. , Vol 74 ( No. 9 ), 1991 , p 2037 – 2066 10.1111/j.1151-2916.1991.tb08259.x 6. Cameron D.W...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003319
EISBN: 978-1-62708-176-4
.... Source: Ref 75 , 76 Fig. 14 Schematic of the double torsion test specimen. Source: Ref 88 Fig. 16 Flexure test specimen with a precrack formed by Vickers indentation Fig. 15 Double-cantilever beam (DCB) test specimen ( Ref 8 ). Slots on both sides of the specimen...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003525
EISBN: 978-1-62708-180-1
... is evaluated. The measurement of modulus across a temperature range is referred to as temperature sweep. Dynamic mechanical analysis offers an advantage over traditional tensile or flexural testing in that the obtained modulus is continuous over the temperature range of interest. In addition, special DMAs can...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003380
EISBN: 978-1-62708-195-5
... and mode II; C, pure mode II Fig. 4 Test specimens for determining G c . (a) Mode I, double-cantilever beam (DCB). (b) Mixed mode I and mode II, mixed-mode bending (MMB). (c) Pure mode II, end notch flexure (ENF) Fig. 5 Experimental techniques to obtain a strain energy release...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003057
EISBN: 978-1-62708-200-6
...Abstract Abstract This article describes testing and characterization methods of ceramics for chemical analysis, phase analysis, microstructural analysis, macroscopic property characterization, strength and proof testing, thermophysical property testing, and nondestructive evaluation techniques...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003037
EISBN: 978-1-62708-200-6
... in.) or 51 by 152 mm (2.0 by 6.0 in.) with the bare honeycomb core bonded directly to 12.7 mm (0.5 in.) thick steel plates. Sandwich panel flexure tests are sometimes used to determine the shear properties of high-density or high-strength core materials. Sandwich panel testing is accomplished...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003444
EISBN: 978-1-62708-195-5
...ASTM standards applicable to element-level testing of composites Table 1 ASTM standards applicable to element-level testing of composites Standard designation (a) Title of standard Property C 297 Flatwise Tensile Strength of Sandwich Constructions Flatwise tension C 363...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003374
EISBN: 978-1-62708-195-5
..., and voltage contrast x-ray spectroscopy. The composite lamina methods include the 90 o transverse flexural and tensile tests, three- and four-point shear, ±45 o and edge delamination tests, the short beam shear test method, and the mode I and mode II fracture tests. It should be pointed out that while...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000629
EISBN: 978-1-62708-181-8
... motor nozzles, and tension, flexural, compressive, and shear loadings. carbon-epoxy composites composite prepreg fractograph resin-matrix composites Fig. 1294 Fracture surface of a Fiberite 934 epoxy resin specimen that failed in tension. The specimen was tested at 25 °C (77 °F...
Book Chapter

By Tim Pepper
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003363
EISBN: 978-1-62708-195-5
...ASTM test methods for characterizing mechanical properties of polyester resins Table 1 ASTM test methods for characterizing mechanical properties of polyester resins Properties ASTM Test Method Tensile strength, modulus, and % elongation D 638 Flexural strength and modulus D...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003453
EISBN: 978-1-62708-195-5
... to ASTM D 638, “Standard Test Method for Tensile Properties of Plastics” The compressive properties, according to ASTM D 695, “Standard Test Method for Compressive Properties of Rigid Plastics” The flexural properties, according to ASTM D 790, “Standard Test Method for Flexural Properties...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
...Abstract Abstract Ceramic-matrix composites (CMCs) are being developed for a number of high-temperature and high-performance applications in industrial, aerospace, and energy conservation sectors. This article focuses on processing, fabrication, testing, and characterization methods of CMCs...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003366
EISBN: 978-1-62708-195-5
...Flame spread index and smoke density comparison of thermosetting resins (ASTM E 84 tunnel test) Table 1 Flame spread index and smoke density comparison of thermosetting resins (ASTM E 84 tunnel test) Resin Flame spread index Smoke density Phenolic 10 10 Halogenated polyester...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006676
EISBN: 978-1-62708-213-6
... mechanical analysis offers an advantage over traditional tensile or flexural testing in that the obtained modulus is continuous over the temperature range of interest. In addition, special DMAs can also be conducted to evaluate creep through the application of constant stress or stress relaxation by using...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003383
EISBN: 978-1-62708-195-5
... about the midplane. Fig. 11 Variation of flexural Young's modulus ( E f ) and damping (Ψ) with ply angle ±θ for high-modulus carbon fiber in DX209 epoxy resin. V f = 0.5 Fig. 19 Variation of specific damping capacity (Ψ) for a series of beams cut at various angles (θ) from a woven...