1-20 of 660 Search Results for

fatigue cracks propagation

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002397
EISBN: 978-1-62708-193-1
.... It addresses fatigue crack propagation and sustained-load crack propagation, as well as the fundamental aspects of fracture in steels. The article illustrates the effects of variations in the alloy chemistry, microstructure, temperature, strain rate, and environment on various fracture toughness or crack...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003544
EISBN: 978-1-62708-180-1
... propagation in different environments. The article concludes with a discussion on rolling-contact fatigue, macropitting, micropitting, and subcase fatigue. corrosion fatigue crack growth crack initiation damage tolerance criterion fatigue fracture fatigue strength fatigue-crack propagation finite...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006776
EISBN: 978-1-62708-295-2
... during their lifetime. This article focuses on fractography of fatigue. It provides an abbreviated summary of fatigue processes and mechanisms: fatigue crack initiation, fatigue crack propagation, and final fracture,. Characteristic fatigue fracture features that can be discerned visually or under low...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000603
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that covers pearlitic and ferritic ductile irons. The fractographs display the following: brittle cleavage fracture; fatigue crack propagation; fatigue and monotonic fracture surfaces; fracture modes in slow monotonic loading and impact loading...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003318
EISBN: 978-1-62708-176-4
... Abstract This article provides a review of fatigue test methodologies and an overview of general fatigue behavior, fatigue crack initiation and fatigue crack propagation of advanced engineering plastics. It also describes the factors affecting fatigue performance of polymers and concludes...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000609
EISBN: 978-1-62708-181-8
... fracture, fracture by overpressurization, inclusion effect, fatigue crack propagation, ductile fatigue striation, secondary cracking, intergranular fracture, and elevated-temperature fracture of alloy steels used in pressure vessels, steam boiler superheater tubes, and box-girder bridges. alloy steel...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002410
EISBN: 978-1-62708-193-1
... of these alloys. The effects of grain boundary and grain size on failure are summarized. The article also discusses the effects of microstructure and extrinsic parameters on fatigue crack propagation (FCP). It details the modeling of FCP rates and creep and creep-fatigue crack growth rates. References 1...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003537
EISBN: 978-1-62708-180-1
... corrosive environment and ductile fracture Crack propagates parallel to flutes Striated or ridged fracture Cyclic loading fatigue striations; Constant spacing, constant stress amplitude; variable spacing, variable stress amplitude or block loading (see Fig. 52 ) Striated surface caused...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000630
EISBN: 978-1-62708-181-8
...-brittle fatigue crack propagation, brittle and ductile fracture, crack-growth mechanisms, tearing, fibrillation, and fatigue striations of these surfaces. crack growth fatigue crack propagation fatigue striations fractograph polycarbonate polyethylene polyimide polymers Fig. 1317...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002357
EISBN: 978-1-62708-193-1
... of crack closure on the stress required to propagate fatigue cracks as a function of notch or flaw size. Source: Fracture (Wells and Landes, Ed.), AIME, 1984, p 215–234 Fig. 19 Modified Frost plot of arrest conditions as a function of initial notch size and K T. Shaded areas indicate regions...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002351
EISBN: 978-1-62708-193-1
... on crack growth rates ( R = 0.1). At T ≤ 927 °C, the crack growth rates in the Paris regime are similar. At the two higher temperatures, the growth rates are an order of magnitude larger than at the lower temperatures. Fig. 18 Vacuum and air/vacuum/air fatigue crack propagation tests. Results...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000605
EISBN: 978-1-62708-181-8
... fracture, brittle fracture, tensile-test fracture, transgranular fracture, cleavage fracture, delayed fracture, corrosion fatigue, inclusion morphology, fatigue crack propagation, and in-service fatigue fracture of various automotive components. These components include tie rod adjusting sleeves...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000607
EISBN: 978-1-62708-181-8
...-embrittlement fracture, fatigue crack propagation, and corrosion fatigue of components made from high-carbon steels. The high-carbon steel components include bull gear, drive shaft, power boiler stoker grate, steel wheel, spring wire, suspension spring, automotive engine valve spring, power spring, cantilever...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002414
EISBN: 978-1-62708-193-1
... pressure on the ductility of the DRA materials. It describes the fatigue behavior, such as stress-life behavior, strain-life behavior, and fatigue crack propagation, of the DRA. References 1. Paul B. , Trans. Metall. Soc. AIME , Vol 218 , Feb 1960 , p 36 2. Geiger A.L...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002366
EISBN: 978-1-62708-193-1
... on the typical experimental observations of formation and propagation of small fatigue cracks under various stress states and explores the relation to long crack fracture mixed-mode fracture mechanics. It discusses state I crystallographic and stage II normal stress-dominated growth, along with some observations...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003313
EISBN: 978-1-62708-176-4
... Abstract The separation of the fatigue process into crack initiation and propagation phases has been an important and useful advance in engineering. The combined approach of strain-control testing and the development fracture mechanics of fatigue crack growth rates is a key advance that allows...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003668
EISBN: 978-1-62708-182-5
...) Notched specimens. Source: Ref 40 Fig. 6 Variation of notch sensitivity index with notch radius for steels tested in bending or axial fatigue loading. t , thickness. Source: Ref 38 Fig. 9 Corrosion-fatigue crack propagation rate ( da / dN ) as a function of the cyclic crack tip...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002353
EISBN: 978-1-62708-193-1
... Table 1 Compilation of measured values of the plastic work of fatigue crack propagation, U , for various alloys and calculated values of A in Eq 3 Metal (a) σy(0.2%), MPa Δ K , MPa m U , J/m 2 × 10 −5 da / dN , n /cycle × 10 −8 n A × 10 3 Ref Steels...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000621
EISBN: 978-1-62708-181-8
... gear wheel and actuator beam, an aircraft wing spar, a fractured aircraft propeller blade, shot peened fillet, an aircraft lower-bulkhead cap, and clevis-attachment lugs. aircraft components corrosion fatigue fatigue crack propagation fatigue cracks fatigue fracture fatigue striations...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002362
EISBN: 978-1-62708-193-1
... of more than 10 mm/s to less than 10 −10 mm/s. (a) Venn diagram of mechanisms. (b) Venn diagram of variables listed in Table 1 Fig. 1 Room-temperature corrosion fatigue crack growth rates. (a) Effect of environment on fatigue crack propagation in 4130 steel with a yield strength of 1330 MPa...