1-20 of 2228

Search Results for fabrics

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook Archive
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003360
EISBN: 978-1-62708-195-5
... Abstract This article describes the types of fabrics and preforms used in the manufacture of advanced composites and related selection, design, manufacturing, and performance considerations. The types of fabrics and preforms include unidirectional and two-directional fabrics; multidirectionally...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003033
EISBN: 978-1-62708-200-6
.... It describes the functions, types, and chemical composition of fiber sizing agents. The article discusses the styles, properties, applications, and weaving methods of unidirectional, two-directional and multidirectionally reinforced fabrics. The article also reviews the use of prepreg resins in aerospace...
Book Chapter

By Trevor Gundberg
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 30 April 2026
DOI: 10.31399/asm.hb.v21.a0007046
EISBN: 978-1-62708-489-5
... Abstract This article describes the types of fabrics and preforms used to manufacture advanced and industrial-grade composites and the related selection, design, manufacturing, and performance considerations. It shows typical properties of one mixed graphite/aramid fabric type. The article...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004171
EISBN: 978-1-62708-184-9
... Abstract This article presents a detailed examination of corrosion at the various production stages of wafer fabrication. The corrosion issues related to batch metal-etch systems and single-wafer metal-etch systems are also discussed. The article provides a case study, which illustrates...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003116
EISBN: 978-1-62708-199-3
... Abstract Fabrication of wrought stainless steels requires use of greater power, more frequent repair or replacement of processing equipment, and application of procedures to minimize or correct surface contamination because of its greater strength, hardness, ductility, work hardenability...
Book Chapter

By John G. Banker, Edward G. Reineke
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001376
EISBN: 978-1-62708-173-3
... steel are welded to the respective ends using conventional fusion-welding processes. Transition joint components are produced by explosion welders at their production facilities and then provided in the form of blocks, strips, or tubular couplings to equipment fabricators for use...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005839
EISBN: 978-1-62708-167-2
... current on the induction coil and process design, and the control of heating in different areas of the inductor part. The article reviews three main tools for adjustment of coil design and fabrication: coupling gap, coil copper profile, and magnetic flux controllers. It examines the method of holding...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005841
EISBN: 978-1-62708-167-2
... Abstract Inductors used for brazing can be machined from solid copper shapes or fabricated out of copper tubing, depending on the size and complexity of the braze joint geometry to be heated. This article provides information on inductors (coils) that are generally classified as solenoid...
Image
Published: 15 January 2021
Fig. 33 Residual stress versus depth profiles for as-fabricated and as-fabricated plus peened additive-manufactured parts More
Image
Published: 01 November 1995
Fig. 10 Splicing of fabric and tape prepegs. Overlap splice is used for fabric at all ply orientations and for tape in a 0° direction. Butt-strap splice is used for fabric in which only warp or fill fibers have been cut. Tape prepreg is aligned parallel to the cut fibers. More
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005840
EISBN: 978-1-62708-167-2
..., and brazing and fabricating the copper coil winding for heating billets, bars, and slabs. The article describes refractory selection criteria and the methods of mounting and securing the induction coil winding, and presents general refractory installation guidelines for induction heating applications...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006904
EISBN: 978-1-62708-392-8
... structure. There are some bioink formulations in which polymerization occurs prior to fabrication, such as with spider silk proteins that are intrinsically capable of physical crosslinking ( Ref 20 ). However, even crosslinked GelMA has insufficient mechanical properties for bioprinting. One way to improve...
Book Chapter

By Charles Kennedy, Frank Rampton
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006048
EISBN: 978-1-62708-172-6
... and microcrystalline tapes, marine petrolatum-based pile systems; cold-applied petrolatum-based paste coating systems; hot-applied microcrystalline wax flood coating systems; wax-based dips, brushons, and sprays; and wax-impregnated fabrics and wax-coated papers. The article also discusses the applications...
Image
Published: 01 January 1987
Fig. 177 Fractured shell of an 865-mm (34-in.) diam pressure vessel fabricated from a 32 by 2440 by 9145 mm (1 1 4 by 96 by 360 in.) plate of ASTM A515, grade 70, steel for pressure vessels. The shell broke during testing at an internal gage pressure of 8.3 MPa (1.2 ksi More
Image
Published: 01 January 1987
Fig. 988 View of the shank end of a fractured aircraft propeller blade fabricated of aluminum alloy 2025-T6. The blade broke by fatigue, which originated at an interior cavity that was provided to contain a balance weight comprised of compacted lead wool. Chemical analysis established More
Image
Published: 01 January 1987
Fig. 1035 Fatigue-fracture surface of a bomb-rack side plate fabricated of aluminum alloy 7075-T6. Saw marks at left were made in opening up the fatigue crack for study. Crack origin was found to be at the edge of an attachment hole (marked A, at right). See Fig. 1036 for a view of the area More
Image
Published: 01 January 1987
Fig. 1060 Surface of a fracture in an aircraft lower-bulkhead cap fabricated from an extrusion of aluminum alloy 7075-T6. The cap was cut open to expose the fracture for inspection, and evidence of corrosion was found along the edge at which fracture was initiated (bottom edge in this view More
Image
Published: 01 January 2002
Fig. 12 Pushrod that fractured in bending fatigue after being fabricated by inertia welding. (a) Configuration and dimensions (given in inches). (b) and (c) Micrographs showing structure of decarburized inner surface and sound metal below the decarburized layer More
Image
Published: 01 January 2002
Fig. 25 Austenitic stainless steel tube that was corroded where a fabric bag was taped to it. Courtesy of M.D. Chaudhari, Columbus Metallurgical Service More
Image
Published: 01 January 2002
Fig. 6 Chevrons on the fracture surface of an induction-hardened axle fabricated from 1541 steel. The V-shaped chevrons point back to an initiation site marked by the arrow at the top of the figure. Component shows fatigue crack growth initiating at the arrow creating the circular-shaped More